Construction of Microporous Zincophilic Interface for Stable Zn Anode

被引:2
|
作者
Yang, Xin [1 ]
Shu, Tie [1 ]
Huang, Haoyu [2 ]
Yi, Hongquan [2 ]
Zhang, Yanchi [2 ]
Xiao, Wei [2 ]
Li, Liang [3 ]
Zhang, Yuxin [4 ]
Ma, Minghao [5 ]
Liu, Xingyuan [6 ]
Yao, Kexin [7 ]
机构
[1] Chongqing Univ, Sch Chem & Chem Engn, Chongqing 400044, Peoples R China
[2] Chongqing Univ, Undergraduate Sch, Chongqing 400044, Peoples R China
[3] Sorbonne Univ Abu Dhabi, Dept Sci & Engn, POB 38044, Abu Dhabi, U Arab Emirates
[4] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
[5] HSXJTU, Hang Tian Sch, Xian 710043, Peoples R China
[6] Chongqing Joint Sch Famous Sch, Chongqing 400030, Peoples R China
[7] Chongqing Univ, Inst Adv Interdisciplinary Studies, Multiscale Porous Mat Ctr, Sch Chem & Chem Engn,State Key Lab Coal Mine Disas, Chongqing 400044, Peoples R China
来源
MOLECULES | 2023年 / 28卷 / 12期
关键词
aqueous zinc ion batteries; MOFs; anode; dendrite growth; ZINC ANODE; PERFORMANCE; CHALLENGES; DESIGN; CARBON;
D O I
10.3390/molecules28124789
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Aqueous zinc ion batteries (AZIBs) are promising electrochemical energy storage devices due to their high theoretical specific capacity, low cost, and environmental friendliness. However, uncontrolled dendrite growth poses a serious threat to the reversibility of Zn plating/stripping, which impacts the stability of batteries. Therefore, controlling the disordered dendrite growth remains a considerable challenge in the development of AZIBs. Herein, a ZIF-8-derived ZnO/C/N composite (ZOCC) interface layer was constructed on the surface of the Zn anode. The homogeneous distribution of zincophilic ZnO and the N element in the ZOCC facilitates directional Zn deposition on the (002) crystal plane. Moreover, the conductive skeleton with a microporous structure accelerates Zn2+ transport kinetics, resulting in a reduction in polarization. As a result, the stability and electrochemical properties of AZIBs are improved. Specifically, the ZOCC@Zn symmetric cell sustains over 1150 h at 0.5 mA cm(-2) with 0.25 mA h cm(-2), while the ZOCC@Zn half-cell achieves an outstanding Coulombic efficiency of 99.79% over 2000 cycles. This work provides a simple and effective strategy for improving the lifespan of AZIBs.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] A Hydrophobic and Zincophilic Interfacial Nanofilm as a Protective Layer for Stable Zn Anodes
    Duan, Fengxue
    Yin, Xiuxiu
    Ba, Junjie
    Li, Junpeng
    Yu, Yue
    Wang, Chunyu
    Wei, Yingjin
    Wang, Yizhan
    ADVANCED FUNCTIONAL MATERIALS, 2024, 34 (10)
  • [22] Synergistically regulating Zn-ion flux and accelerating ion transport kinetics via zincophilic covalent organic framework interlayer for stable Zn metal anode
    Liang, Liping
    Su, Long
    Zhang, Xiao
    Wang, Yuanqi
    Ren, Weirong
    Gao, Xinpei
    Zheng, Liqiang
    Lu, Fei
    CHEMICAL ENGINEERING JOURNAL, 2024, 485
  • [23] A novel hydrophobic-zincophilic bifunctional layer for stable Zn metal anodes
    Zhou, Xuan
    Chen, Renpeng
    Cui, Enhui
    Liu, Qin
    Zhang, Hong
    Deng, Jiahui
    Zhang, Nannan
    Xie, Can
    Xu, Lin
    Mai, Liqiang
    ENERGY STORAGE MATERIALS, 2023, 55 : 538 - 545
  • [24] Constructing robust zincophilic-channels on Zn anode for long-life Zn-ion batteries
    Kim, Soochan
    Hwang, Uiseok
    Yang, Kaiwei
    Cho, Misuk
    Nam, Jae-Do
    Lee, Youngkwan
    CHEMICAL ENGINEERING JOURNAL, 2022, 440
  • [25] Dynamic reconstruction of Ni-Zn alloy solid-electrolyte interface for highly stable Zn anode
    Qian Zhang
    Yuhang Dai
    Kangning Zhao
    Chengyi Zhang
    Ruihu Lu
    Jinghao Li
    Shuhan Jin
    Lei Zhang
    Qinyou An
    Liqiang Mai
    Nano Research, 2023, 16 : 11604 - 11611
  • [26] Achieving stable Zn metal anode via a hydrophobic and Zn2+-conductive amorphous carbon interface
    Li, Lianrui
    Zhang, Yan
    Du, Changlong
    Zhou, Xueqing
    Xiong, Hualin
    Wang, Guizhen
    Lu, Xihong
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2024, 657 : 644 - 652
  • [27] Robust zincophilic-hydrophobic protection layer induces preferential growth of (002) crystal plane towards ultra-stable Zn anode
    Gou, Lei
    Liang, Kai
    Wang, Wei
    Yang, Zheqi
    Zhu, Lin
    Ma, Yue
    Li, Hui
    Zhang, Zizhuo
    Fan, Xiao-Yong
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2025, 686 : 764 - 775
  • [28] Dynamic reconstruction of Ni-Zn alloy solid-electrolyte interface for highly stable Zn anode
    Zhang, Qian
    Dai, Yuhang
    Zhao, Kangning
    Zhang, Chengyi
    Lu, Ruihu
    Li, Jinghao
    Jin, Shuhan
    Zhang, Lei
    An, Qinyou
    Mai, Liqiang
    NANO RESEARCH, 2023, 16 (09) : 11604 - 11611
  • [29] Engineering zincophilic sites on Zn surface via plant extract additives for dendrite-free Zn anode
    Zhang, Lei
    Miao, Licheng
    Xin, Wenli
    Peng, Huiling
    Yan, Zichao
    Zhu, Zhiqiang
    ENERGY STORAGE MATERIALS, 2022, 44 : 408 - 415
  • [30] Biomacromolecule guiding construction of effective interface layer for ultra-stable zinc anode
    Yang, Jiaqi
    Qiu, Meijia
    Zhu, Mengni
    Weng, Chaocang
    Li, Yue
    Sun, Peng
    Mai, Wenjie
    Xu, Min
    Pan, Likun
    Li, Jinliang
    ENERGY STORAGE MATERIALS, 2024, 67