Effects of heat treatment on the corrosion behavior and mechanical properties of aluminum alloy 2024

被引:14
|
作者
El Garchani, Fatima Ezzohra [1 ]
Lgaz, Hassane [2 ]
Kaya, Savas [3 ]
Lee, Han-Seung [4 ]
Ibrahim, Sobhy M. [5 ]
Chafiq, Maryam [6 ]
Ko, Young Gun [6 ]
Kabiri, Moulay Rachid [1 ]
机构
[1] Univ Moulay Ismail, Lab Energet Mat & Sustainable Dev, ENSAM, Meknes 50500, Morocco
[2] Hanyang Univ, Innovat Durable Bldg & Infrastructure Res Ctr, Ctr Creat Convergence Educ, ERICA, 55 Hanyangdaehak-ro, Sangrok-gu, Ansan 15588, Gyeonggi Do, South Korea
[3] Sivas Cumhuriyet Univ, Hlth Serv Vocat Sch, Dept Pharm, TR-58140 Sivas, Turkiye
[4] Hanyang Univ ERICA, Dept Architectural Engn, 55 Hanyangdaehak-ro, San-grok-gu, Ansan 15588, Gyeonggi Do, South Korea
[5] King Saud Univ, Coll Sci, Dept Biochem, PO B 2455, Riyadh 11451, Saudi Arabia
[6] Yeungnam Univ, Sch Mat Sci & Engn, Mat Electrochem Grp, Gyongsan 38541, South Korea
基金
新加坡国家研究基金会;
关键词
Aluminum alloy; Corrosion; Microstructure; AA2024; Heat treatment; Tensile test; AL-CU-MG; LOCALIZED CORROSION; AGING TREATMENT; PRECIPITATION; PARTICLES; FORMABILITY; MICROSTRUCTURE; FATIGUE; COMPLEX; PHASES;
D O I
10.1016/j.jmrt.2023.05.278
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Aluminum alloy, specifically 2024, is extensively utilized in the automotive and aerospace industries due to its light weight and superior mechanical properties. This study explores the corrosion behavior and mechanical characteristics of this alloy following quenching and aging heat treatments. Accelerated corrosion tests involved immersing samples in a salt spray chamber with a 5% NaCl solution, maintained at a temperature of 40 degrees C with a neutral pH. The alloy's microstructure and corrosion behavior were examined before and after the corrosion test, which included a heat treatment at 495 degrees C and aging for five days. Multiple tests, such as Vickers microhardness, optical microscopy, scanning electron microscopy (SEM), and tensile tests were performed. The surface characteristics, specifically the refined microstructure and residual stresses, were analyzed and their impact on localized corrosion was evaluated. The maximum strength value rose from 411 MPa to 512 MPa, and elongation increased correspondingly. Concerning corrosion sensitivity, a reduction was observed in the following order: AA2024-T3 (natural condition), AA2024-T3 (tempered condition), and AA2024-T3 (aged condition). The aged treatment appeared to enhance corrosion resistance, potentially due to the minimized size of corrosion products observed post-etching in various regions. (c) 2023 The Authors. Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:1355 / 1363
页数:9
相关论文
共 50 条
  • [41] Effect of Heat Treatment Parameters on Mechanical Properties of 5052 Aluminum Alloy
    Jia, Xiangdong
    Zhao, Yang
    Xu, Siqi
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (03): : 963 - 972
  • [42] Effects of cryorolling, room temperature rolling and aging treatment on mechanical and corrosion properties of 7050 aluminum alloy
    Xiong, Hanqing
    Zhou, Yuexin
    Yang, Peng
    Kong, Charlie
    Yu, Hailiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 853
  • [43] Effects of heat treatment on the microstructure and corrosion behavior of manganese aluminum bronzes
    Haubner, R.
    Strobl, S.
    Ball, G.
    Linhardt, P.
    Biezma, M. V.
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2024, 61 (9-10): : 769 - 782
  • [44] Effect of annealing treatment on the mechanical properties and corrosion behaviors of 01570 aluminum alloy
    Wang, X. H.
    Wang, J. H.
    Song, J.
    Fu, C. W.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2014, 65 (08): : 809 - 814
  • [45] Effect of heat treatment on the mechanical strength, intergranular and exfoliation corrosion of 7075 aluminum alloy
    Emerson Zavaleta-Gutierrez, Nilthon
    Rolando Polo-Briceno, Elmer
    Damian Nique-Gutierrez, Norberto
    De Cicco, Hernan
    MATERIA-RIO DE JANEIRO, 2018, 23 (02):
  • [46] Effects of aging treatment on corrosion properties of 1933 aluminum alloy forging
    Zhang, Yong
    Zhang, Xin-Ming
    Liu, Sheng-Dan
    Ou, Jun
    Xu, Min
    Zhong, Qi-Ming
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2011, 21 (07): : 1527 - 1534
  • [47] Effects of electropulsing frequency on mechanical properties, corrosion behavior and microstructure of a creep-aged 7050 aluminum alloy
    Dai, Hanfang
    Xu, Guofu
    Li, Yao
    Guo, Guangyi
    Peng, Xiaoyan
    MATERIALS CHARACTERIZATION, 2022, 194
  • [48] Deposition and corrosion behavior of silicate conversion coatings on aluminum alloy 2024
    Kazemi, M.
    Danaee, I.
    Zaarei, D.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2014, 45 (07) : 574 - 581
  • [49] Effect of surface burnishing on texture and corrosion behavior of 2024 aluminum alloy
    Lv Jinlong
    Luo Hongyun
    SURFACE & COATINGS TECHNOLOGY, 2013, 235 : 513 - 520
  • [50] Intergranular corrosion and mechanical property evolution in AA2024 alloy through heat treatment
    Fatima Ezzohra El Garchani
    Moulay Rachid Kabiri
    The International Journal of Advanced Manufacturing Technology, 2023, 128 : 3273 - 3282