Excellent Energy Storage Performance of ZnO doped (Pb,La)(Zr,Sn,Ti)O3 Based Antiferroelectric Ceramics at an Ultra-Low Sintering Temperature of 940 degree celsius

被引:1
|
作者
Zhao, Han [1 ,2 ]
Xu, Ran [1 ,2 ]
Wang, Meng Jiao [1 ,2 ]
Wang, Gang [1 ,2 ]
Sun, Hong Chen [1 ,2 ]
Wang, Xiao Zhi [1 ,2 ]
Zhu, Qing Shan [1 ,2 ]
Wei, Xiao Yong [1 ,2 ]
Feng, Yu Jun [1 ,2 ]
Xu, Zhuo [1 ,2 ]
机构
[1] Xi An Jiao Tong Univ, Elect Mat Res Lab, Minist Educ, Xian 710049, Peoples R China
[2] Xi An Jiao Tong Univ, Int Ctr Dielect Res, Sch Elect & Informat Engn, Xian 710049, Peoples R China
关键词
(Pb; La); (Zr; Sn; Ti)O3-based; antiferroelectric; ceramics; sintering; temperature; Ultra-low; LEAD-ZIRCONATE-TITANATE; BREAKDOWN STRENGTH; DENSITY; EFFICIENCY; CUO;
D O I
10.1002/adfm.202316674
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
(Pb,La)(Zr,Sn,Ti)O-3-based antiferroelectric ceramics have excellent energy storage performance(more than 90% efficiency), which make them have great application advantages in the field of ceramic capacitors. However, the sintering temperature of (Pb,La)(Zr,Sn,Ti)O-3-based antiferroelectric ceramics is generally above 1250 degree celsius, which limits application as a material for ceramic capacitors. Cu inner electrode has a low co-firing temperature and high conductivity and a low cost price, making it more competitive in the field of ceramic capacitor inner electrode. Therefore, the first step is to reduce the sintering temperature of (Pb,La)(Zr,Sn,Ti)O-3-based ceramics to below 1000 degree celsius(co-firing temperature with Cu inner electrode), which is the key and difficult point. In this paper, Pb0.94La0.02Sr0.04(Zr0.45Sn0.47Ti0.08)(0.995)O-3(PLSZST) antiferroelectric ceramics are doped with ZnO, which effectively reduce the sintering temperature. Among them, PLSZST-1 wt% ZnO is sintered at an ultra-low sintering temperature (T-Sintering = 940 degree celsius), which is 330 degree celsius lower than that of PLSZST(T-Sintering = 1270 degree celsius) without doping ZnO. At the same time, PLSZST-1 wt%ZnO obtain a recoverable energy density of 4.26J cm(-3) and an energy efficiency of 95.5% at 230 kV cm(-1). The pulse discharge energy density (W-dis = 3.92 J cm(-3)) and discharge time (t(0.9) = 351 ns) are obtained at 220 kV cm(-1), and the current density (C-D = 1338A cm(-2)) and power density (P-D = 134MW cm(-3)) are obtained at 200 kV cm(-1). The results provide a possible material basis for Cu internal electrode ceramic capacitors.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Temperature Dependence of Energy Storage in Pb0.90La0.04Ba0.04[(Zr0.7Sn0.3)0.88Ti0.12]O3 Antiferroelectric Ceramics
    Xu, Ran
    Xu, Zhuo
    Feng, Yujun
    He, Hongliang
    Tian, Jingjing
    Huang, Dong
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2016, 99 (09) : 2984 - 2988
  • [42] High recoverable energy density over a wide temperature range in Sr modified (Pb,La)(Zr,Sn,Ti)O3 antiferroelectric ceramics with an orthorhombic phase
    Zhang, Qingfeng
    Tong, Huifen
    Chen, Jian
    Lu, Yinmei
    Yang, Tongqing
    Yao, Xi
    He, Yunbin
    APPLIED PHYSICS LETTERS, 2016, 109 (26)
  • [43] High energy density and efficiency in (Pb,La)(Zr,Sn,Ti)O3 antiferroelectric ceramics with high La3+ content and optimized Sn4+ content
    Yu, Yuxi
    Zhang, Yangyang
    Zou, Kailun
    Chen, Guang
    Zhang, Ying
    Li, Hao
    Lu, Yinmei
    Zhang, Qingfeng
    He, Yunbin
    CERAMICS INTERNATIONAL, 2019, 45 (18) : 24419 - 24424
  • [44] Enhancing energy storage performance in multilayer ceramic capacitors with (Pb,La)(Zr,Sn,Ti)O3-based antiferroelectric solid solutions
    Dou, Zhanming
    Yang, Ying
    Zhou, Lin
    Luo, Gengguang
    Li, Yuhong
    Hu, Jun
    Wang, Sixuan
    Wang, Wei
    Ruan, Shengjie
    Zhang, Guangzu
    Jiang, Shenglin
    Li, Kanghua
    APPLIED MATERIALS TODAY, 2024, 41
  • [45] Large Energy Density in Ba Doped Pb0.97La0.02(Zr0.65Sn0.3Ti0.05)O3 Antiferroelectric Ceramics with Improved Temperature Stability
    Zhang, Guangzu
    Liu, Pin
    Fan, Baoyan
    Liu, Huan
    Zeng, Yike
    Qiu, Shiyong
    Jiang, Shenglin
    Li, Qi
    Wang, Qing
    Liu, Jianguo
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2017, 24 (02) : 744 - 748
  • [46] Effects of glass additions on the dielectric properties and energy storage performance of Pb0.97La0.02(Zr0.56Sn0.35Ti0.09)O3 antiferroelectric ceramics
    Chen, Shengchen
    Yang, Tongqing
    Wang, Jinfei
    Yao, Xi
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2013, 24 (12) : 4764 - 4768
  • [47] Excellent Energy Storage and Charge-Discharge Performance in (Pb1-x Ca x )(Zr0.55Sn0.45)O3 Antiferroelectric Ceramics
    Yu, Chao
    Wang, Shibin
    Yan, Xuling
    Li, Weiqiu
    Yu, Yuliang
    Zhao, Xiaobo
    Yao, Yingbang
    Tao, Tao
    Liang, Bo
    Gong, Weiping
    Lu, Sheng-Guo
    ACS APPLIED MATERIALS & INTERFACES, 2025, 17 (03) : 5066 - 5077
  • [48] Effects of glass additions on the dielectric properties and energy storage performance of Pb0.97La0.02(Zr0.56Sn0.35Ti0.09)O3 antiferroelectric ceramics
    Shengchen Chen
    Tongqing Yang
    Jinfei Wang
    Xi Yao
    Journal of Materials Science: Materials in Electronics, 2013, 24 : 4764 - 4768
  • [49] Low temperature synthesis of (Pb,La)(Zr,Sn,Ti)O3 powders by citrate process
    Quanyong Guo
    Qiang Li
    Lihong Xue
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2007, 22 : 526 - 528
  • [50] Low Temperature Synthesis of (Pb,La)(Zr,Sn,Ti)O3 Powders by Citrate Process
    郭泉泳
    李强
    Journal of Wuhan University of Technology(Materials Science Edition), 2007, (03) : 526 - 528