Mechanical Properties of Five Esthetic Ceramic Materials Used for Monolithic Restorations: A Comparative In Vitro Study

被引:3
|
作者
Almohammed, Saleh N. [1 ]
Alshorman, Belal [1 ]
Abu-Naba'a, Layla A. [1 ]
机构
[1] Jordan Univ Sci & Technol, Fac Dent, Dept Prosthodont, Irbid 22110, Jordan
来源
CERAMICS-SWITZERLAND | 2023年 / 6卷 / 02期
关键词
aging; brittleness; flexural strength; hardness; lithium disilicate; mechanical properties; monolithic; polymer-infiltrated ceramic; toughness; zirconia; TETRAGONAL ZIRCONIA POLYCRYSTAL; LOW-TEMPERATURE DEGRADATION; BIAXIAL FLEXURAL STRENGTH; Y-TZP CERAMICS; FRACTURE-TOUGHNESS; HIGHLY-TRANSLUCENT; OPTICAL-PROPERTIES; DENTAL CERAMICS; FATIGUE; MICROSTRUCTURE;
D O I
10.3390/ceramics6020061
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Monolithic zirconia and hybrid ceramic restorations have been widely used in the last decade for both anterior and posterior dental restorations. However, their use lacks sufficient scientific evidence in most cases, as the expeditious manufacturing of these versatile ceramic materials exceeds the limits of in vitro and/or in vivo validation. This study aimed to evaluate and compare the mechanical properties (flexural strength, fracture toughness, Vickers hardness, and brittleness index) of three CAD-CAM monolithic multilayer zirconia ceramics (GNX-Ceramill Zolid(& REG;) Gen-X, ZCP-IPS e.max(& REG;) ZirCAD, and UPC-Upcera(& REG;) Esthetic Explore Prime) and one CAD-CAM monolithic multilayer polymer-infiltrated hybrid ceramic (ENM-Vita(& REG;) Enamic) with a CAD-CAM monolithic lithium disilicate ceramic as a control (EMX -IPS e.max(& REG;) CAD). A total of 160 discs (GNX = 32, ZCP = 32, UPC = 32, ENM = 32, and EMX = 32) were cut, polished, and fully sintered (except for the ENM). Half of the samples for each group were subjected to hydrothermal aging. Descriptive analysis and ANOVA tests were used to compare the groups. The zirconia groups showed significantly higher mechanical properties than the EMX group for both the non-aged and aged samples (p < 0.05). The ENM group showed the lowest brittleness index, while EMX showed the highest. The mechanical properties of monolithic multilayer zirconia ceramics were generally better than those of monolithic multilayer polymer-infiltrated hybrid ceramic and lithium disilicate ceramic. All groups showed, to some extent, a change in their mechanical properties after aging, with the ENM being the most affected.
引用
收藏
页码:1031 / 1049
页数:19
相关论文
共 50 条
  • [21] Influence of shading technique on mechanical fatigue performance and optical properties of a 4Y-TZP ceramic for monolithic restorations
    Auzani, Maria Luiza
    Dapieve, Kiara Serafini
    Zucuni, Camila Pauleski
    Rocha Pereira, Gabriel Kalil
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 102
  • [22] In Vitro Study of the Action of Coconut Water and Sugarcane Juice on the Surface of Esthetic Restorations
    de Lima, Aline Lins
    Valenca, Ana Maria Gondim
    de Lima, Severino Jackson Guedes
    de Alexandria, Adilis Kalina Felix
    Claudino, Ligia Viera
    da Silva, Naiana Braga
    PESQUISA BRASILEIRA EM ODONTOPEDIATRIA E CLINICA INTEGRADA, 2007, 7 (01): : 43 - 50
  • [23] A novel customized ceramic bracket for esthetic orthodontics: in vitro study
    Yang, Liu
    Yin, Guangfu
    Liao, Xiaoming
    Yin, Xing
    Ye, Niansong
    PROGRESS IN ORTHODONTICS, 2019, 20 (01)
  • [24] Investigation of the Influence of Gastric Acid on the Surface Roughness of Ceramic Materials of Metal-Ceramic Restorations. An In Vitro Study
    Matsou, Eirini
    Vouroutzis, Nikolaos
    Kontonasaki, Eleana
    Paraskevopoulos, Konstantinos M.
    Koidis, Petros
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2011, 24 (01) : 26 - 29
  • [25] A novel customized ceramic bracket for esthetic orthodontics: in vitro study
    Liu Yang
    Guangfu Yin
    Xiaoming Liao
    Xing Yin
    Niansong Ye
    Progress in Orthodontics, 20
  • [26] Retention of luting agents used for implant-supported restorations: A comparative In-Vitro study
    Aladag, A.
    Sahan, M. H.
    Akkus, N. O.
    Aktas, R.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2020, 23 (08) : 1073 - 1078
  • [27] Alterations in the mechanical properties of the extracted human teeth to be used as biological restorations on storing them in different storage media: an in vitro study
    Kantoor, Pallavi
    Srivastava, Nikhil
    Rana, Vivek
    Adlakha, Vivek K.
    DENTAL TRAUMATOLOGY, 2015, 31 (04) : 308 - 313
  • [28] Optical properties of currently used zirconia-based esthetic restorations fabricated with different techniques
    Turgut, Sedanur
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2020, 32 (01) : 26 - 33
  • [29] Comparative study of hygrothermal properties of five thermal insulation materials
    Ducoulombier, Laure
    Lafhaj, Zoubeir
    CASE STUDIES IN THERMAL ENGINEERING, 2017, 10 : 628 - 640
  • [30] Monolithic Zirconia Partial Coverage Restorations: An In Vitro Mastication Simulation Study
    Gupta, Savita
    Abdulmajeed, Awab
    Donovan, Terry
    Boushell, Lee
    Bencharit, Sompop
    Sulaiman, Taiseer A.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2021, 30 (01): : 76 - 82