Microstructure Evolution and Hardness Improvement of WC-Co Composites Sintered with Fe Substituting Part of Co Binder

被引:4
|
作者
Li, Xun [1 ]
Zhang, Junfei [2 ]
Zhang, Qiang [2 ]
Zhang, Xianwei [2 ]
Ji, Vincent [3 ]
Liu, Jinlong [1 ]
机构
[1] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Minist Educ, Shenyang 110819, Peoples R China
[2] Liaoning Wuhuan Special Mat & Intelligent Equipmen, Shenyang 113122, Peoples R China
[3] Univ Paris Saclay, Inst Chim Mol & Mat Orsay, F-91405 Orsay, France
关键词
WC-Co; Fe; eta phase; grain growth; hardness; toughness; NI-CO; GRAIN-GROWTH; METAL; BEHAVIOR; MECHANISM; NICKEL;
D O I
10.3390/coatings13010116
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
WC-13Co (wt.%) composite with Fe added was prepared by pressureless sintering, and its microstructure and mechanical properties were analyzed by X-ray Diffraction (XRD), Scanning Electronic Microscopy (SEM), Energy Dispersive Spectroscopy (EDS) and Vickers hardness tester. The effect of Fe and C content on the microstructure of the eta phase, binder phase, grain size and porosity, as well as mechanical properties in the W-Co-Fe-C system, was discussed quantitatively. The position of added Fe in the lattice of the composites is clarified. When 2%-4% Fe was added, Fe existes in both the binder phase and the low-carbon eta phase. In the lattice of the eta phase, Fe occupies the position of Co and Fe uniformly existes in the binder with the structure of simple cubic when the composites is in the eutectic phase region. Differently from the previous report that the growth of WC in liquid Fe was severely limited, the size of WC in the W-Co-Fe-C system increases from 1.14 mu m to 1.21 mu m when the content of Fe increases from 0 to 4%, which indicates that the growth behavior of WC in liquid CoFe was different from that in liquid Fe, but closer to that in liquid Co. The sample added both 2% Fe and 1% C has the optimum matching of hardness and toughness. Compared with the hardness of 979 HV30 in the sample without adding Fe and C, the hardness of the sample with both 2% Fe and 1% C added achieved 1071 HV30, which is increased by 9.4% under the conditions of a slight increase in fracture toughness.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Microstructure and hardness of WC-Co particle reinforced iron matrix surface composite
    Zhang Peng
    Zeng Shaolian
    Zhang Zhiguo
    Li Wei
    ChinaFoundry, 2013, 10 (06) : 374 - 379
  • [32] Characterization and properties of sintered WC-Co and WC-Ni-Fe hard metal alloys
    Chang, Shih-Hsien
    Chen, Song-Ling
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 585 : 407 - 413
  • [33] MICROSTRUCTURE AND MICROPROPERTIES OF WC-CO ALLOYS
    FRENCH, DN
    JOURNAL OF METALS, 1969, 21 (03): : A70 - &
  • [34] MICROSTRUCTURE AND MICROPROPERTIES OF WC-CO ALLOYS
    FRENCH, DN
    INTERNATIONAL JOURNAL OF POWDER METALLURGY, 1969, 5 (03): : 47 - &
  • [35] A MICROSTRUCTURAL MODEL RELATING FRACTURE-TOUGHNESS AND HARDNESS IN WC-CO COMPOSITES
    LAUGIER, MT
    POWDER METALLURGY INTERNATIONAL, 1986, 18 (05): : 330 - 332
  • [36] PALMQVIST CRACKING IN WC-CO COMPOSITES
    LAUGIER, MT
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1985, 4 (02) : 207 - 210
  • [37] STUDY OF NANOSTRUCTURED WC-CO COMPOSITES
    FANG, ZG
    EASON, JW
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 1995, 13 (05): : 297 - 303
  • [38] Effect of Joining Condition on Plastic Deformation, Microstructure and Bonding Strength for WC-Co to WC-Co
    Gonda, Hidenobu
    Shirai, Yasuhiro
    Yasui, Toshiaki
    Ohashi, Osamu
    Fukumoto, Masahiro
    STEEL RESEARCH INTERNATIONAL, 2010, 81 (09) : 1156 - 1159
  • [39] Quantitative analysis of the effect of the binder phase composition on grain growth in WC-Co sintered materials
    V. Chabretou
    C. H. Allibert
    J. M. Missiaen
    Journal of Materials Science, 2003, 38 : 2581 - 2590
  • [40] Quantitative analysis of the effect of the binder phase composition on grain growth in WC-Co sintered materials
    Chabretou, V
    Allibert, CH
    Missiaen, JM
    JOURNAL OF MATERIALS SCIENCE, 2003, 38 (12) : 2581 - 2590