Innovative prevention of stress corrosion crack propagation in nuclear power pipe welds

被引:0
|
作者
Kong, Xiaofei [2 ,3 ]
Wang, Xin [2 ,3 ]
Lin, Bingchi [2 ,3 ]
Xiong, Zhiliang [2 ,3 ]
Deng, Xiaoyun [2 ,3 ]
Li, Xiao [1 ]
Lu, Yongxin [1 ]
机构
[1] Xian Shiyou Univ, Sch Mat Sci & Engn, Xian 710065, Peoples R China
[2] State Key Lab Nucl Power Safety Technol & Equipmen, Shenzhen, Peoples R China
[3] China Nucl Power Engn Co Ltd, Shenzhen, Peoples R China
关键词
contour method; finite element method; residual stress; welded joint; FINITE-ELEMENT-ANALYSIS; RESIDUAL-STRESS; NUMERICAL-SIMULATION; REPAIR; MICROSTRUCTURE; BEHAVIOR; JOINTS;
D O I
10.1515/mt-2023-0153
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Failure caused by stress corrosion cracking (SCC) is inevitable during the long-term service of nuclear power pipe welds. This is mainly due to the propagation of microcracks in the deposited metal, which seriously affects the operation safety of nuclear power pressure pipes. Overlay welding is practical for pressure pipe repair welding, which can introduce compressive residual stress inside the weld seam. In this work, a diagonal T-pipe joint was fabricated using tungsten inert gas arc welding with ERRS-3 wire, and an overlay weld was also fabricated using tungsten inert gas arc welding with ERRS-3 wire under circumstances of water in the pipe and no water in the pipe. And then the contour method and finite element method were employed to measure and calculate the residual stress distribution in the diagonal T-pipe joint. Both results showed that overlay welding can introduce compressive residual stresses into the pipe joint. The compressive residual stress zone area inside the weld seam with water in the pipe is larger than that without water in the pipe, and the compressive residual stress zone area varies at different positions of the weld seam. This work is expected to promote the application of overlay weld technology in the diagonal T-shaped pipe joint repair and prevent stress corrosion crack propagation of nuclear power pipe welds.
引用
收藏
页码:1145 / 1154
页数:10
相关论文
共 50 条
  • [11] SURFACE MORPHOLOGIES OF CRACK DURING STRESS CORROSION CRACK PROPAGATION.
    Chu, Youngchang
    Yang Dazhuang
    Key Engineering Materials, 1987, 20-28 (pt 1-4)
  • [12] State of the art of stress corrosion cracking of welds in nuclear environments
    Hoffmeister, H.
    Welding in the World, 2008, 52 (SPEC. ISS.) : 491 - 498
  • [13] Thermomechanical Manipulation of Crack-Tip Stress Field for Resistance to Stress Corrosion Crack Propagation
    Singh Raman, R. K.
    Ibrahim, R. N.
    Wu, F.
    Rihan, R.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (13): : 3217 - 3223
  • [14] Thermomechanical Manipulation of Crack-Tip Stress Field for Resistance to Stress Corrosion Crack Propagation
    R.K. Singh Raman
    R.N. Ibrahim
    F. Wu
    R. Rihan
    Metallurgical and Materials Transactions A, 2008, 39 : 3217 - 3223
  • [15] Influence of stress ratio on fatigue crack propagation behavior of stainless steel welds
    Kusko, CS
    Dupont, JN
    Marder, AR
    WELDING JOURNAL, 2004, 83 (02) : 59S - 64S
  • [16] Stress corrosion crack propagation affected by microstructures for nuclear steam turbine rotor steels in the simulated environment
    Weng, Shuo
    Huang, Yuhui
    Lin, Shuxian
    Xuan, Fu-Zhen
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 : 725 - 742
  • [17] AE response of α-brass during stress corrosion crack propagation
    Lapitz, P.
    Ruzzante, J.
    Alvarez, M. G.
    CORROSION SCIENCE, 2007, 49 (10) : 3812 - 3825
  • [18] PLANE OF CRACK PROPAGATION IN STRESS CORROSION FRACTURE IN COPPER BERYLLIUM
    SYLWESTROWICZ, WD
    CORROSION, 1970, 26 (12) : 552 - +
  • [19] STRESS-CORROSION AND CRACK-PROPAGATION IN SIOUX QUARTZITE
    PECK, L
    JOURNAL OF GEOPHYSICAL RESEARCH, 1983, 88 (NB6): : 5037 - 5046
  • [20] Effect of strain rate and potential on the propagation of stress corrosion crack
    Niu, L
    Zhang, CQ
    Lin, HC
    ACTA PHYSICO-CHIMICA SINICA, 2003, 19 (07) : 616 - 620