Study on Fusion Zone Size, Pore Characteristics, and Mechanical Properties of 6063 Aluminum Alloy Cold Metal Transfer Mix plus Synchropulse Welded Joint

被引:0
|
作者
Huan, Peng-Cheng [1 ]
Wei, Xia [1 ,2 ]
Wang, Xiao-Nan [3 ]
Qi, Xiao-Nan [1 ]
Chen, Xia-Ming [3 ]
Chen, Wen-Gang [4 ]
Nagaumi, Hiromi [3 ]
Di, Hong-Shuang [1 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, State Key Lab Rolling & Automat, Shenyang 110819, Liaoning, Peoples R China
[2] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Anisotropy & Texture Mat, Shenyang 110819, Liaoning, Peoples R China
[3] Soochow Univ, Sch Iron & Steel, Suzhou 215002, Jiangsu, Peoples R China
[4] Southwest Forestry Univ, Sch Mech & Transportat, Kunming 650224, Yunnan, Peoples R China
基金
中国国家自然科学基金;
关键词
6063 aluminum alloy; cold metal transfer; mechanical properties; microstructure; pore characteristics; ARC; MICROSTRUCTURE; WIRE; PARAMETERS; STRENGTH; POROSITY;
D O I
10.1007/s11665-022-07741-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
ER5183 filler wire is used as filler metal for CMT MIX + Synchropulse welding of 6063 aluminum alloy sheets. The relationships among the fusion zone (FZ) size, pore characteristics, microstructure and mechanical properties are studied. The results show that the heat and convection intensity of the molten pool increase as the heat input increases, so that more base metal is melted and the weld width increases. The porosity and chain-like pores are closely related to the FZ size. The FZ size characteristic index (k) is established to predict the porosity and chain-like pores. The lower the k value is, the more difficult chain-like pores are to generate. Properly increasing the heat input eliminates the chain-like pores without aggravating the softening. The chain-like pores enormously reduce the effective load-bearing area of the FZ, which leads to the pretty poor mechanical properties of the FZ. Considering that the high porosity weakens the fatigue life, it is recommended to properly increase the heat input to improve the service performance of aluminum alloy welded joints on the premise that the full penetration welded joint has been obtained.
引用
收藏
页码:8892 / 8903
页数:12
相关论文
共 50 条
  • [31] Microstructure and mechanical properties of ADC12/6063-T6 aluminum alloy butt joint achieved by metal inert gas groove welding
    Wang, Ye
    Zhao, Mi
    Xu, Hongyu
    Hu, Maoliang
    Ji, Zesheng
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2019, 233 (10) : 2120 - 2124
  • [32] Multi-objective optimization of activated cold metal transfer welded AA 6063-MgAZ31B dissimilar alloy joint using Taguchi and particle swarm algorithm
    Bansal, Abhi
    Vettivel, S. C.
    Kumar, Mukesh
    MULTISCALE AND MULTIDISCIPLINARY MODELING EXPERIMENTS AND DESIGN, 2025, 8 (01)
  • [33] EFFECT OF CORROSION PROCESS ON MECHANICAL PROPERTIES AND ACOUSTIC EMISSION CHARACTERISTICS OF AL/ZINC-COATED STEEL WELDED BY COLD METAL TRANSFER
    Sriwongras, Piyapong
    Dostal, Petr
    MENDELNET 2015, 2015, : 539 - 544
  • [34] Microstructure and Mechanical Properties of Ti-6 Al-4V Alloy Joints Welded via the Cold Metal Transfer Method
    Gao, Fuyang
    Yan, Yangyang
    Song, Dejun
    Li, Yaozong
    Yang, Shengli
    Yu, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [35] Microstructure and Mechanical Properties Characteristics of 2319 Aluminum Alloy Fabricated Using Cold Metal Transfer Pulsed Advanced (CMT-PADV) Wire Arc Additive Manufacturing
    Bian, Wenzhuo
    Wang, Jun
    Li, Qianning
    Lu, Jiahao
    Fu, Kai
    Zhang, Liang
    Wang, Huixia
    METALS AND MATERIALS INTERNATIONAL, 2025,
  • [36] Mechanical and microstructural properties of robotic Cold Metal Transfer (CMT) welded 5083-H111 and 6082-T651 aluminum alloys
    Gungor, Beytullah
    Kaluc, Erdinc
    Taban, Emel
    Sik, Aydin S. S.
    MATERIALS & DESIGN, 2014, 54 : 207 - 211
  • [37] Microstructure and mechanical properties of 2060 Al-Li alloy welded by alternating current cold metal transfer with high-frequency pulse current
    Wang, Liwei
    Hu, Huan
    Yan, Huan
    Liu, Ying
    Wu, Ziqin
    Narayanaswamy, Balaji
    Liang, Zhimin
    Wang, Dianlong
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2021, 40 (01) : 214 - 227
  • [38] Effect of wire current on microstructure and properties of 7075-T6 aluminum alloy joint welded by double-wire pulsed cold metal transition method
    Zhang Z.
    Li X.
    Zhu D.
    Qu S.
    Wang X.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2022, 43 (11): : 68 - 77
  • [39] Joint Characteristics and Corrosion Properties of Bypass-Current Double-Sided Arc-Welded Aluminum 6061 Alloy with Al–Si Filler Metal
    Yu-Gang Miao
    Ben-Shun Zhang
    Bin-Tao Wu
    Xiao-Xiao Wang
    Guang-Yu Chen
    Duan-Feng Han
    Acta Metallurgica Sinica (English Letters), 2016, 29 : 360 - 366
  • [40] Joint Characteristics and Corrosion Properties of Bypass-Current Double-Sided Arc-Welded Aluminum 6061 Alloy with Al–Si Filler Metal
    Yu-Gang Miao
    Ben-Shun Zhang
    Bin-Tao Wu
    Xiao-Xiao Wang
    Guang-Yu Chen
    Duan-Feng Han
    ActaMetallurgicaSinica(EnglishLetters), 2016, 29 (04) : 360 - 366