Mechanical and tribological properties of 5A06 aluminum alloy at low temperature

被引:4
|
作者
Ye, Tao [1 ]
Jia, Zhen-yuan [1 ]
Ma, Jian-wei [1 ]
Yu, Wu-jiang [2 ]
Wang, Jia-sen [2 ,3 ]
Zhang, Lian-wan [2 ,3 ]
Tian, Xue-bao [1 ]
Wang, Shuang [1 ]
机构
[1] Dalian Univ Technol, Sch Mech Engn, Key Lab Precis & Nontradit Machining Technol, Minist Educ, Dalian 116024, Peoples R China
[2] Beijing Inst Astronaut Syst Engn, Beijing 100000, Peoples R China
[3] Beijing Key Lab Cryogen Technol Res, Beijing 100000, Peoples R China
基金
中国国家自然科学基金;
关键词
aluminum; mechanical properties; friction behavior; wear mechanism; low temperature; TRIBOPAIR; WEAR;
D O I
10.1088/2051-672X/acb72c
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
There are significant differences in the mechanical and tribological properties of 5A06 aluminum alloys subjected to a wide temperature range, and the related research has received very limited attention so far. In this paper, the mechanical properties of 5A06 aluminum alloy were obtained by tensile test at temperature as low as 77K, which laid a foundation for analyzing its tribological properties. Then, dry linear reciprocating sliding wear tests were performed on a ball-on-disc tribometer to explore the friction behavior and wear mechanism of 5A06 aluminum alloy at different temperatures from low temperature (173K) to room temperature (293K). Finally, the wear morphology and chemical composition of the worn surface were characterized by an optical 3D measurement system and a scanning electron microscope equipped with an energy dispersive spectroscopy. The results indicate that the ambient temperature affects the tribological properties of 5A06 aluminum alloy by changing its mechanical properties and the dissipation of friction heat. Compared with 293K, the coefficient of friction decreases by 14.66% and the wear rate decreases by 70.79% at 173K. The main wear mechanisms of 5A06 aluminum alloy are delamination wear and oxidation wear at 293K and 273K, and a combination of abrasive wear, adhesive wear and oxidation wear at 223K and 173K.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] Correlation between microstructure and properties of 2219/5A06 dissimilar aluminum alloy welded joint
    Li H.
    Xu G.
    Zhang Y.
    Wu S.
    Wang F.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2020, 41 (09): : 8 - 15
  • [22] Interfacial reaction behavior and mechanical properties of 5A06 Al alloy soldered with Sn-1Ti-xGa solders at a low temperature
    宋立志
    肖勇
    奚邦富
    李佳琪
    张建
    China Welding, 2023, 32 (02) : 23 - 31
  • [23] Effects of plastic deformation of solid phase on mechanical properties and microstructure of wrought 5A06 aluminum alloy in directly semisolid thixoforging
    Jiang, Jufu
    Liu, Yingze
    Xiao, Guanfei
    Wang, Ying
    Xiao, Xinquan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 831
  • [24] Laser beam oscillating welding of 5A06 aluminum alloys: Microstructure, porosity and mechanical properties
    Wang, Zhimin
    Oliveira, J. P.
    Zeng, Zhi
    Bu, Xianzheng
    Peng, Bei
    Shao, Xinyu
    OPTICS AND LASER TECHNOLOGY, 2019, 111 : 58 - 65
  • [25] Effects of plastic deformation of solid phase on mechanical properties and microstructure of wrought 5A06 aluminum alloy in directly semisolid thixoforging
    Jiang J.
    Liu Y.
    Xiao G.
    Wang Y.
    Xiao X.
    Jiang, Jufu (jiangjufu@hit.edu.cn), 1600, Elsevier Ltd (831):
  • [26] Static mechanical properties and failure behaviors of self-piercing riveted joints in aluminum alloy 5A06 after aging
    Ye, Kai
    Zhao, Lun
    Abbas, Zeshan
    Li, Chengwang
    Liu, Gaoyu
    Lei, Le
    Lu, Jiehao
    Islam, Md Shafiqul
    THIN-WALLED STRUCTURES, 2024, 201
  • [27] Mechanism of Crack Initiation of Dissimilar Joints between 2219 Aluminum Alloy and 5A06 Aluminum Alloy
    Chen, Chao
    Li, Qingqing
    Lin, Sanbao
    Zhou, Jing
    Fan, Chenglei
    Yang, Chunli
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (03): : 775 - 781
  • [28] Mechanical properties of ultrasonic welded and self-piercing riveted joints in a 5A06 aluminum alloy and a TA1 titanium alloy
    Lun, Zhao
    Huo, Xiaole
    Zeshan, Abbas
    Liang, Zhaofeng
    MATERIALS TESTING, 2024, 66 (06) : 883 - 895
  • [29] Mechanism of Crack Initiation of Dissimilar Joints between 2219 Aluminum Alloy and 5A06 Aluminum Alloy
    Chen Chao
    Li Qingqing
    Lin Sanbao
    Zhou Jing
    Fan Chenglei
    Yang Chunli
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (03) : 775 - 781
  • [30] Microbial corrosion behavior and mechanism of 5A06 aluminum alloy under low dose proton radiation
    Chen, Nana
    Liu, Qianqian
    Feng, Yali
    Zou, Shiwen
    Yao, Qiong
    Lu, Lin
    Wu, Junsheng
    Xiao, Kui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 4533 - 4540