Investigation of transient processes of tritium release from biphasic lithium ceramics Li4SiO4-Li2TiO3 at negative neutron flux pulse

被引:5
|
作者
Kulsartov, Timur [1 ,2 ,3 ]
Shaimerdenov, Asset [4 ,5 ]
Zaurbekova, Zhanna [3 ,5 ]
Knitter, Regina [6 ]
Chikhray, Yevgen [2 ,5 ]
Askerbekov, Saulet [2 ,4 ]
Akhanov, Assyl [4 ]
Kenzhina, Inesh [1 ,4 ,7 ]
Aitkulov, Magzhan [4 ]
Sairanbayev, Darkhan [4 ]
Bugubay, Zhanar [4 ]
机构
[1] Satbayev Univ, Alma Ata, Kazakhstan
[2] Al Farabi Kazakh Natl Univ, IETP, Alma Ata, Kazakhstan
[3] Inst Atom Energy, Branch NNC RK, Kurchatov, Kazakhstan
[4] Inst Nucl Phys, Alma Ata, Kazakhstan
[5] Al Farabi Kazakh Natl Univ, Alma Ata, Kazakhstan
[6] Karlsruhe Inst Technol, Karlsruhe, Germany
[7] Kazakh Britain Tech Univ, Alma Ata, Kazakhstan
关键词
Biphasic lithium ceramic; Tritium; Helium; Neutron irradiation; Tritium release; LI4SIO4; PEBBLES; LI2TIO3-LI4SIO4; FABRICATION; BEHAVIOR;
D O I
10.1016/j.nme.2023.101489
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Biphasic lithium ceramics based on lithium orthosilicate Li4SiO4 and lithium metatitanate Li2TiO3 is one of the most promising materials for breeder blankets of future fusion reactors. One of the important issues of biphasic lithium ceramics application in the fusion reactor blanket is to determine the parameters and mechanisms of tritium transfer within and from the ceramics.This paper continues the analysis of irradiation experiments carried out at the WWR-K reactor (Almaty, Kazakhstan) with a sample of biphasic lithium ceramics Li4SiO4-Li2TiO3 (pebbles of lithium orthosilicate with 35 mol% lithium metatitanate with diameter 250--1250 & mu;m). The section of the experiment in which the reactor was temporarily shutdown for 1.5 h was investigated in detail. During this period of time the sample temperature rapidly decreased from 665 degrees C to 100 degrees C, generation of tritium and helium in the lithium ceramic sample ceased, but the desorption of previously generated gases from the ceramic surface continued.The experiments were carried out by the vacuum extraction method. The nature of tritium-containing molecules and helium release for that specified time interval was analyzed. The kinetics of tritium release from ceramics in the experiment during reactor shutdown was simulated and the expression for the effective diffusion coefficient D = 5e-11(m2/s)& BULL;exp(-20(kJ/mole)/RT) was determined. It was suggested that one the most realistic mechanisms for tritium release is the mechanism associated with both diffusion and desorption of tritium from the pebbles surface and release from the open pores of the pebble.This mode of the experiment made it possible to estimate the parameters of tritium release immediately after irradiation, which imitates the conditions of breeding blanket operation in the fusion reactor.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] Reaction Kinetics for the Synthesis of Li4SiO4 by Solid State Reaction from Li2SiO3 and Li2CO3 for Tritium Breeder
    Xiang, Maoqiao
    Zhang, Yingchun
    Zhang, Yun
    Liu, Wei
    Wang, Chaofu
    Yu, Yonghong
    JOURNAL OF FUSION ENERGY, 2016, 35 (04) : 652 - 659
  • [42] Reaction Kinetics for the Synthesis of Li4SiO4 by Solid State Reaction from Li2SiO3 and Li2CO3 for Tritium Breeder
    Maoqiao Xiang
    Yingchun Zhang
    Yun Zhang
    Wei Liu
    Chaofu Wang
    Yonghong Yu
    Journal of Fusion Energy, 2016, 35 : 652 - 659
  • [43] Thermal desorption of tritium and helium from lithium ceramics Li2TiO3+5mol% TiO2 after neutron irradiation
    Kulsartov, Timur
    Ponkratov, Yuriy
    Zaurbekova, Zhanna
    Gordienko, Yuriy
    Tazhibayeva, Irina
    Kenzhina, Inesh
    Samarkhanov, Kuanysh
    Tulubayev, Yevgeniy
    Shaimerdenov, Asset
    Udartsev, Sergey
    JOURNAL OF NUCLEAR MATERIALS, 2023, 585
  • [44] Effects of long-term high temperature annealing on Li2TiO3 and advanced core-shell Li2TiO3-Li4SiO4 tritium breeders
    Gu, Shouxi
    Ji, Baolong
    Wang, Chi
    Qi, Qiang
    Zhou, Hai-Shan
    Zhang, Yingchun
    Luo, Guang-Nan
    JOURNAL OF NUCLEAR MATERIALS, 2024, 590
  • [45] Correlation between tritium release and thermal annealing of damages in neutron-irradiated Li4SiO4
    Morimoto, Y
    Akahori, S
    Shimada, A
    Iguchi, K
    Okuno, K
    Nishikawa, M
    Munakata, K
    Baba, A
    Kawagoe, T
    Moriyama, H
    Kawamoto, K
    Okada, M
    FUSION TECHNOLOGY, 2001, 39 (02): : 634 - 638
  • [46] EFFECT OF WATER FORMATION REACTION ON TRITIUM RELEASE BEHAVIOR FROM Li4SiO4
    Yamasaki, H.
    Kashimura, K.
    Kanazawa, T.
    Katayama, K.
    Yamashita, N.
    Fukada, S.
    Nishikawa, M.
    FUSION SCIENCE AND TECHNOLOGY, 2011, 60 (03) : 1151 - 1154
  • [47] Competition of surface reactions of tritium release from irradiated Li4SiO4 pebbles
    Chunmei Kang
    Chengjian Xiao
    Xiaojun Chen
    Shuming Peng
    Xiaolin Wang
    Science China(Chemistry), 2015, 58 (05) : 839 - 844
  • [48] Competition of surface reactions of tritium release from irradiated Li4SiO4 pebbles
    Kang, Chunmei
    Xiao, Chengjian
    Chen, Xiaojun
    Peng, Shuming
    Wang, Xiaolin
    SCIENCE CHINA-CHEMISTRY, 2015, 58 (05) : 839 - 844
  • [49] Competition of surface reactions of tritium release from irradiated Li4SiO4 pebbles
    Chunmei Kang
    Chengjian Xiao
    Xiaojun Chen
    Shuming Peng
    Xiaolin Wang
    Science China Chemistry, 2015, 58 : 839 - 844
  • [50] Tritium release from Li4SiO4 ceramic pebbles in high magnetic field
    Ran, Guangming
    Xiao, Chengjian
    Chen, Xiaojun
    Gong, Yu
    Zhao, Linjie
    Wang, Xiaolin
    FUSION ENGINEERING AND DESIGN, 2015, 101 : 124 - 127