Deactivation and regeneration of sulfur-poisoned supported palladium complexes

被引:12
|
作者
Figoli, NS [1 ]
LArgentiere, PC [1 ]
机构
[1] UNL,FIQ,CATEDRA QUIM INORGAN,RA-3000 SANTA FE,ARGENTINA
关键词
sulfur resistance; palladium; supported complexes; regeneration;
D O I
10.1016/S1381-1169(97)00027-7
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The deactivation by thiophene of the [PdCl2(CH3SOCH3)(2)] and the [PdCl2(NH2(CH2)(12)CH3)(2)] complexes supported on gamma-Al2O3, during the selective hydrogenation of styrene has been studied at 353 K and 10 kg cm(-2). Although both complexes are deactivated when the feed contains more than 300 ppm thiophene, the [PdCl2(NH2(CH2)(12)CH3)(2)] supported complex is more sulfur resistant. Thiophene is partially eliminated by hydrogen treatments at 353 K and 10 kg cm(-2) thereby indicating that thiophene has not substituted, at least totally, the complex ligands.
引用
收藏
页码:141 / 146
页数:6
相关论文
共 50 条
  • [41] INVESTIGATION OF PROCESSES OF ELECTROCHEMICAL SULFUR OXIDATION AND REGENERATION OF IRIDIC ELECTRODES POISONED BY IT - ELECTROLYTE-SULFUR ACID
    SUTYAGINA, AA
    MATVEEVA, TM
    SEMENENKO, MN
    ZHURNAL FIZICHESKOI KHIMII, 1985, 59 (04): : 961 - 964
  • [42] Deactivation by coking of supported palladium catalysts. Effect of time and temperature
    Marecot, P
    Akhachane, A
    Micheaud, C
    Barbier, J
    APPLIED CATALYSIS A-GENERAL, 1998, 169 (01) : 189 - 196
  • [43] On the nature of the deactivation of supported palladium nanoparticle catalysts in the decarboxylation of fatty acids
    Ping, Eric W.
    Pierson, John
    Wallace, Robert
    Miller, Jeffrey T.
    Fuller, Thomas F.
    Jones, Christopher W.
    APPLIED CATALYSIS A-GENERAL, 2011, 396 (1-2) : 85 - 90
  • [44] Permeability of palladium with hydrogen. The loss of diffusing power of pure palladium under the action of temperature. Regeneration of poisoned palladium
    Lombard, V
    Eichner, C
    Albert, M
    COMPTES RENDUS HEBDOMADAIRES DES SEANCES DE L ACADEMIE DES SCIENCES, 1936, 202 : 1777 - 1779
  • [45] EFFECT OF SULFUR ON THE CHEMISORPTIVE PROPERTIES OF SUPPORTED PALLADIUM AND PLATINUM
    MATHIEU, MV
    PRIMET, M
    COMPTES RENDUS DE L ACADEMIE DES SCIENCES SERIE II, 1984, 299 (08): : 419 - 422
  • [46] SULFUR POISONING OF SUPPORTED PALLADIUM METHANOL SYNTHESIS CATALYSTS
    BERUBE, MN
    SUNG, B
    VANNICE, MA
    APPLIED CATALYSIS, 1987, 31 (01): : 133 - 157
  • [47] BEHAVIOR OF PALLADIUM ELECTRODES POISONED WITH SULFUR DURING CYCLIC ANODIC-CATHODIC POLARIZATION
    SUTYAGINA, AA
    PEREPELITSA, VA
    SOVIET ELECTROCHEMISTRY, 1984, 20 (08): : 1036 - 1039
  • [48] Regeneration of supported palladium catalyst for selective hydrogenation of acetylene
    Almanza, LO
    Martinez, OI
    CATALYST DEACTIVATION 2001, PROCEEDINGS, 2001, 139 : 311 - 318
  • [49] NAFION SUPPORTED CATIONIC PALLADIUM COMPLEXES AS CATALYSTS
    SEEN, AJ
    CAVELL, KJ
    MAU, AWH
    HODGES, AM
    JOURNAL OF MEMBRANE SCIENCE, 1994, 87 (1-2) : 149 - 157
  • [50] Mechanism of deactivation of palladium-containing hydrogenation catalysts in the presence of sulfur compounds
    Yurkina, OV
    de Vekki, AV
    Kraev, YL
    PETROLEUM CHEMISTRY, 2004, 44 (03) : 160 - 165