The effect of repair protocols and chewing simulation on the microtensile bond strength of two resin matrix ceramics to composite resin

被引:2
|
作者
Elkassaby, Annan Ahmed [1 ]
Kandil, Mohamed M. [1 ]
Alian, Ghada Atef [1 ]
机构
[1] Ain Shams Univ, Dept Dent Biomat Dent, Cairo, Egypt
关键词
Polymer infiltrated ceramic network; Resin nanoceramics; Cyclic loading; Artificial aging; Mechanical fatigue; Mechanical aging; SURFACE TREATMENTS; CAD/CAM MATERIALS; BLOCKS; CEMENT;
D O I
10.1186/s12903-024-03932-4
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Background To assess the micro tensile bond strength (mu TBS) of two resin matrix ceramic (RMC) blocks bonded to composite resin by using different repair protocols with and without chewing simulation (CS). Materials and methods Two resin matrix ceramic blocks (Vita Enamic and Lava Ultimate) were divided into 4 groups according to the surface treatments: Bur grinding (control), Bur grinding + silane, 9.5% HF acid etching, and 9.5% HF acid etching + silane. The single bond universal adhesive was applied on all specimens after the surface treatments according to the manufacturer's instructions, it was administered actively on the treated surface for 20 s and then light cured for 10 s, followed by incremental packing of composite resin to the treated surface. Each group was further divided into 2 subgroups (with/without chewing simulation for 500,000 cycles). A micro tensile bond strength test was performed for each group (n = 15). The effect of surface treatments on the materials was examined by using a scanning electron microscope (SEM). The micro tensile bond strength (MPa) data were analyzed with a three-way ANOVA, the independent t-test, and one-way ANOVA followed by the Tukey post-hoc test. Results mu TBS results were significantly higher for Lava Ultimate than Vita Enamic for all the surface treatment protocols with (p < 0.01). The chewing simulation significantly negatively affected the micro-tensile bond strength (p < 0.001). Bur grinding + saline exhibited the highest bond strength values for Lava Ultimate, both with and without chewing simulation. For Vita Enamic, bur grinding + saline and HF acid + saline showed significantly higher bond strength values compared to other surface treatments, both with and without chewing simulation (p <= 0.05). Conclusion Bur grinding + silane could be recommended as a durable repair protocol for indirect resin matrix ceramics blocks with composite resin material.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] Effect of Different Surface Treatments on Repair Bond Strength of CAD/CAM Resin-Matrix Ceramics
    Arkoy, Semih
    Ulusoy, Mutahhar
    MATERIALS, 2022, 15 (18)
  • [22] Effect of preheating of low shrinking resin composite on intrapulpal temperature and microtensile bond strength to dentin
    El-Deeb, Heba A.
    El-Aziz, Sara Abd
    Mobarak, Enas H.
    JOURNAL OF ADVANCED RESEARCH, 2015, 6 (03) : 471 - 478
  • [23] Influence of surface treatments and adhesive protocols on repair bond strength of glass-matrix and resin-matrix CAD/CAM ceramics
    Turunc-Oguzman, Rana
    Sismanoglu, Soner
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2023, 35 (08) : 1322 - 1331
  • [24] EFFECT OF DEPROTEINIZATION AND TUBULAR OCCLUSION ON MICROTENSILE BOND STRENGTH AND MARGINAL MICROLEAKAGE OF RESIN COMPOSITE RESTORATIONS
    Baseggio, Wagner
    Consolmagno, Elaine Cristina
    Negreiros de Carvalho, Flavia Lunardelli
    Ueda, Julio Katuhide
    Schmitt, Vera Lucia
    Formighieri, Luis Alberto
    Naufel, Fabiana Scarparo
    JOURNAL OF APPLIED ORAL SCIENCE, 2009, 17 (05) : 462 - 466
  • [25] Effect of filler content on the microtensile bond strength of composite resin and dentin in Class I cavities
    Han, Bing
    Dong, Yanmei
    Gao, Xuejun
    Wang, Xiaoyan
    Tian, Fucong
    QUINTESSENCE INTERNATIONAL, 2012, 43 (02): : E16 - E22
  • [26] Effectiveness of indirect composite resin silanization evaluated by microtensile bond strength test
    Honda, Mauro Itaru
    Florio, Flavia Martao
    Basting, Roberta Tarkany
    AMERICAN JOURNAL OF DENTISTRY, 2008, 21 (03): : 153 - 158
  • [27] Microtensile Bond Strength Between Resin-Matrix CAD/CAM Ceramics and Resin Cement after Various Surface Modifications and Artificial Aging
    Papadopoulos, Constantinos
    Dionysopoulos, Dimitrios
    Pahinis, Kimon
    Koulaouzidou, Elisabeth
    Tolidis, Kosmas
    JOURNAL OF ADHESIVE DENTISTRY, 2021, 23 (03): : 255 - 265
  • [28] Repair Bond Strength of Composite Resin to Aged Resin and Glass-Matrix CAD/CAM Ceramic Materials Using Two Different Repair Systems
    Alnafaiy, Sarah
    Labban, Nawaf
    Maawadh, Ahmed
    Alshehri, Huda
    Albaijan, Refal
    COATINGS, 2021, 11 (11)
  • [29] Microtensile Bond Strength of Self-Adhesive Resin Cements to CAD/CAM Resin-Matrix Ceramics Prepared with Different Surface Treatments
    Bayazit, Elif Ozturk
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2019, 32 (05) : 433 - 438
  • [30] MICROTENSILE BOND STRENGTH EVALUATION OF RESIN COMPOSITE REPAIRED USING UNIVERSAL ADHESIVES
    Alkatheeri, Mohammad S.
    Almazyad, Nawaf
    Almegbel, Bandar
    Alrowaily, Fawaz
    Fakeeha, Iyad
    Aljarbou, Fahd
    Alayad, Abdullah
    INTERNATIONAL JOURNAL OF MEDICAL DENTISTRY, 2020, 24 (01) : 9 - 15