Study on fusion boundary microstructure and mechanical properties of austenitic stainless steel-nickel based dissimilar alloy materials welded joints

被引:2
|
作者
Zhao, Xilong [1 ]
Ren, Kangming [1 ]
Lu, Xinhong [1 ]
He, Feng [1 ]
Jiang, Yuekai [1 ]
机构
[1] Lanzhou Jiaotong Univ, Sch Mat Sci & Engn, Lanzhou, Peoples R China
基金
中国国家自然科学基金;
关键词
Austenitic; Overlayer; GTAW-P and SMAW; Weld; Cracks; Property; DUCTILITY-DIP CRACKING; METAL; BEHAVIOR; MARTENSITE; WATER; WORK; WIRE; CR;
D O I
10.1016/j.engfracmech.2023.109140
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
The metallographic test, microhardness test, and shear punch test of overlayer joint were carried out. The microstructure distribution and micro-zone mechanical properties of overlayer-girth weld fusion boundary (O-G), overlayer-austenitic (O-A) fusion boundary, and austenitic-grith weld fusion boundary (A-G) were studied respectively. At the same time, the type II boundary, DDC, and liquefaction crack were discovered. The results show that the microstructures on both sides of the O-G fusion boundary are gamma phase and austenite-ferrite, respectively. There are three types of fusion limitations: type II boundary, direct fusion boundary, and transition fusion boundary. There are DDCs in the transition fusion boundary of the O-G zone, and liquefaction cracks caused by composition segregation in the inner of overlayer. The microstructures on both sides of the O-A fusion boundary are gamma phase and uniaxial austenite, respectively, and there is no evident transition zone. Microstructures on both sides of the A-G fusion boundary are equiaxed austenite and austenite-ferrite (lath-skeleton-short rod). The average microhardness and shear strength of the O-A-G fusion border overlayer is the highest, 241 HV and 782 MPa respectively, and the microhardness decreases to 215 HV at DDCs defect. The microhardness and shear strength of base metal are 212 HV, 661 MPa, respectively. The microhardness and shear strength of the girth weld are 192 HV, 600 MPa, respectively. The maximum shear work of O zone is 1.62 J, and the minimum O-G fusion boundary is 1.12 J.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Local mechanical properties of dissimilar metal TIG welded joints of CoCrFeMnNi high entropy alloy and AISI 304 austenitic steel
    Michael Rhode
    Kjell Erxleben
    Tim Richter
    Dirk Schroepfer
    Tobias Mente
    Thomas Michael
    Welding in the World, 2024, 68 : 1563 - 1573
  • [42] Local mechanical properties of dissimilar metal TIG welded joints of CoCrFeMnNi high entropy alloy and AISI 304 austenitic steel
    Rhode, Michael
    Erxleben, Kjell
    Richter, Tim
    Schroepfer, Dirk
    Mente, Tobias
    Michael, Thomas
    WELDING IN THE WORLD, 2024, 68 (06) : 1563 - 1573
  • [43] Mechanical Properties Evaluation and Crack Propagation Behavior in Dissimilar Metal Welded Joints of 304 L Austenitic Stainless Steel and SA508 Low-Alloy Steel
    Sun, Yuman
    Xue, He
    Yang, Fuqiang
    Wang, Shuai
    Zhang, Shun
    He, Jinxuan
    Bashir, Rehmat
    SCIENCE AND TECHNOLOGY OF NUCLEAR INSTALLATIONS, 2022, 2022
  • [44] Microstructure, mechanical and corrosion properties of friction stir welded high nitrogen nickel-free austenitic stainless steel
    Li, H. B.
    Jiang, Z. H.
    Feng, H.
    Zhang, S. C.
    Li, L.
    Han, P. D.
    Misra, R. D. K.
    Li, J. Z.
    MATERIALS & DESIGN, 2015, 84 : 291 - 299
  • [45] Microstructure and mechanical properties of dissimilar friction stir welded type 304 austenitic stainless steel to Q235 low carbon steel
    Wang, Hongduo
    Wang, Kuaishe
    Wang, Wen
    Huang, Liying
    Peng, Pai
    Yu, Hailiang
    MATERIALS CHARACTERIZATION, 2019, 155
  • [46] A study of mechanical properties of friction welded mild steel to stainless steel joints
    Ananthapadmanaban, D.
    Rao, V. Seshagiri
    Abraham, Nikhil
    Rao, K. Prasad
    MATERIALS & DESIGN, 2009, 30 (07) : 2642 - 2646
  • [47] Microstructure, mechanical properties and formability of friction stir welded dissimilar materials of IF-steel and 6061 Al alloy
    Semih Mahmut Aktarer
    Dursun Murat Sekban
    Tevfik Kucukomeroglu
    Gencaga Purcek
    International Journal of Minerals, Metallurgy, and Materials, 2019, 26 : 722 - 731
  • [48] Microstructure, mechanical properties and formability of friction stir welded dissimilar materials of IF-steel and 6061 Al alloy
    Semih Mahmut Aktarer
    Dursun Murat Sekban
    Tevfik Kucukomeroglu
    Gencaga Purcek
    InternationalJournalofMineralsMetallurgyandMaterials, 2019, 26 (06) : 722 - 731
  • [49] Microstructure, mechanical properties and formability of friction stir welded dissimilar materials of IF-steel and 6061 Al alloy
    Aktarer, Semih Mahmut
    Sekban, Dursun Murat
    Kucukomeroglu, Tevfik
    Purcek, Gencaga
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 26 (06) : 722 - 731
  • [50] Structure and properties of titanium alloy/copper-nickel/stainless steel welded joints
    Chang J.
    Yu G.
    Cao R.
    Yan Y.
    Sui R.
    Xi X.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2023, 44 (07): : 48 - 55