Microstructural features induced by a high magnetic field in a hypereutectoid steel during austenitic decomposition

被引:70
|
作者
Zhang, YD
Esling, C
Gong, ML
Vincent, G
Zhao, X
Zuo, L [1 ]
机构
[1] Northeastern Univ, Key Lab, Minist Educ, Shenyang 110004, Peoples R China
[2] Univ Metz, LETAM, CNRS, UMR 7078, F-57045 Metz, France
基金
中国国家自然科学基金;
关键词
steel; phase transformation; magnetic field; pearlite; cementite;
D O I
10.1016/j.scriptamat.2006.02.009
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A 12-T magnetic field was introduced during the austenitic decomposition of a high carbon steel at various cooling rates. It was found that the magnetic field applied can reduce the amount of proeutectoid cementite, increase the lamellar spacing of pearlite and decrease the frequencies of low angle misorientations in ferrite. The experimental results of this work prove the shift of the eutectoid point to high carbon side and high temperature side by the application of a magnetic field. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1897 / 1900
页数:4
相关论文
共 50 条
  • [31] Microstructural characterisation and change in a.c. magnetic susceptibility of duplex stainless steel during spinodal decomposition
    Lo, K. H.
    Lai, J. K. L.
    JOURNAL OF NUCLEAR MATERIALS, 2010, 401 (1-3) : 143 - 148
  • [32] Microstructural evolution of an austenitic stainless steel during a complex hot forging sequence
    Tsukahara, H
    Chaze, AM
    Chastel, Y
    Noyes, JL
    Hollard, S
    THERMEC '97 - INTERNATIONAL CONFERENCE ON THERMOMECHANICAL PROCESSING OF STEELS AND OTHER MATERIALS, VOLS I-II, 1997, : 603 - 609
  • [33] Microstructural evolution in 304 austenitic stainless steel during friction stir welding
    Kokawa, Hiroyuki
    Park, Seung Hwan C.
    Sato, Yutaka S.
    Okamoto, Kazutaka
    Hirano, Satoshi
    Inagaki, Masahisa
    ADVANCED WELDING AND MICRO JOINING / PACKAGING FOR THE 21ST CENTURY, 2008, 580-582 : 9 - +
  • [34] Microstructural Evolution During Normal/Abnormal Grain Growth in Austenitic Stainless Steel
    Mohammad Shirdel
    Hamed Mirzadeh
    Mohammad Habibi Parsa
    Metallurgical and Materials Transactions A, 2014, 45 : 5185 - 5193
  • [35] Microstructural evolution of 304 austenitic stainless steel during friction stir welding
    Kokawa, H
    Park, SHC
    Sato, YS
    Okamoto, K
    Hirano, S
    Inagaki, M
    PROCEEDINGS OF THE FOURTEENTH (2004) INTERNATIONAL OFFSHORE AND POLAR ENGINEERING CONFERENCE, VOL 4, 2004, : 73 - 77
  • [36] Microstructural Evolution During Normal/Abnormal Grain Growth in Austenitic Stainless Steel
    Shirdel, Mohammad
    Mirzadeh, Hamed
    Parsa, Mohammad Habibi
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (11): : 5185 - 5193
  • [37] Prediction of metal temperature by microstructural features in creep exposed austenitic stainless steel with sparse modeling
    Endo, Akihiro
    Sawada, Kota
    Nagata, Kenji
    Yoshikawa, Hideki
    Shouno, Hayaru
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS-METHODS, 2021, 1 (01): : 225 - 233
  • [38] NDE of fatigue damap in austenitic stainless steel by measuring and inversion of damage-induced magnetic field
    Chen, ZM
    Aoto, K
    Miya, K
    ELECTROMAGNETIC NONDESTRUCTIVE EVALUATION (VI), 2002, 23 : 127 - 134
  • [39] Features of discontinuous decomposition of austenitic nitrogenized steel after shock-wave loading
    Zel'dovich V.I.
    Uvarov A.I.
    Tereshchenko N.A.
    Frolova N.Yu.
    Litvinov B.V.
    Purygin N.P.
    Doklady Physics, 2000, 45 (1) : 27 - 29
  • [40] Crystallographic Features of Decomposition of g-Phase in Austenitic Corrosion-Resistant Steel
    Lobanov, M. L.
    Pastukhov, V. I.
    Redikultsev, A. A.
    METAL SCIENCE AND HEAT TREATMENT, 2020, 62 (7-8) : 423 - 429