Relationship between Structure and Properties of Intermetallic Materials Based on γ-TiAl Hardened In Situ with Ti3Al

被引:10
|
作者
Avdeeva, Varvara [1 ]
Bazhina, Arina [2 ]
Antipov, Mikhail [2 ]
Stolin, Alexander [2 ]
Bazhin, Pavel [2 ]
机构
[1] Russian Acad Sci, Kurnakov Inst Gen & Inorgan Chem, Leninskii Prospekt 31, Moscow 119991, Russia
[2] Russian Acad Sci, Merzhanov Inst Struct Macrokinet & Mat Sci, Akad Osipyana 8, Moscow 142432, Russia
关键词
intermetallic; shear deformation; high temperature; tribology; HIGH-TEMPERATURE SYNTHESIS; MECHANICAL-PROPERTIES; MICROSTRUCTURE EVOLUTION; TRIBOLOGY BEHAVIOR; PHASE-COMPOSITION; FRICTION LAYER; TIAL ALLOYS; COMPOSITE; WEAR; AG;
D O I
10.3390/met13061002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, intermetallic materials based on & gamma;-TiAl in situ strengthened with the Ti3Al phase have been obtained from the initial components of titanium and aluminum under the conditions of free SHS-compression in one technological step and in ten seconds. This method combines the process of the combustion of initial components in the mode of self-propagating high-temperature synthesis (SHS) with high-temperature shear deformation of the synthesized materials. The following initial compositions have been studied (mol): Ti-Al, 1.5 Ti-Al, and 3 Ti-Al. Thermodynamic calculations have been carried out and the actual combustion temperature of the compositions under study has been measured. To increase the exothermicity of the studied compositions, a "chemical furnace" based on a mixture of Ti-C powders has been used, which allows us to increase the combustion temperature and stabilize the combustion front. It has been found that the actual combustion temperature of the selected compositions increased from 890-1120 to 1000-1350 & DEG;C. The results of X-ray powder diffraction and SEM are presented, mechanical and tribological characteristics of the obtained materials are measured, and 3D images of wear grooves are given. It has been found that a decrease in Ti molar fraction and an increase in Al molar fraction in the initial mixture lead to an increase in the mechanical (hardness up to 10.2 GPa, modulus of elasticity up to 215 GPa) and tribological characteristics (wear up to 4.5 times, coefficient of friction up to 2.4 times) of intermetallic materials.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Diffusion of Au in the Intermetallic Compound Ti3Al
    Koizumi, Y.
    Tanaka, T.
    Minamino, Y.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (12): : 2919 - 2926
  • [32] Diffusion of Si in Ti3Al intermetallic compound
    Koizumi, Y
    Sakakibara, Y
    Minamino, Y
    Tsuji, N
    DIFFUSION IN MATERIALS: DIMAT 2004, PTS 1 AND 2, 2005, 237-240 : 334 - 339
  • [33] Diffusion of Au in the Intermetallic Compound Ti3Al
    Y. Koizumi
    T. Tanaka
    Y. Minamino
    Metallurgical and Materials Transactions A, 2009, 40 : 2919 - 2926
  • [34] DEFORMATION AND RECRYSTALLIZATION BEHAVIOR OF THE TIAL PHASE CONSTITUTING THE TIAL/TI3AL LAMELLAR STRUCTURE OF TI-RICH TIAL COMPOUNDS
    YAMAGUCHI, M
    ISIJ INTERNATIONAL, 1991, 31 (10) : 1127 - 1133
  • [35] Thermodynamics of yttrium and oxygen in molten Ti, Ti3Al, and TiAl
    Yoshinao Kobayashi
    Fumitaka Tsukihashi
    Metallurgical and Materials Transactions B, 1998, 29 : 1037 - 1042
  • [36] Thermodynamics of yttrium and oxygen in molten Ti, Ti3Al, and TiAl
    Kobayashi, Y
    Tsukihashi, F
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1998, 29 (05): : 1037 - 1042
  • [37] DISSOCIATION OF SUPERDISLOCATIONS IN THE INTERMETALLIC COMPOUND TI3AL
    THOMAS, M
    VASSEL, A
    VEYSSIERE, P
    SCRIPTA METALLURGICA, 1987, 21 (04): : 501 - 506
  • [38] Compton Profile Study of Intermetallic Ti3Al
    Vyas, V.
    Sharma, G.
    Mishra, M. C.
    Joshi, K. B.
    Sharma, B. K.
    OPTICS: PHENOMENA, MATERIALS, DEVICES, AND CHARACTERIZATION: OPTICS 2011: INTERNATIONAL CONFERENCE ON LIGHT, 2011, 1391
  • [39] Strain ageing in α2(Ti3Al)- and γ(TiAl)-based titanium aluminides
    Fröbel, U
    Appel, F
    GAMMA TITANIUM ALUMINIDES 2003, 2003, : 467 - 474
  • [40] Strain ageing in γ(TiAl)-based and α2(Ti3Al) titanium aluminides
    Froebel, Ulrich
    Appel, Fritz
    INTERMETALLICS, 2006, 14 (10-11) : 1187 - 1193