Deformation Behavior and Microstructure of 6061 Aluminum Alloy Processed by Severe Plastic Deformation Using Biaxial Alternate Forging

被引:1
|
作者
Ha, Seong-Ho [1 ]
Shin, Young-Chul [1 ]
机构
[1] Korea Inst Ind Technol, Incheon 21999, South Korea
关键词
biaxial alternate forging; severe plastic deformation; FEM; AA6061; mechanical property; AL-MG ALLOY; STRENGTH; DUCTILITY; HOT;
D O I
10.3390/ma17050968
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The deformation behavior and microstructure of 6061 aluminum alloy processed by severe plastic deformation (SPD) using biaxial alternate forging that can evaluate the forming limit and mechanical properties of alloys, simultaneously, were investigated in this study. A finite element (FE) analysis on the biaxial alternating forging process, considering the strain-hardening coefficient and forging pass of the material, was conducted. When the strain-hardening coefficient is 0, an average effective strain of 440% was found within a diameter of 4 mm in the core of the workpiece after eight passes, while it was 300% at the same pass number when the strain-hardening coefficient was 0.2. The average effective strain estimated from the FE analysis was about 264% after eight passes of forging, which is considered to be a level of SPD that significantly exceeds the elongation of the raw material. As a result of the tensile test according to the forging pass, after two passes, the strength of the material could be gradually improved without significant degradation of elongation. Even though a large strain of 264% was found after eight passes were applied, deformed grains and twins with no recrystallized structure in optical microstructures with different forging passes were found.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] Pitting Corrosion Resistance of Anodized Aluminum-Copper Alloy Processed by Severe Plastic Deformation
    Son, In-Joon
    Nakano, Hiroaki
    Oue, Satoshi
    Kobayashi, Shigeo
    Fukushima, Hisaaki
    Horita, Zenji
    MATERIALS TRANSACTIONS, 2008, 49 (11) : 2648 - 2655
  • [42] Microstructure and mechanical properties of Mg-Li alloy processed by severe plastic deformation and annealing
    Lin, Kai
    Kang, Zhi-Xin
    Fang, Qiang
    Zhang, Jun-Yi
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2013, 23 (12): : 3267 - 3274
  • [43] Pitting corrosion resistance of anodized aluminum-copper alloy processed by severe plastic deformation
    Son, In-Joon
    Nakano, Hiroaki
    Oue, Satoshi
    Kobayashi, Shigeo
    Fukushima, Hisaaki
    Horita, Zenji
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2008, 72 (05) : 353 - 359
  • [44] Microstructure control using severe plastic deformation
    Horita, Zenji
    Oh-ishi, Keiichiro
    Kaneko, Kenji
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2006, 7 (07) : 649 - 654
  • [45] Effects of strain rate and temperature on hot tensile deformation of severe plastic deformed 6061 aluminum alloy
    Khamei, A. A.
    Dehghani, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 627 : 1 - 9
  • [46] Hot tensile deformation behavior of Mg-Zn-Al magnesium alloy tubes processed by severe plastic deformation
    Eftekhari, M.
    Fata, A.
    Faraji, G.
    Mashhadi, M. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 742 : 442 - 453
  • [47] An overview on the corrosion behavior of steels processed by severe plastic deformation
    Cardona, Diana M. Marulanda
    Nieto, Fabio E. Castillejo
    MATERIALS TRANSACTIONS, 2023, 64 (07) : 1317 - 1324
  • [48] Microstructure of a metal-polymer composite processed by severe plastic deformation
    Sauvage, Xavier
    Malandain, Jean-Jacques
    Hohenwarter, A.
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2, 2008, 584-586 : 306 - 309
  • [49] Microstructure and mechanical properties of pure nickel processed by severe plastic deformation
    Nurislamova, GV
    Islamgaliev, RK
    Valiev, RZ
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION, 2006, 503-504 : 579 - 584
  • [50] An Investigation of Cavity Development during Superplastic Flow in a Zinc-Aluminum Alloy Processed Using Severe Plastic Deformation
    Kawasaki, Megumi
    Langdon, Terence G.
    MATERIALS TRANSACTIONS, 2012, 53 (01) : 87 - 95