Study on impregnation process optimization for regenerating the spent V2O5-WO3/TiO2 catalysts

被引:4
|
作者
Gu, Chunyu [1 ]
Wang, Qiulin [1 ]
Lu, Yicen [1 ]
Tang, Minghui [2 ]
Lu, Shengyong [2 ,3 ]
Jin, Jing [1 ]
机构
[1] Univ Shanghai Sci & Technol, Sch Energy & Power Engn, Shanghai 200093, Peoples R China
[2] Zhejiang Univ, Inst Thermal Power Engn, State Key Lab Clean Energy Utilizat, Hangzhou 310027, Peoples R China
[3] Zhejiang Univ Taizhou, Res Inst, Taizhou 318012, Peoples R China
来源
MOLECULAR CATALYSIS | 2023年 / 550卷
基金
中国国家自然科学基金; 上海市自然科学基金;
关键词
Catalyst regeneration; Spent catalyst; Drying process; deNO(x); SO2/H2O resistance; SCR CATALYSTS; REDUCTION SCR; NO; NH3-SCR; V2O5/WO3-TIO2; TEMPERATURE; SURFACE; NH3; WO3; PERFORMANCE;
D O I
10.1016/j.mcat.2023.113578
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
It is of great economic value and environmental significance to extend the service life of commercial SCR catalysts. Water and acid wash as well as thermal regeneration were often used to remove toxic substances (such as dust, metal sulfates and metal chlorides) residual on catalyst surface so as to reduce the replacement frequency of catalyst, but easily lead to the loss of active components. In this paper, impregnation method was used to supplement the lost active components of the spent honeycombed V2O5-WO3/TiO2 (labeled as VW/Ti) catalyst, and the effects of drying duration and impregnation solution concentration on NH3-SCR performance of catalyst were studied. The results showed that the catalyst dried for 6 h at 110 degrees C exhibited the best deNOx activity and sulfur/water resistance. Further prolonging or shortening drying duration reduced the catalytic activity instead. It can be attributed that proper drying duration constructs abundant pore channels inside catalyst, optimizes active components dispersion, reduces diffusion resistance of reactants into the inner surface and provides more effective active sites on catalyst surface for adsorption and oxidation of reactants. With rise of V content in impregnation solution from 1.06 wt.% to 3.61 wt.%, deNO(x) activity as well as SO2/H2O resistance of catalyst improves at 150-300 degrees C. Besides, key influence factors are also discussed based on reaction kinetics analysis.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Selective Catalytic Reduction of NOx with Ammonia and Hydrocarbon Oxidation Over V2O5-MoO3/TiO2 and V2O5-WO3/TiO2 SCR Catalysts
    Zheng, Lei
    Casapu, Maria
    Stehle, Matthias
    Deutschmann, Olaf
    Grunwaldt, Jan-Dierk
    TOPICS IN CATALYSIS, 2019, 62 (1-4) : 129 - 139
  • [32] Effect of the V4+(3+)/V5+ ratio on the denitration activity for V2O5-WO3/TiO2 catalysts
    Dong, Guo-jun
    Bai, Yang
    Zhang, Yu-feng
    Zhao, Yuan
    NEW JOURNAL OF CHEMISTRY, 2015, 39 (05) : 3588 - 3596
  • [33] V2O5-WO3/TiO2催化剂的制备
    张新堂
    李振兴
    合成材料老化与应用, 2015, 44 (01) : 77 - 81+95
  • [34] A promising method to recover spent V2O5-WO3/TiO2 catalyst: treatment by vanadium-titanium magnetite sintering process
    Long, Hong-ming
    Zhang, Yu-dong
    Yang, Tao
    Qian, Li-xin
    Yu, Zheng-wei
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2022, 29 (08) : 1176 - 1184
  • [35] Selective leaching of V, W and recycling of TiO2 carrier from waste V2O5-WO3/TiO2 catalysts by mixed alkali liquor
    Zhang, Xinyuan
    Zhang, Shengen
    Deng, Lifeng
    Wang, Jianshan
    Wu, Boyu
    Liu, Bo
    Zhang, Bolin
    SUSTAINABLE CHEMISTRY AND PHARMACY, 2023, 36
  • [36] Study on the Calcium-poisoning Mechanism of the V2O5-WO3/TiO2 SCR Catalyst
    He D.
    Ren H.
    Zhu T.
    Zhang Q.
    Tao L.
    Yingyong Jichu yu Gongcheng Kexue Xuebao/Journal of Basic Science and Engineering, 2018, 26 (01): : 1 - 11
  • [37] EXPERIMENTAL AND KINETIC MODELING STUDY OF DENOX ON AN INDUSTRIAL V2O5-WO3/TIO2 CATALYST
    PINOY, LJ
    HOSTEN, LH
    CATALYSIS TODAY, 1993, 17 (1-2) : 151 - 158
  • [38] Study on the local difference of monolithic honeycomb V2O5-WO3/TiO2 denitration catalyst
    Wang, Jinxiu
    Miao, Jifa
    Yu, Weijia
    Chen, Yanting
    Chen, Jinsheng
    MATERIALS CHEMISTRY AND PHYSICS, 2017, 198 : 193 - 199
  • [39] Efficient recovery of scrapped V2O5-WO3/TiO2 SCR catalyst by cleaner hydrometalurgical process
    Lou, Wenbo
    Zhang, Yang
    Zheng, Shili
    Li, Ping
    Zhang, Ying
    Zhang, Yi
    Zhao, Bo
    Li, Zhefei
    Jin, Wei
    HYDROMETALLURGY, 2019, 187 : 45 - 53
  • [40] Variations in the physicochemical properties of spent honeycomb V2O5-WO3/TiO2 catalysts from PC and CFB boilers SCR denitration systems
    Wen, Chaolu
    Guo, Yanxia
    Yan, Kezhou
    Zhang, Huirong
    FUEL, 2023, 347