Microstructure evolution and mechanical properties of pulse high current diffusion bonding γ-TiAl alloy to Ti2AlNb alloy

被引:7
|
作者
Fan, Jiafeng [1 ]
Li, Xiaoqiang [1 ]
Pan, Cunliang [1 ]
Zhu, Zhenceng [1 ]
Wang, Xuecheng [1 ]
Qu, Shengguan [1 ]
Yang, Chao [1 ]
Hou, Jinbao [2 ]
机构
[1] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Met Mat, Guangdong Key Lab Adv Met Mat Fabricat & Forming, Guangzhou 510640, Peoples R China
[2] AVIC Mfg Technol Inst, Aeronaut Key Lab Welding & Joining Technol, Beijing 100024, Peoples R China
关键词
Diffusion welding; Pulse high current; TiAl and Ti 2 AlNb alloy; Diffusion coefficient; DEFORMATION MECHANISMS; OXIDATION BEHAVIOR; INTERLAYER; FOIL;
D O I
10.1016/j.intermet.2023.108044
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The development of lightweight high-temperature materials and their processing methods are receiving increasing attention as the need for improved performance and energy efficiency in aero-engines increase. In this study, the gamma-TiAl alloy was successfully soundly bonded to Ti2AlNb alloy by pulsed high current (PHC) diffusion welding. The effect of different high level (HL)/low level (LL) of composite pulse current on the microstructure and mechanical properties of the joints have been studied. The representative interface microstructure of PHC-950 degrees C TiAl/Ti2AlNb joint was gamma-TiAl substrate/diffusion bonding zone/Ti2AlNb impacted zone/Ti2AlNb sub-strate. The diffusion bonding zone was composed of continuous equiaxed alpha 2 grains and a small amount of B2 and O phases. The alpha 2 phase in the diffusion bonding zone was mainly transformed from the gamma phase in gamma-TiAl substrate and the B2 and O phase in Ti2AlNb substrate. The composite pulse current has a significant promoting effect on the diffusion of elements and joint formation. The diffusion coefficients of DAl and DNb in hot-pressing (HP, without current effect) diffusion welding joint at interface were 2 x 10-14 m2/s and 0.92 x 10-14 m2/s, respectively. In the representative PHC-950 degrees C joint with HL/LL = 12/2 cycles (single cycle duration 3.3 ms), diffusion coefficients of DAl-12/2, DNb-12/2 at interface were 19.62 x 10-14 m2/s, 13.34 x 10-14 m2/s, respectively. Increasing the duration of LL would weaken the current effect. The current waveform parameters were tuned to HL/LL = 12/4 and 12/6 cycles, the diffusion coefficients of DAl-12/4, DNb-12/4 DAl-12/6 and DNb-12/6 were reduced to 15.69 x 10-14 m2/s, 12.49 x 10-14 m2/s, 15.31 x 10-14 m2/s and 10.99 x 10-14 m2/s, respectively. The PHC-950 degrees C joints have the highest shear strength of 257.3 MPa at HL/LL = 12/2 cycles, reaching 83.3% of the base material strength. The HP-950 degrees C TiAl/Ti2AlNb joint has a shear strength of 230.5 MPa, reaching 74.6% of the base material strength. The shear strength of PHC-950 degrees C joints at HL/LL = 12/4 and 12/6 reduced to 205.3 MPa, 195.8 MPa due to insufficient element diffusion and damages the bonding quality. This work provides a strategy that contributes to reduce the thermal damage of base metal and improve the joint forming efficiency.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Effect of processing parameters on the microstructure and mechanical properties of TiAl/Ti2AlNb laminated composites
    Li, Donghai
    Wang, Binbin
    Luo, Liangshun
    Li, Xuewen
    Xu, Yanjin
    Li, BinQiang
    Hawezy, Diween
    Wang, Liang
    Su, Yanqing
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 109 : 228 - 244
  • [42] Effect of welding temperature on microstructure and mechanical properties of TiAl/Ti2AlNb spark plasma diffusion welded joint
    Ma, Mingqian
    Chen, Chunhuan
    Chai, Lu
    Lv, Yanlong
    Hou, Jinbao
    Zhang, Boxian
    WELDING IN THE WORLD, 2022, 66 (05) : 985 - 994
  • [43] Microstructure and Properties of the Near-β Isothermally Forged Ti2AlNb Based Alloy
    Zhang Jianwei
    Liang Xiaobo
    Cheng Yunjun
    Zeng Weidong
    Xue Qiang
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (05) : 1157 - 1160
  • [44] Effect of Heat Treatment on Microstructure and Mechanical Properties of Near-β Forged Ti2AlNb Based Alloy
    热处理对近β锻造的多元Ti2AlNb基合金组织和性能的影响
    He, Yongsheng (heysh1210@126.com), 2018, Science Press (47):
  • [45] Microstructure and properties of the near-β isothermally forged Ti2AlNb based alloy
    Zhang, J. (TiAl@superalloy.cn), 1600, Science Press (43):
  • [46] Effect of Heat Treatment on Microstructure and Mechanical Properties of Near-β Forged Ti2AlNb Based Alloy
    He Yongsheng
    Hu Rui
    Luo Wenzhong
    He Tao
    Lai Yunjin
    Du Yujun
    Liu Xianghong
    Yang Jieren
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (11) : 3460 - 3467
  • [47] Elemental Composition, Phase Diagram, Microstructure, Fabrication Processes, and Mechanical Properties of Ti2AlNb Alloy: A Review
    Fu, Yanqi
    Su, Zimu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (23) : 12819 - 12846
  • [48] Microstructure and mechanical properties of vacuum diffusion bonding joints for γ-TiAl based alloy
    Du, Zhihao
    Zhang, Kaifeng
    Lu, Zhen
    Jiang, Shaosong
    VACUUM, 2018, 150 : 96 - 104
  • [49] Research and prospect of Ti2AlNb alloy
    Liu S.-S.
    Cao J.-X.
    Zhou Y.
    Dai S.-L.
    Huang X.
    Cao C.-X.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2021, 31 (11): : 3106 - 3126
  • [50] Effects of hot deformation parameters on lamellar microstructure evolution of Ti2AlNb based alloy
    Zeng, Wei-Dong, 1998, Central South University of Technology (24):