Microstructural and mechanical behaviour of friction welded SS316L components fabricated by selective laser melting

被引:1
|
作者
Lanka, Dinesh [1 ]
Damodaram, R. [2 ]
Sivaprasad, K. [1 ]
Prashanth, K. G. [3 ,4 ]
机构
[1] Natl Inst Technol, Dept Met & Mat Engn, Adv Mat Proc Lab, Tiruchirappalli 620015, India
[2] Sri Sivasubramaniya Nadar Coll Engn, Dept Mech Engn, Chennai 603110, India
[3] Tallinn Univ Technol, Dept Mech & Ind Engn, Ehitajate Tee 5, EE-19086 Tallinn, Estonia
[4] Vellore Inst Technol, Sch Mech Engn, CBCMT, Vellore 630014, Tamil Nadu, India
来源
关键词
Selective laser melting; Plastic deformation; Stainless steel 316 L; Mechanical properties; rotary friction welding; STAINLESS-STEEL; INCONEL; 718; PROPERTY;
D O I
10.1016/j.mtcomm.2023.107430
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The research study on solid state welding, especially rotary friction welding (FW) on the selective laser melted (SLM) components is limited. The present study is performed to deduce the scope of FW on SLM stainless steel (SS) 316 L parts and also to understand the plastic deformation effect on SLM components. The obtained results can be considered as a reference for the dissimilar welding joints of SS316L with other metallic systems in future studies. The microstructural analysis revealed significant changes in microstructural features like grain morphology and grain orientation. Also, it showed the conventional three distinct zones during the FW process, viz., base metal (BM), heat affected zone (HAZ) and weld zone (WZ). The columnar grains in the BM change into elongated deformed grains while moving towards the WZ. The findings also confirmed the existence of homogeneous equiaxed grains due to complete recrystallization in the WZ. The refined grains, resulted in improved hardness by 23 % at the WZ, when compared with SLM sample. Tensile test results demonstrated an enhancement of yield strength of about 190 MPa, however by sacrificing the ductility. WZ has achieved higher hardness and strength than the SLM component, even though the dislocation density is very high in later one. To understand this coupled effect, work hardening calculations and strengthening contributions were evaluated. The results from strengthening mechanisms confirmed that Hall-Petch strengthening is the dominant strengthening contribution in the welded samples and in case of as built parts it was due to dislocation strengthening.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Microstructural Characterization of the Transition in SS316L and IN625 Bimetallic Fabricated Using Hybrid Additive Manufacturing
    Bettencourt, Christopher J.
    Kouraytem, Nadia
    JOM, 2023, 75 (12) : 5079 - 5087
  • [42] Mechanical characterization and microstructural evolution of Inconel 718 and SS316L TIG weldments at high temperatures
    Yelamasetti, Balram
    Devi, B. Tulasi Lakshmi
    Saxena, Kuldeep K.
    Sonia, Pankaj
    Vardhan, T. Vishnu
    Sree, N. Santhi
    Khubnani, Rashi
    Abdo, Hany Sayed
    Alnaser, Im
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 196 - 207
  • [43] Effect of elevated temperature on wear performance of laser powder bed fusion fabricated SS316L
    Kumar, Navin
    Chandrakumar, Palanisamy
    Cep, Robert
    Arun Prasad, M.
    Sadilek, Marek
    Samal, S. P.
    AIP ADVANCES, 2025, 15 (02)
  • [44] Process optimization for directed energy deposition of SS316L components
    Pei-Yi Lin
    Fang-Cheng Shen
    Kuo-Tsai Wu
    Sheng-Jye Hwang
    Huei-Huang Lee
    The International Journal of Advanced Manufacturing Technology, 2020, 111 : 1387 - 1400
  • [45] Microstructure and Mechanical Properties of 316L Stainless Steel Fabricated Using Selective Laser Melting
    N. Iqbal
    E. Jimenez-Melero
    U. Ankalkhope
    J. Lawrence
    MRS Advances, 2019, 4 : 2431 - 2439
  • [46] Effect of Preheating on Mechanical Properties of 316L Stainless Steel Fabricated by Selective Laser Melting
    Xie Miaoxia
    Xin Qike
    Li Yanxin
    Raza, Khan Muhammad
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2022, 49 (08):
  • [47] Microstructure and Anisotropy of the Mechanical Properties of 316L Stainless Steel Fabricated by Selective Laser Melting
    Zhou, Baogang
    Xu, Pingwei
    Li, Wei
    Liang, Yilong
    Liang, Yu
    METALS, 2021, 11 (05)
  • [48] Microstructure and Mechanical Properties of 316L Stainless Steel Fabricated Using Selective Laser Melting
    Iqbal, N.
    Jimenez-Melero, E.
    Ankalkhope, U.
    Lawrence, J.
    MRS ADVANCES, 2019, 4 (44-45) : 2431 - 2439
  • [49] Process optimization for directed energy deposition of SS316L components
    Lin, Pei-Yi
    Shen, Fang-Cheng
    Wu, Kuo-Tsai
    Hwang, Sheng-Jye
    Lee, Huei-Huang
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 111 (5-6): : 1387 - 1400
  • [50] Experimental investigation on process parameters induced mechanical and microstructural properties for laser powder bed fusion additive manufacturing of SS316L
    Gor, Meet
    Soni, Harsh
    Srivastava, Nishkarsh
    Arora, Amit
    Sahlot, Pankaj
    Oza, Ankit
    Gehlot, Anita
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART E-JOURNAL OF PROCESS MECHANICAL ENGINEERING, 2023,