Scallop formation and dissolution of Cu-Sn intermetallic compound during solder reflow

被引:145
|
作者
Ma, D [1 ]
Wang, WD [1 ]
Lahiri, SK [1 ]
机构
[1] Inst Mat Res & Engn, Singapore 117602, Singapore
关键词
D O I
10.1063/1.1445283
中图分类号
O59 [应用物理学];
学科分类号
摘要
In an effort to elucidate the mechanism of scallop formation during reflow of solder/Cu joints in flip-chip and ball-grid array technologies, a planar intermetallic compound layer (mostly Cu6Sn5) was initially formed by solid-state annealing of SnPb/Cu joints at 150 degreesC for ten days. Upon subsequent reflow, dissolution of the intermetallics and formation of scallops were observed. Detailed investigation has indicated that a thermal grooving process due to dissolution of the intermetallic compound during the initial reflow cycles contributes to the formation of scalloped structures, the morphology of which is dictated by the force equilibrium condition. Upon subjecting the solder joints to several reflows, the average intermetallic layer thickness was found to first decrease and then increase, which is shown to be in good agreement with the prediction made by a model based on simultaneous dissolution and growth of the intermetallic compound during reflow. The kinetics of dissolution-growth process during reflow has also been shown to depend on the initial intermetallic thickness and the shape of the solder cap. (C) 2002 American Institute of Physics.
引用
收藏
页码:3312 / 3317
页数:6
相关论文
共 50 条
  • [21] Growth kinetic studies of Cu-Sn intermetallic compound and its effect on shear strength of LCCC SMT solder joints
    Chan, YC
    So, ACK
    Lai, JKL
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1998, 55 (1-2): : 5 - 13
  • [22] Effect of Cu-Sn intermetallic compound reactions on the Kirkendall void growth characteristics in Cu/Sn/Cu microbumps
    Park, Jong-Myeong
    Kim, Seung-Hyun
    Jeong, Myeong-Hyeok
    Park, Young-Bae
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2014, 53 (05)
  • [23] Growth kinetic studies of Cu-Sn intermetallic compound and its effect on shear strength of LCCC SMT solder joints
    City Univ of Hong Kong, Kowloon, Hong Kong
    Mater Sci Eng B Solid State Adv Technol, 1-2 (5-13):
  • [24] Evaluation of intermetallic phase formation and concurrent dissolution of intermetallic during reflow soldering
    Schaefer, M
    Laub, W
    Fournelle, RA
    Liang, J
    DESIGN & RELIABILITY OF SOLDERS AND SOLDER INTERCONNECTIONS, 1997, : 247 - 257
  • [25] Suppressing the growth of Cu-Sn intermetallic compounds in Ni/Sn-Ag-Cu/Cu-Zn solder joints during thermal aging
    Yu, Chi-Yang
    Chen, Wei-Yu
    Duh, Jenq-Gong
    INTERMETALLICS, 2012, 26 : 11 - 17
  • [26] Effect of Solder Joint Thickness on Intermetallic Compound Growth Rate of Cu/Sn/Cu Solder Joints During Thermal Aging
    Zhu, Yan
    Sun, Fenglian
    JOURNAL OF ELECTRONIC PACKAGING, 2016, 138 (04)
  • [27] The growth behavior of Cu-Sn intermetallic compounds during aging
    Chang, JL
    Janz, D
    Liu, XQ
    Yu, LH
    Xie, XM
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 : 332 - 335
  • [28] Formation and growth of intermetallic compound layers at the interface during laser soldering using Sn-Ag Cu solder on a Cu Pad
    Nishikawa, Hiroshi
    Iwata, Noriya
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 215 : 6 - 11
  • [29] Effect of supersaturation of Cu on reaction and intermetallic compound formation between Sn–Cu solder and thin film metallization
    J. S. Ha
    T. S. Oh
    K. N. Tu
    Journal of Materials Research, 2003, 18 : 2109 - 2114
  • [30] Intermetallic compound formation in Sn-Co-Cu, Sn-Ag-Cu and eutectic Sn-Cu solder joints on electroless Ni(P) immersion Au surface finish after reflow soldering
    Sun, Peng
    Andersson, Cristina
    Wei, Xicheng
    Cheng, Zhaonian
    Shangguan, Dongkai
    Liu, Johan
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2006, 135 (02): : 134 - 140