Mechanical properties and microstructure of nano-modified geopolymer concrete containing hybrid fibers after exposure to elevated temperature

被引:31
|
作者
Zhang, Peng [1 ]
Sun, Yaowen [1 ]
Wu, Jingjiang [2 ]
Hong, Jian [2 ]
Gao, Zhen [1 ]
机构
[1] Zhengzhou Univ, Sch Water Conservancy & Transportat, Zhengzhou 450001, Peoples R China
[2] Commun Construct Co CSCEC 7th Div Co Ltd, Zhengzhou 450004, Peoples R China
基金
中国国家自然科学基金;
关键词
Geopolymer concrete; Elevated temperature; Mechanical properties; Ultrasonic test; Microstructure; FLY-ASH-GEOPOLYMER; STRENGTH; RESISTANCE; SILICA; BOND;
D O I
10.1016/j.conbuildmat.2023.134044
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Geopolymer concrete (GPC) has a promising future as an eco-friendly material for refractory engineering applications. It is significant to investigate the changes in mechanical properties of nano-modified geopolymer concrete containing hybrid fibers (NHF-GPC) after exposure to elevated temperature for construction fireresistant design. In this study, the macro-mechanical property tests and micro tests were carried out on geopolymer concrete containing hybrid fibers with different nano-SiO2 (NS) contents (0-2 %) after exposure to different elevated temperatures (200-800 degrees C). The coupling relationships of compressive, tensile and flexural strengths of NHF-GPC with temperature and NS content were established separately. And the relative sound velocity and damage degree were selected as acoustic parameters to construct a relationship model with the compressive strength loss rate. The results indicated that the compressive, tensile and flexural strengths of NHFGPC were enhanced at 200 degrees C, while higher temperatures significantly reduced the mechanical properties of NHF-GPC. At the same temperature, the compressive, tensile and flexural strengths of NHF-GPC all increased and then decreased with increasing NS content, and reached the peak at a NS content of 1.5 %. The matrix became denser at 200 degrees C, while at greater than 200 degrees C, the water evaporated, the number of microcracks increased abruptly, and the porosity enlarged. The mass loss of NHF-GPC after elevated temperature mainly occurred below 600 degrees C, when there was no new material phase generated inside the matrix. And the established model can be used for the identification on the strength damage degree after elevated temperature exposure of NHF-GPC, and it can offer a conceptual foundation for the assessment of elevated temperature damage and the life prediction of GPC in the practical applications.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Effects of Liquid Nitrogen Cooling on the Microstructure Properties of Nano-Modified Concrete Under Hot Conditions
    Kattoof, Iman
    Hassan, Maan S.
    Hasan, Shatha S.
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2022, 47 (10) : 12569 - 12583
  • [22] Effects of Liquid Nitrogen Cooling on the Microstructure Properties of Nano-Modified Concrete Under Hot Conditions
    Iman Kattoof
    Maan S. Hassan
    Shatha S. Hasan
    Arabian Journal for Science and Engineering, 2022, 47 : 12569 - 12583
  • [23] Mechanical Properties of Lightweight Oil Palm Geopolymer Concrete under Elevated Temperature
    Ibrahim, H. A.
    Sultan, H. K.
    INTERNATIONAL JOURNAL OF ENGINEERING, 2025, 38 (03): : 661 - 669
  • [24] Durability and Mechanical Properties of Granulated Blast Furnace Slag Based Geopolymer Concrete Containing Polyolefin Fibers and Nano Silica
    Mohammadhossein Mansourghanaei
    Morteza Biklaryan
    Alireza Mardookhpour
    KSCE Journal of Civil Engineering, 2024, 28 : 209 - 219
  • [25] Durability and Mechanical Properties of Granulated Blast Furnace Slag Based Geopolymer Concrete Containing Polyolefin Fibers and Nano Silica
    Mansourghanaei, Mohammadhossein
    Biklaryan, Morteza
    Mardookhpour, Alireza
    KSCE JOURNAL OF CIVIL ENGINEERING, 2024, 28 (01) : 209 - 219
  • [26] The mechanical and durability properties of concrete containing hybrid synthetic fibers
    Sadrinejad, Iman
    Madandoust, Rahmat
    Ranjbar, Malek Mohammad
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 178 : 72 - 82
  • [27] Effect of elevated temperature on the mechanical properties and microstructure of heavy-weight magnetite concrete with steel fibers
    Thomas, C.
    Rico, J.
    Tamayo, P.
    Ballester, F.
    Setien, J.
    Polanco, J. A.
    CEMENT & CONCRETE COMPOSITES, 2019, 103 : 80 - 88
  • [28] Mechanical Performance of Steel-PVA Hybrid Fiber Concrete After Elevated Temperature Exposure
    Xiao, Liangli
    Yan, Huiling
    Zhu, Zhiying
    Xu, Chengxiang
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2024,
  • [29] Review on Mechanical Properties of Fiber-Reinforced Geopolymer Concrete After High-Temperature Exposure
    Chen, Pang
    Li, Yunhe
    Yin, Liang
    Wang, Zhixin
    IRANIAN JOURNAL OF SCIENCE AND TECHNOLOGY-TRANSACTIONS OF CIVIL ENGINEERING, 2024, 48 (6) : 3829 - 3851
  • [30] Bond performance between FRP bars and geopolymer concrete after elevated temperature exposure
    Zhao, Jun
    Wang, Shuaibin
    Wang, Zike
    Wang, Kang
    Fu, Chunhao
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 384