Plasma Hydrogenation of High-Carbon Structural Steel Wires under Different Prestressing Levels

被引:0
|
作者
El-Amoush, Amjad Saleh [1 ]
Al-Duheisat, Salman A. [2 ]
机构
[1] Al Balqa Appl Univ, Coll Engn, Dept Mat & Met Engn, POB 7181, Al Salt 19117, Jordan
[2] Ajloun Natl Univ, Coll Engn, Ajloun 26810, Jordan
关键词
Plasma hydrogenation; hydrogen embrittlement; high-carbon steel Ovire; prestressing; STRESS-CORROSION CRACKING; HIGH-STRENGTH STEEL; EMBRITTLEMENT SUSCEPTIBILITY; CATHODIC PROTECTION; COLD-DRAWN; RESIDUAL-STRESSES; EUROFER; 97; DIFFUSION; MECHANISM; BEHAVIOR;
D O I
10.1590/1980-5373-MR-2022-0358
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High-carbon structural steel wires were prestressed to various levels in a plasma hydrogenation environment and then pulled in a slow strain rate test (SSRT). The effect of plasma hydrogenation under different prestressing levels on the material's tensile response and hydrogen embrittlement was noted. It was found that the ultimate tensile strength (UTS), yield strength, and ductility of the steel wire samples are decreased by plasma hydrogenation and prestressing levels. The more drastic decrease in the UTS, yield strength, and ductility is found in the plasma hydrogenated prestressing steel to a higher prestressing level. Moreover, the hydrogen embrittlement index of the steel wire samples is significantly increased by plasma hydrogenation and prestressing level. The highly plasma hydrogenated prestressing steel wire samples exhibit complete brittle fracture. A mixed mode of fracture, i.e., ductile and brittle, was observed at the surface of the plasma hydrogenated prestressing steel wire samples at lower levels. The hydrogen embrittlement areas at the fracture surfaces of steel wire samples are observed to increase with plasma hydrogenation and prestressing levels. More severe hydrogen cracking and blistering resulted in the fracture surfaces of plasma-hydrogenated prestressing steel wire samples with higher levels.
引用
收藏
页数:11
相关论文
共 50 条