Built-up edge formation and flank wear evolution in conventional machining of AZ91 magnesium alloy

被引:2
|
作者
Alshibi, Assem [1 ]
Nasreldin, Abdelrahman [1 ]
Pervaiz, Salman [1 ]
机构
[1] Rochester Inst Technol, Dept Mech & Ind Engn, Dubai Campus,Techno Point Bldg,POB 341055, Dubai, U Arab Emirates
关键词
Orthogonal cutting; orthogonal turning; AZ91; magnesium alloy; tool wear; built-up edge; built-up layer; adhesion; TOOL WEAR; TICN; DRY; TIN; OPTIMIZATION; TEMPERATURE; COATINGS; LAYER;
D O I
10.1177/09544089231163120
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Magnesium alloys are largely desirable in numerous industries today because of their intrinsically attractive properties. Low density and high strength coupled with significant biocompatibility are the main advantages. Machining of magnesium alloys is challenging as a result of the persistent chip ignition risk as well as material build-up on the tool due to their softness. Therefore, magnesium alloys' machinability has not been fully assessed in the available literature. The present work aims to address this aperture by assessing flank wear progression and the prevalence of adhesion-driven built-up edge (BUE) and built-up layer (BUL) in different tool coating materials during the dry short-interval conventional orthogonal turning of AZ91 magnesium alloy. A higher and lower combination of feed rates and cutting speeds were utilized for all tools to compare the possible range of maximum flank wear land width, average flank wear land width, and chip contact length while capturing and assessing said parameters through digital and optical microscopy. The data presented a large prevalence of adhesion wear across all tool coating types which is portrayed by the cyclic behaviour of the flank wear land width plots, which resulted from the repeated accumulation and wear of deposited workpiece material. The TiCN-coated tool presented the least amounts of BUL and BUE throughout both levels of testing, while the TiN-coated tool presented the largest amounts of average flank wear land width due to recurrent aberrative local deposition accumulation and extended streak line depositions. TiN-coated, Al2O3-coated, and uncoated tools presented higher average flank wear land width than the TiCN-coated tool by 8.5%, 3.1%, and 27.2% during level 1 cutting conditions and 84.8%, 21.3%, and 37.2% during level 2 cutting conditions. This implies the TiCN coating's increased resistance to elevated cutting temperatures, and in turn, reduced deposition of material through adhesion.
引用
收藏
页码:2486 / 2497
页数:12
相关论文
共 50 条
  • [31] MICROSTRUCTURAL CHARACTERIZATION AND WEAR BEHAVIOR OF WC-CoCr COATING ON AZ91 MAGNESIUM ALLOY
    Buchtik, Martin
    Masilko, Jiri
    Vyklicky, Ondrej
    Filipensky, Jan
    Wasserbauer, Jaromir
    Ptacek, Petr
    28TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2019), 2019, : 922 - 927
  • [32] Effect of thermo-mechanical parameters on microstructure evolution of AZ91 magnesium alloy
    Chen, Xiaohui
    Zhong, Zhiping
    Jin, Feixiang
    Ye, Liyan
    INTERNATIONAL CONFERENCE ON THE TECHNOLOGY OF PLASTICITY, ICTP 2017, 2017, 207 : 908 - 913
  • [33] Effect of deep cryogenic treatment on microstructure, creep and wear behaviors of AZ91 magnesium alloy
    Asl, Kaveh Meshinchi
    Tari, Alireza
    Khomamizadeh, Farzad
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 27 - 31
  • [34] Wear resistance of ceramic coating on AZ91 magnesium alloy by micro-arc oxidation
    赵晖
    刘正
    陈立佳
    陈吉
    韩忠
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S3) : 1814 - 1818
  • [35] Wear resistance of ceramic coating on AZ91 magnesium alloy by micro-arc oxidation
    Zhao Hui
    Liu Zheng
    Chen Li-jia
    Chen Ji
    Han Zhong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1814 - S1818
  • [36] Mechanisms of joint formation throughout semisolid stir welding of AZ91 magnesium alloy
    Hossein, V. A.
    Aashuri, H.
    Kokabi, A.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2013, 23 (09) : 2585 - 2590
  • [37] The effect of different modifiers in AlSi7Mg0.3 alloy on built-up edge formation in machining
    Martinovskỳ, Michal
    Madl, Jan
    Manufacturing Technology, 2016, 16 (01): : 173 - 178
  • [38] Analysis of the evolution of the Built-Up Edge and Built-Up Layer formation mechanisms in the dry turning of aeronautical aluminium alloys
    Gomez-Parra, A.
    Alvarez-Alcon, M.
    Salguero, J.
    Batista, M.
    Marcos, M.
    WEAR, 2013, 302 (1-2) : 1209 - 1218
  • [39] Fretting Wear Behavior of Micro-Arc Oxidation Coating Fabricated on AZ91 Magnesium Alloy
    Zhang, Fei
    Yin, Meigui
    Li, Qiang
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2022, 144 (04):
  • [40] Influence of rotational speed on the microstructural, mechanical and wear behaviour of FSPed cast AZ91 magnesium alloy
    Tripathi, Hariom
    Bharti, Ajaya
    Dev, Rahul
    Chauhan, Akhilesh Kumar
    Saxena, Kuldeep K.
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2024,