Transient thermal stresses developed during speed sintering of 3 mol% yttria-stabilized tetragonal zirconia polycrystals

被引:4
|
作者
Alshahrani, Abdulaziz M. [1 ,2 ]
Lim, Chek Hai [1 ]
Kim, Jeongho [3 ]
Zhang, Yu [1 ,4 ]
机构
[1] Univ Penn, Sch Dent Med, Dept Prevent & Restorat Sci, Philadelphia, PA 19104 USA
[2] King Khalid Univ, Coll Dent, Dept Restorat Dent Sci, Abha, Saudi Arabia
[3] Univ Connecticut, Dept Civil & Environm Engn, 261 Glenbrook Rd, U-3037, Storrs, CT 06269 USA
[4] Univ Penn, Sch Dent Med, Dept Prevent & Restorat Sci, 240 South 40th St, Levy Bldg 109, Philadelphia, PA 19104 USA
基金
美国国家卫生研究院;
关键词
Speed sintering; Transient stresses; Zirconia green compacts; 3Y-TZP; Finite element analysis; FIXED DENTAL PROSTHESES; MECHANICAL-PROPERTIES; RESTORATIONS; TRANSLUCENCY; GRADIENTS; PORCELAIN; CERAMICS; STRENGTH; FRACTURE; CROWNS;
D O I
10.1016/j.dental.2023.04.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To investigate transient thermal stresses that developed in 3Y-TZP green compacts during speed sintering.Methods: A total of 312 disc-shaped green compacts (o17.1 x1, 1.5, 2, 2.5, 3 mm) were cold-isostatically pressed from 3Y-TZP powder (Zpex, Tosoh Corp.) for speed sintering studies as well as compositional analysis and biaxial flexural strength measurements (both at room temperature and following heating at 90 degrees C/min to 500 degrees C). Flexural strength was determined using the piston-on-3-ball method. Phase assemblies were analyzed using the X-ray diffraction method. Effects of heating/cooling rates on transient stresses were investigated by conducting definitive sintering studies to determine the threshold for fracture. Finite element analysis (FEA) was used to validate the experimental findings using measured thermomechanical properties.Results: The bulk and relative density of the green compact were 2.95 +/- 0.03 g/cm3 and 48.52% +/- 0.45%. The flexural strength was drastically decreased from 10.3 +/- 0.4 MPa to 1.09 +/- 0.07 MPa following heating at 90 degrees C/min to 500 degrees C. The monoclinic and tetragonal contents were 54.9% and 45.1%, respectively. The threshold for fracture was located at 500 degrees C during the first heating stage with a 90 degrees C/min heating rate in specimens of 2.5 mm thickness or greater. No fractures occurred in the second heating stage and cooling phase. The FEA estimated that the principal transient tensile stress was similar to 1.14 MPa at 500 degrees C during the heating phase, which exceeded the corresponding flexural strength (1.09 +/- 0.07 MPa).ignificance: Advanced FEA methods are an accurate and efficient tool to analyze the history of transient stresses during sintering of ceramic dental restorations.
引用
收藏
页码:522 / 528
页数:7
相关论文
共 50 条
  • [31] Strain hardening in superplastic codoped yttria-stabilized tetragonal-zirconia polycrystals
    Sasaki, K
    Nakano, M
    Mimurada, J
    Ikuhara, Y
    Sakuma, T
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (12) : 2981 - 2986
  • [32] Fast firing of 3 mol% yttria-stabilized zirconia: On the effect of heating rate on sintering
    Biesuz, Mattia
    De Bona, Emanuele
    Maniere, Charles
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2024, 107 (10) : 6596 - 6606
  • [33] LOW-TEMPERATURE SUPERPLASTIC FLOW OF YTTRIA-STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS
    BOUTZ, MMR
    WINNUBST, AJA
    BURGGRAAF, AJ
    NAUER, M
    CARRY, C
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1994, 13 (02) : 103 - 111
  • [34] Effect of the current density on the densification of 3 mol% yttria-stabilized zirconia in flash sintering
    Liu, Dianguang
    Li, Xiao
    Liu, Fangzhou
    Liu, Jinling
    Gao, Yan
    Ren, Ke
    Wang, Yiguang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 825
  • [35] Tetragonal BiFeO3 on yttria-stabilized zirconia
    Liu, Heng-Jui
    Du, Yu-Hao
    Gao, Peng
    Huang, Yen-Chin
    Chen, Hsiao-Wen
    Chen, Yi-Chun
    Liu, Hsiang-Lin
    He, Qing
    Ikuhara, Yuichi
    Chu, Ying-Hao
    APL MATERIALS, 2015, 3 (11):
  • [36] Sintering of ultra-fine tetragonal yttria-stabilized zirconia ceramics
    Hwan-Cheol Kim
    In-Jin Shon
    In-Kyoon Jeong
    In-Yong Ko
    Z. A. Munir
    Journal of Materials Science, 2007, 42 : 9409 - 9414
  • [37] Sintering of ultra-fine tetragonal yttria-stabilized zirconia ceramics
    Kim, Hwan-Cheol
    Shon, In-Jin
    Jeong, In-Kyoon
    Ko, In-Yong
    Munir, Z. A.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (22) : 9409 - 9414
  • [38] Structural evolution of plasma-sprayed nanoscale 3 mol% and 5 mol% yttria-stabilized zirconia coatings during sintering
    Zhao, Yan
    Gao, Yang
    APPLIED SURFACE SCIENCE, 2017, 425 : 1033 - 1039
  • [39] Tetragonal phase stabilization and densification in AC flash-sintered 1.5 mol% yttria-stabilized zirconia polycrystals with high toughness
    Ong, Fei Shen
    Nambu, Kohta
    Hosoi, Kohei
    Kawamura, Kenta
    Masuda, Hiroshi
    Feng, Bin
    Matsui, Koji
    Ikuhara, Yuichi
    Yoshida, Hidehiro
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (02) : 1036 - 1043
  • [40] Optimal sandblasting conditions for conventional-type yttria-stabilized tetragonal zirconia polycrystals
    Okada, Masahiro
    Taketa, Hiroaki
    Torii, Yasuhiro
    Irie, Masao
    Matsumoto, Takuya
    DENTAL MATERIALS, 2019, 35 (01) : 169 - 175