Coupling effect of thermal aging and pre-strain on fracture behavior of SMAW welded joints

被引:3
|
作者
Wang, Chunhui [1 ,2 ]
Fan, Minyu [3 ]
Yu, Min [3 ]
Yu, Weiwei [3 ]
Liu, Zheng [1 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Daya Bay Nucl Power Operat & Management Co Ltd, Shenzhen 518120, Peoples R China
[3] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
关键词
SMAW welded joints; Pre-strain; Thermal aging; Fracture toughness; Charpy impact test; DUPLEX STAINLESS-STEELS; MECHANICAL-PROPERTIES; DIFFERENT LOCATIONS; TOUGHNESS; EMBRITTLEMENT; MICROSTRUCTURE; TIG;
D O I
10.1016/j.engfracmech.2023.109224
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A repairing process is commonly needed to correct installation slope and geometrical deviation of nuclear power piping, but the resulting pre-strain has obvious degradation impacts on the long-term operation of surge pipeline, especially for the shielded metal arc welding (SMAW) joints. In this paper, to investigate the embrittlement induced by thermal aging and pre-strain, the SMAW welded joints with the base metal Z2CND18-12N2 and welded metal ER316L were subjected to different pre-strain (0%, 8%, 12% and 15%) and the accelerated thermal aging from 0 h to 13000 h at 400 celcius. Then, the Charpy impact test and compact tension fracture test were conducted to determine fracture properties of the SMAW welded joints. Results showed that both thermal aging and pre-strain can significantly reduce the fracture properties of SMAW welded joints. The impact absorbed energy reached stable after thermal aging 500 h, but it has been decreasing with the pre-strain varying from 0% to 15%. Moreover, it is shown that for pre-strained SMAW welded joints, with the increase of thermal aging duration, the absorbed energy first recovers, and then de-creases until stable. Compared with pre-strain, the influence of thermal aging is dominant. Finally, combined with microscopic analysis, the comprehensive effects of thermal aging and pre-strain on the embrittlement mechanism of SMAW welded joints were discussed.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Tensile and fatigue behavior of resistance spot-welded HSLA steel sheets: Effect of pre-strain in association with dislocation density
    Janardhan, Gorti
    Kishore, Kaushal
    Dutta, Krishna
    Mukhopadhyay, Goutam
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 793
  • [32] Effect of pre-strain on hydrogen induced cracking of PAW welded 304 austenitic stainless steel
    Zhou, Chilou
    Ren, Yingjie
    Yokogawa, Kiyoshi
    Xue, Jinxin
    Li, Xiang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 54 : 713 - 728
  • [33] EFFECT OF DYNAMIC LOADING ON FRACTURE BEHAVIOR OF WELDED JOINTS OF STRUCTURAL STEEL
    Zhang LiZhang YufengHuo LixingSchool of Material Scienceand Engineering
    Chinese Journal of Mechanical Engineering, 2004, (03) : 346 - 348
  • [34] Effects of Pre-Strain on the Aging Behavior of Al 7075 Alloy for Hot-Stamping Capability
    Jung, Seon-Ho
    Lee, Jongsup
    Kawasaki, Megumi
    METALS, 2018, 8 (02):
  • [35] Effect of Pre-Strain on the Fatigue Behavior of Extruded AZ31 Alloys
    Wu Yanjun
    INTERNATIONAL CONFERENCE ON MATERIALS SCIENCES AND NANOMATERIALS, 2017, 230
  • [36] Effect of pre-strain on ratcheting behavior of A668 Class D steel
    Tripathy, S.
    Mondal, A. K.
    Dutta, K.
    5TH NATIONAL CONFERENCE ON PROCESSING AND CHARACTERIZATION OF MATERIALS, 2016, 115
  • [37] EFFECT OF PRE-STRAIN ON YIELD SURFACES IN COPPER
    MAIR, WM
    PUGH, HLD
    JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 1964, 6 (02): : 150 - &
  • [38] Effect of pre-strain on microstructure evolution and fracture behavior of undermatching X80 pipeline steel girth weld
    Dai, Lianshuang
    Jia, Haidong
    Yang, Fulai
    Zhang, Shichao
    Zhang, Zheng
    Feng, Qingshan
    Que, Yongbin
    Wu, Yi
    MATERIALS RESEARCH EXPRESS, 2024, 11 (05)
  • [39] EFFECT OF PRE-STRAIN ON YIELD SURFACES IN COPPER
    HSU, TC
    MAIR, WM
    PUGH, HLD
    JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 1964, 6 (04): : 424 - &
  • [40] Quantitative evaluation of fracture toughness deterioration due to Pre-strain
    Ozawa, Takumi
    Kawabata, Tomoya
    Mikami, Yoshiki
    ENGINEERING FRACTURE MECHANICS, 2022, 272