Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215

被引:0
|
作者
Liang Kai [1 ]
Yao Zhihao [1 ]
Xie Xishan [1 ]
Yao Kaijun [1 ]
Dong Jianxin [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
SP2215 heat-resistant alloy; long term aging; precipitation; stress rupture strength; property; PRECIPITATION KINETICS; MECHANICAL-PROPERTIES; AUSTENITIC STEEL; EVOLUTION; SUPER304H; BEHAVIOR; M23C6; CREEP;
D O I
10.11900/0412.1961.2022.00539
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
With the improvement of the steam parameters of thermal power units, the requirements put forward for the stress rupture strength and structural stability of heat-resistant materials for boiler superheater/reheater pipes become higher. SP2215, as a new heat-resistant alloy, is an excellent candidate for 620-650 degrees C ultra-supercritical boiler superheater/reheater. In this study, the correlation between microstructure evolution and properties of the SP2215 heat-resistant alloy aging at different temperatures and time was studied via a series of creep and impact tests. The results show that the SP2215 alloy has excellent microstructure stability in high-temperature condition. Moreover, various nanoscale precipitations such as Cu-rich, MX, NbCrN, and M23C6 phases occur during aging. In the early period of aging, with the increase in aging temperature and aging time, the precipitations increase rapidly, improving the strength of the material; however, the impact toughness of the SP2215 alloy decreases considerably, with substantial intergranular fracture caused by the continuous precipitation and growth of M23C6 at the boundary, as shown with the quantitative calculation using the JMA model. In the late period of aging, the precipitations gradually stabilize, and the grain size remains in the range of 4.5-5 grade. As a result, the 1 x 10(5) h stress rupture strength of the SP2215 alloy at 650 and 700 degrees C still remain more than 120 and 70 MPa, respectively. Hence, the alloy can be used as a domestic replacement for foreign HR3C, Super304H, and other similar heat-resistant alloys.
引用
收藏
页码:797 / 811
页数:15
相关论文
共 34 条
  • [21] Precipitate evolution during the aging of Super304H steel and its influence on impact toughness
    Wang, Xue
    Li, You
    Chen, Dongxu
    Sun, Jianhua
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 754 : 238 - 245
  • [22] Isothermal aging embrittlement in an Fe-22Cr-25Ni alloy
    Wei, Limin
    Hao, Weixun
    Cheng, Yi
    Tan, Shuping
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 737 : 40 - 46
  • [23] Xiao J M, 1987, ALLOY PHASE PHASE TR, P250
  • [24] Xie X S, 2016, Chin Pat, Patent No. [201310719141.4, 2013107191414]
  • [25] Xie Xi Shan, 2018, steel pipe, V47, P23
  • [26] Microstructural evolution and the effect on hardness and plasticity of S31042 heat-resistant steel during creep
    Yang, Yahong
    Zhu, Lihui
    Wang, Qijiang
    Zhu, Changchun
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 608 : 164 - 173
  • [27] Stress Rupture Fracture Model and Microstructure Evolution for Waspaloy
    Yao, Zhihao
    Zhang, Maicang
    Dong, Jianxin
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2013, 44A (07): : 3084 - 3098
  • [28] Microstructural Evolution and the Effect on Mechanical Properties of S30432 Heat-resistant Steel during Aging at 650°C
    Zhang, Yujie
    Zhu, Lihui
    Qi, Anfang
    Lu, Zhengran
    [J]. ISIJ INTERNATIONAL, 2010, 50 (04) : 596 - 600
  • [29] Zheng Z J, 2011, BOILER TECHNOL, V42, P46
  • [30] Precipitation Kinetics of M23C6 Carbides in the Super304H Austenitic Heat-Resistant Steel
    Zhou, Qingwen
    Ping, Shaobo
    Meng, Xiaobo
    Wang, Ruikun
    Gao, Yan
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (12) : 6130 - 6139