The Effect of Casting Technique and Severe Straining on the Microstructure, Electrical Conductivity, Mechanical Properties and Thermal Stability of the Al-1.7 wt.% Fe Alloy

被引:7
|
作者
Medvedev, Andrey [1 ]
Zhukova, Olga [1 ]
Enikeev, Nariman [2 ]
Kazykhanov, Vil [1 ]
Timofeev, Victor [3 ]
Murashkin, Maxim [1 ,2 ]
机构
[1] Ufa Univ Sci & Technol, Inst Phys Adv Mat, 32 Zaki Validi Str, Ufa 450076, Russia
[2] St Petersburg State Univ, Lab Dynam & Extreme Characterist Promising Nanostr, St Petersburg 198504, Russia
[3] Siberian Fed Univ, Dept Elect Engn, 79 Svobodnyy Prospekt, Krasnoyarsk 660041, Russia
基金
俄罗斯科学基金会;
关键词
Al-Fe alloys; electromagnetic mold; severe plastic deformation; equal channel angular pressing; cold rolling; ultrafine grain structure; mechanical properties; electrical conductivity; thermal stability; HIGH-PRESSURE TORSION; ULTRAFINE-GRAINED AL; ECAP-CONFORM; PRINCIPLES; SPD;
D O I
10.3390/ma16083067
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper features the changes in microstructure and properties of an Al-Fe alloy produced by casting with different solidification rates followed by severe plastic deformation and rolling. Particularly, different states of the as-cast Al-1.7 wt.% Fe alloy, obtained by conventional casting into a graphite mold (CC) and continuous casting into an electromagnetic mold (EMC), as well as after equal-channel angular pressing and subsequent cold rolling, were studied. Due to crystallization during casting into a graphite mold, particles of the Al6Fe phase are predominantly formed in the cast alloy, while casting into an electromagnetic mold leads to the formation of a mixture of particles, predominantly of the Al2Fe phase. The implementation of the two-stage processing by equal-channel angular pressing and cold rolling through the subsequent development of the ultrafine-grained structures ensured the achievement of the tensile strength and electrical conductivity of 257 MPa and 53.3% IACS in the CC alloy and 298 MPa and 51.3% IACS in the EMC alloy, respectively. Additional cold rolling led to a further reduction in grain size and refinement of particles in the second phase, making it possible to maintain a high level of strength after annealing at 230 degrees C for 1 h. The combination of high mechanical strength, electrical conductivity, and thermal stability can make these Al-Fe alloys a promising conductor material in addition to the commercial Al-Mg-Si and Al-Zr systems, depending on the evaluation of engineering cost and efficiency in industrial production.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Influences of high temperature on the microstructural, electrical and mechanical properties of Ni-23 wt.% Al alloy
    Karakose, Ercan
    Keskin, Mustafa
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2015, 106 (01) : 29 - 42
  • [32] Effect of Titanium and Carbon on Microstructure and Mechanical Properties of Disordered Solid Solution Fe–7 wt%Al Alloy
    Shishir Chaudhary
    Shivkumar Khaple
    V. V. Satya Prasad
    A. Sambasiva Rao
    R. G. Baligidad
    Transactions of the Indian Institute of Metals, 2015, 68 : 809 - 815
  • [33] Effect of Er on Microstructure, Electrical Conductivity, Mechanical Properties, and Corrosion Resistance of an Al-Zr Alloy
    Hu, Xionglei
    Wang, Chunxia
    Ma, Guorui
    He, Kezhun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [34] Effect of Nb, Y and Zr on thermal stability of nanocrystalline Al-4.5 wt.% Cu alloy prepared by mechanical alloying
    Kumar, A. Prem
    Muthaiah, V. M. Suntharavel
    Mula, Suhrit
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 722 : 617 - 627
  • [35] Microstructure, Mechanical Properties, Electric and Thermal Conductivity of the As-Extruded Al-x(1.0 wt.% Zn+0.5 wt.% Cu) Alloys (x=1, 2 and 4)
    Kim, Yong-Ho
    Yoo, Hyo-Sang
    Son, Hyeon-Taek
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2020, 20 (07) : 4248 - 4252
  • [36] Investigation of mechanical, electrical, and thermal properties of a Zn-1.26 wt% Al alloy
    Cadirli, Emin
    Sahin, Mevlut
    JOURNAL OF MATERIALS SCIENCE, 2011, 46 (05) : 1414 - 1423
  • [37] Microstructure, Tensile and Fatigue Properties of Al-5 wt.%Mg Alloy Manufactured by Twin Roll Strip Casting
    Heo, Joon-Young
    Baek, Min-Seok
    Euh, Kwang-Jun
    Lee, Kee-Ahn
    METALS AND MATERIALS INTERNATIONAL, 2018, 24 (05) : 992 - 1001
  • [38] Effect of carbon on mechanical properties of Fe-23 wt% Al alloy
    Baligidad, RG
    Radhakrishna, A
    Sarma, DS
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (20) : 5537 - 5539
  • [39] Effect of carbon on mechanical properties of Fe-23 wt% Al alloy
    R. G. Baligidad
    A. Radhakrishna
    D. S. Sarma
    Journal of Materials Science, 2005, 40 : 5537 - 5539
  • [40] Effect of intense plastic straining on microstructure and mechanical properties of an Al-Mg-Sc alloy
    Kaibyshev, R.
    Avtokratova, E.
    Sitdikov, O.
    15TH INTERNATIONAL CONFERENCE ON THE STRENGTH OF MATERIALS (ICSMA-15), 2010, 240