Early mechanical strength, hydration mechanism and leaching behavior of alkali-activated slag/fly ash paste filling materials

被引:15
|
作者
Liu, Shulong [1 ,3 ]
Wang, Yiming [1 ,3 ]
Wu, Aixiang [1 ,3 ]
Shi, Daqing [1 ,3 ]
Yang, Shixing [1 ,3 ]
Ruan, Zhuen [1 ,2 ,3 ]
Song, Xintao [1 ,3 ]
Zhang, Minzhe [1 ,3 ]
机构
[1] Univ Sci & Technol Beijing, Sch Civil & Resources Engn, Beijing 100083, Peoples R China
[2] Shunde Grad Sch Univ Sci & Technol Beijing, Foshan 528399, Peoples R China
[3] Univ Sci & Technol Beijing, Key Lab High Efficient Min & Safety Met Mines, Minist Educ, Beijing 100083, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Alkali -activated material; Activator; Cemented paste backfill; Compressive strength; Heavy metals immobilization; HEAVY-METAL IMMOBILIZATION; COMPRESSIVE STRENGTH; FLY-ASH; TAILINGS; BACKFILL; TEMPERATURE; HYDROXIDE; BINDER;
D O I
10.1016/j.jobe.2024.108481
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The enhancement of the early strength of the filling body is regarded as a critical technology for shortening the mining & filling cycle and achieving efficient production. It is a high-value utilization pathway to entirely replace Ordinary Portland Cement (OPC) with industrial waste residue. Hence, in this research, ground granulated blast furnace slag (GGBFS) and fly ash (FA) were selected as aluminosilicate precursors. The effects of single-component and binary activation of Na2SiO3, Na2SO4, Na2CO3, NaOH, NaAlO2 and triethanolamine (TEA) on the mechanical strength of backfill were systematically investigated. The microstructural evolution mechanism of hydration products was elucidated using XRD, TG-DTG, SEM and MIP analyses. The leaching characteristics and immobilization mechanism of heavy metals were further revealed. The experimental results indicated that the activator contributed an alkaline environment and active ions to the initial hydrolysis reaction of precursors and the polycondensation reaction of silica tetrahedra and aluminum tetrahedra with Ca2+ drove the hardening and development of the hydration products. Na2SiO3 exhibited the superior activation effect among single-component activators, while the binary activator presented notable "promoting and inhibiting characteristics". Moreover, the binary activator composed of 4% Na2SiO3 and 4% NaAlO2 conducted the highest compressive strength at 3 d and 7 d. The dominant hydration products of the backfill were ettringite, C-S-H gels, C-A-S-H gels and zeolite-like products. The density of microstructures and the crystallinity of hydration products were significantly enhanced ascribed to the synergistic and complementary effects of Na2SiO3 and NaAlO2. Heavy metals were immobilized by the hydration products through physical encapsulation and chemical bonding, and the leaching concentrations of all heavy metals (Pb, Cd, Cr(VI), Zn, Mn, As and Cu, etc.) were lower than the standard limits of Class III in GB/T 14848-2017.
引用
收藏
页数:16
相关论文
共 50 条
  • [11] Mechanical property and structure of alkali-activated fly ash and slag blends
    Yang, Tao
    Yao, Xiao
    Zhang, Zuhua
    Wang, Hao
    JOURNAL OF SUSTAINABLE CEMENT-BASED MATERIALS, 2012, 1 (04) : 167 - 178
  • [12] Binding mechanism and properties of alkali-activated fly ash/slag mortars
    Chi, Maochieh
    Huang, Ran
    CONSTRUCTION AND BUILDING MATERIALS, 2013, 40 : 291 - 298
  • [13] Effect of Steel Slag on Hydration Kinetics and Rheological Properties of Alkali-Activated Slag Materials: A Comparative Study with Fly Ash
    Han, Fanghui
    Zhu, Ziqin
    Zhang, Hongbo
    Li, Yuchen
    Fu, Ting
    MATERIALS, 2024, 17 (10)
  • [14] Effects of Fly Ash/Slag Ratio and Liquid/Binder Ratio on Strength of Alkali-activated Fly Ash/Slag Mortars
    Chi, Maochieh
    Liu, Yenchun
    ADVANCES ON MATERIALS ENGINEERING, 2013, 377 : 50 - 54
  • [15] Effect of metakaolin on the autogenous shrinkage of alkali-activated slag-fly ash paste
    Li, Zhenming
    Liang, Xuhui
    Chen, Yun
    Ye, Guang
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 278
  • [16] Internal curing of alkali-activated slag-fly ash paste with superabsorbent polymers
    Li, Zhenming
    Zhang, Shizhe
    Liang, Xuhui
    Granja, Jose
    Azenha, Miguel
    Ye, Guang
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 263
  • [17] A mix design methodology of slag and fly ash-based alkali-activated paste
    Sun, Beibei
    Sun, Yubo
    Ye, Guang
    De Schutter, Geert
    CEMENT & CONCRETE COMPOSITES, 2022, 126
  • [18] Thermodynamic modeling of alkali-activated fly ash paste
    Chen, Yun
    Ma, Bin
    Chen, Jiayi
    Li, Zhenming
    Liang, Xuhui
    de Lima, Luiz Miranda
    Liu, Chen
    Yin, Suhong
    Yu, Qijun
    Lothenbach, Barbara
    Ye, Guang
    CEMENT AND CONCRETE RESEARCH, 2024, 186
  • [19] Leaching resistance of alkali-activated slag and fly ash mortars exposed to organic acid
    Li, Zihui
    Peethamparan, Sulapha
    GREEN MATERIALS, 2018, 6 (03) : 117 - 130
  • [20] Properties of ion leaching of alkali-activated blast furnace slag at early hydration
    Kang, Seungmin
    Bak, Sol-A
    Kim, Kyungnam
    Song, Myongshin
    ADVANCES IN CEMENT RESEARCH, 2016, 28 (03) : 151 - 157