Fracture strength of endocrown maxillary restorations using different preparation designs and materials

被引:2
|
作者
Al Fodeh, Rami S. [1 ]
Al-Johi, Omer S. [1 ]
Alibrahim, Anas N. [1 ]
Al-Dwairi, Ziad N. [1 ]
Husain, Nadin Al -Haj [2 ,3 ,4 ]
Ozcan, Mutlu [2 ,3 ,5 ]
机构
[1] Jordan Univ Sci & Technol, Fac Dent, Dept Prosthodont, Irbid, Jordan
[2] Univ Zurich, Ctr Dent Med, Div Dent Biomat, Clin Reconstruct Dent, Zurich, Switzerland
[3] Univ Zurich, Ctr Dent Med, Clin Masticatory Disorders & Dent Biomat, Zurich, Switzerland
[4] Univ Bern, Sch Dent Med, Dept Reconstruct Dent & Gerodontol, Bern, Switzerland
[5] Univ Zurich, Clin Prevent Dent Periodontol & Cariol, Ctr Dent Med, Plattenstr 11, CH-8032 Zurich, Switzerland
关键词
Dental materials; Endocrown; Endodontically treated teeth; Lithium discilicate; Multilayer zirconia; Prosthodontics; ENDODONTICALLY TREATED TEETH; BIOMECHANICAL BEHAVIOR; LITHIUM DISILICATE; BITE FORCE; RESISTANCE; POST; CROWNS; TOOTH; CORE;
D O I
10.1016/j.jmbbm.2023.106184
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Purpose: This study investigated the impact of preparation design and material types on fracture strength in maxillary premolars endocrowns after thermodynamic aging.Materials and methods: Eighty two-rooted maxillary premolar crowns underwent endodontic treatment (N = 80, n = 10). The teeth were categorized into ten groups (4-mm deep with no intracanal extension lithium disilicate glass ceramic & multilayer zirconia endocrowns (LE0 & ZE0); 4-mm deep with 4-mm intracanal extension in one canal (LE1 & ZE1); 4-mm deep with 2-mm intracanal extensions in both canals (LE2 & ZE2); flat overlays with no endocore (LO & ZO); glass fiber reinforced post & core and crown (LC & ZC)). After cementation, all specimens were subjected to 1500 thermocycles and 1,200,000 chewing cycles with an axial occlusal load of 49 N. A static loading test was performed at a non-axial 45 loading using a universal testing machine and failure modes (Type I: restoration debonding; Type II: restoration fracture; Type III: restoration/tooth complex fracture above bone level; Type IV: restoration/tooth complex fracture below bone level) were evaluated using a stereoscope. Data were ananalzed using 2-way ANOVA and Tukey's tests (alpha = 0.05).Results: The endocrowns manufactured from multilayered zirconia and pressed lithium disilicate glass ceramic exhibited a fracture load ranging between 1334 +/- 332 N and 756 +/- 150 N, with ZC presenting the highest and LE2 the lowest values. The differences were not statistically significant (p > 0.05).Conclusion: All endocrowns tested in this study performed similar considering the different designs and materials tested. The distribution of fracture modes did not differ significantly depending on the design of the restoration and the type of material used.
引用
收藏
页数:7
相关论文
共 50 条
  • [21] Effect of Endocrown Restorations with Different CAD/CAM Materials: 3D Finite Element and Weibull Analyses
    Gulec, Laden
    Ulusoy, Nuran
    BIOMED RESEARCH INTERNATIONAL, 2017, 2017
  • [22] Fracture Resistance of Ceramic Veneers with Different Preparation Designs
    Akoglu, Burcin
    Gemalmaz, Deniz
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (05): : 380 - 384
  • [23] Effects of different cusp coverage restorations on the fracture resistance of endodontically treated maxillary premolars
    Kalay, Tugba Serin
    Yildirim, Tahsin
    Ulker, Mustafa
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 116 (03): : 404 - 410
  • [24] Fracture strength of different core build-up designs
    Bolhuis, HPB
    De Gee, AJ
    Feilzer, AJ
    Davidson, CL
    AMERICAN JOURNAL OF DENTISTRY, 2001, 14 (05): : 286 - 290
  • [25] Fracture strength and failure mode for different ceramic veneer designs
    Castelnuovo, J
    Tjan, AHL
    Phillips, K
    Nicholls, JI
    Kois, JC
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 803 - 803
  • [26] Fracture resistance of five different metal framework designs for metal-ceramic restorations
    Ulusoy, M
    Toksavul, S
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2002, 15 (06) : 571 - 574
  • [27] Comparative Evaluation of Two Different Preparation Designs and Materials on the Fracture Resistance of Laminate Veneers: An In Vitro Study
    Soni, Pranjal S.
    Sanyal, Pronob
    CUREUS JOURNAL OF MEDICAL SCIENCE, 2024, 16 (08)
  • [28] Influence of different metal restorations bonded with resin on fracture resistance of endodontically treated maxillary premolars
    Costa, LCS
    Pegoraro, LF
    Bonfante, G
    JOURNAL OF PROSTHETIC DENTISTRY, 1997, 77 (04): : 365 - 369
  • [29] Fracture strength of extended class I composite restorations with different restorative techniques
    Leyton, Brenda S.
    Rached, Rodrigo N.
    Ignacio, Sergio A.
    Souza, Evelise M.
    ODONTOLOGY, 2022, 110 (02) : 269 - 277
  • [30] Biomechanical behavior of endocrown restorations with different CAD-CAM materials: A 3D finite element and in vitro analysis
    Zheng, Ziting
    He, Yunyan
    Ruan, Wenhao
    Ling, Zhiting
    Zheng, Chunqing
    Gai, Yawen
    Yan, Wenjuan
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 125 (06): : 890 - 899