Microstructure, mechanical property and bonding mechanism of SiC ceramic joint using a novel Y2Si2O7/Mullite glass-ceramic interlayer

被引:12
|
作者
Sun, Liangbo [1 ,2 ]
Wang, Shuohao [1 ]
Hou, Chuanmei [1 ]
Wang, Dongbao [1 ]
Liu, Chunfeng [1 ,2 ]
Zhang, Xinghong [3 ]
Zhang, Jie [1 ,2 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Ctr Anal Measurement & Comp, Harbin 150001, Peoples R China
[3] Harbin Inst Technol, Natl Key Lab Sci & Technol Adv Composites Special, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
SiC ceramic; Glass; -ceramic; Joining; Microstructure; Bonding mechanism; SILICON-CARBIDE; THERMAL-EXPANSION; CRYSTALLIZATION; IRRADIATION; FILLER;
D O I
10.1016/j.ceramint.2023.02.155
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Joining of SiC ceramics with a pre-oxidized or unoxidized surface and the subsequent mechanical properties have been studied using Y2O3-Al2O3-SiO2 glass bonding method, and the mechanism of interface bonding was revealed. The joining parameter of interest was temperature from 1400 degrees C to 1500 degrees C for a dwell time 10 min. The microstructure, compositions, and interfacial properties were characterized via electron microscopy and X-ray diffractometry. A multiphase glass-ceramic interlayer mainly consisting of Y2Si2O7 and mullite was formed in the joint, which possessed good thermal matching with the SiC substrate. Moreover, the softening temperature of glass-ceramic could exceed to 1200 degrees C. The joint obtained from the pre-oxidized SiC substrate exhibited a more reliable interface bonding than the unoxidized surface. A preferable shear strength of 48 MPa was achieved within 10 min at 1420 degrees C. The elemental diffusion at the interface and the chemical bonding between glass -ceramic and SiC contributed to a reliable SiC-SiC joint.
引用
收藏
页码:17885 / 17893
页数:9
相关论文
共 50 条
  • [31] Hot corrosion behaviour of the γ-Y2Si2O7 ceramic exposed to NaVO3 or V2O5 molten salt
    Fang, Bin
    Li, Yi
    Xu, Xi
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2023, 74 (08): : 1233 - 1245
  • [32] Microstructure and physico-mechanical properties of Al2O3-doped sustainable glass-ceramic foams
    da Costa, Fabiana Pereira
    da Silva Morais, Crislene Rodrigues
    Pinto, Haroldo Cavalcanti
    Rodrigues, Alisson Mendes
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 256
  • [33] Fabrication of Y2Si2O7 coating and its oxidation protection for C/SiC composites
    Ma, Qing-song
    Cai, Li-hui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (02) : 390 - 396
  • [34] Temperature-frequency dependence and mechanism of dielectric properties for γ-Y2Si2O7
    侯志灵
    曹茂盛
    袁杰
    宋维力
    Chinese Physics B, 2010, (01) : 510 - 514
  • [35] Helium bubbles in Gd2Ti2O7 borosilicate glass-ceramic composites
    Jiang, Menghan
    Mir, Anamul Haq
    Bahri, Mounib
    Zhang, Yingjie
    Browning, Nigel
    Whittle, Karl
    Patel, Maulik
    JOURNAL OF NUCLEAR MATERIALS, 2023, 581
  • [36] Temperature-frequency dependence and mechanism of dielectric properties for γ-Y2Si2O7
    Hou Zhi-Ling
    Cao Mao-Sheng
    Yuan Jie
    Song Wei-Li
    CHINESE PHYSICS B, 2010, 19 (01)
  • [37] A novel high reflective glass-ceramic ink with Bi2Ti2O7 nanocrystals used for the photovoltaic glass backplane
    Jiao, Jinxu
    Yang, Miao
    Li, Jingwei
    Xiong, Dehua
    Li, Hong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (08) : 3630 - 3636
  • [38] Microstructure and mechanical properties of a lithium disilicate glass-ceramic in the SiO2-Li2O-K2O-ZnO-P2O5 system
    Schweiger, M
    Cramer, SV
    Höland, W
    Rheinberger, V
    GLASS SCIENCE AND TECHNOLOGY-GLASTECHNISCHE BERICHTE, 2000, 73 : 20 - 27
  • [39] Fabrication and thermal shock resistance of multilayer γ-Y2Si2O7 environmental barrier coating on porous Si3N4 ceramic
    Wang, Chao
    Chen, Meng
    Wang, Hongjie
    Fan, Xingyu
    Xia, Hongyan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (03) : 689 - 695
  • [40] Microstructure and mechanical properties of transient liquid phase bonding Ti3SiC2 ceramic to SUS430 steel using an Al interlayer
    Zhao, Jing-xiang
    Li, Xi-chao
    Shi, Jing
    Cheng, Qiang
    Xu, Bin
    Sun, Ming-yue
    Zheng, Li-li
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2024, 31 (10) : 2475 - 2488