Effect of hierarchical martensitic microstructures on the ductile-brittle transition behavior of friction stir welded reduced activation ferritic/ martensitic steel

被引:0
|
作者
Li, Shengli [1 ]
Shi, Lei [1 ]
Chen, Ji [1 ]
Yang, Xinqi [2 ]
Hartmaier, Alexander [3 ]
Wu, Chuansong [1 ]
机构
[1] Shandong Univ, Inst Mat Joining, MOE Key Lab Liquid Solid Struct Evolut & Mat Proc, Jinan 250061, Peoples R China
[2] Tianjin Univ, Sch Mat Sci & Engn, Tianjin Key Lab Adv Joining Technol, Tianjin 300350, Peoples R China
[3] Ruhr Univ Bochum, Interdisciplinary Ctr Adv Mat Simulat ICAMS, D-44801 Bochum, Germany
关键词
Reduced activation ferritic/martensitic steel; Friction stir welding; Austenite reconstruction; Precipitates evolution; Ductile-brittle transition; MECHANICAL-PROPERTIES; FERRITIC/MARTENSITIC STEELS; JOINTS; TOUGHNESS; CRYSTALLOGRAPHY; FRACTURE; GRAINS; ZONE;
D O I
10.1016/j.msea.2024.146267
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The welded joints of reduced activation ferritic/martensitic (RAFM) steel should exhibit superior toughness to ensure that structural components are not prone to fracture due to irradiation embrittlement under long-term neutron irradiation conditions. Friction stir welding (FSW) of RAFM steel was performed, considering the potential advantages of obtaining welded joints with a good balance of strength and toughness. This work systematically investigated the effect of hierarchical martensitic microstructural evolution on the impact toughness of friction stir welded (FSWed) RAFM steel in the as-welded condition and post-weld tempering treatment at 760 degrees C. Prior austenite reconstruction based on the electron backscatter diffraction (EBSD) technology and precipitate analysis according to the transmission electron microscopy (TEM) data were conducted to study the microstructural evolution comprehensively. Tempering treatment reduces the average hardness of the SZ from 446 HV to 269 HV, but it remains 39 HV higher than that of the base material (BM). The tensile specimens containing whole regions of the welded joint all fracture in the BM. The ultimate tensile strength (UTS) of the tensile specimens containing only the SZ reaches 1033.7 MPa and 799.0 MPa in the as-weld and tempered at 760 degrees C conditions, respectively, which is greater than the 689.3 MPa of the BM. The FSWed joint of RAFM steel in the as-welded condition has acceptable toughness, and its ductile-brittle transition temperature (DBTT) corresponding to 68 J impact absorbed energy reaches -74.2 degrees C. Post-weld tempering treatment at 760 degrees C further reduces the DBTT to -110.7 degrees C, slightly higher than the -114.8 degrees C of the BM. The refined grain size is the crucial microstructure that determines the FSWed joint of RAFM steel has better toughness and lower DBTT than fusion welded joints.
引用
收藏
页数:18
相关论文
共 50 条
  • [31] Torsional behavior of a friction welded martensitic stainless steel
    Kati, Nida
    Ozan, Sermin
    MATERIALS TESTING, 2016, 58 (09) : 742 - 747
  • [32] Strong and ductile reduced activation ferritic/martensitic steel additively manufactured by selective laser melting
    Jiang, M. G.
    Chen, Z. W.
    Tong, J. D.
    Liu, C. Y.
    Xu, G.
    Liao, H. B.
    Wang, P.
    Wang, X. Y.
    Xu, M.
    Lao, C. S.
    MATERIALS RESEARCH LETTERS, 2019, 7 (10): : 426 - 432
  • [33] Anisotropy in tensile and ductile-brittle transition behavior of ODS ferritic steels
    Kasada, R.
    Lee, S. G.
    Isselin, J.
    Lee, J. H.
    Omura, T.
    Kimura, A.
    Okuda, T.
    Inoue, M.
    Ukai, S.
    Ohnuki, S.
    Fujisawa, T.
    Abe, F.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 180 - 184
  • [34] Microstructures and mechanical properties of reduced activation ferritic/ martensitic steel fabricated by laser melting deposition
    Feng, Junyi
    Zhang, Peilei
    Jia, Zhiyuan
    Yu, Zhishui
    Fang, Chao
    Yan, Hua
    Shi, Haichuan
    Tian, Yingtao
    FUSION ENGINEERING AND DESIGN, 2021, 173
  • [35] Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel
    Chen, Shenghu
    Rong, Lijian
    JOURNAL OF NUCLEAR MATERIALS, 2015, 459 : 13 - 19
  • [36] Effect of specimen size on fatigue properties of reduced activation ferritic/martensitic steel
    Hirose, T
    Sakasegawa, H
    Kohyama, A
    Katoh, Y
    Tanigawa, H
    EFFECTS OF RADIATION ON MATERIALS: 20TH INTERNATIONAL SYMPOSIUM, 2001, 1045 : 535 - 545
  • [37] Oxidation studies of Indian reduced activation ferritic martensitic steel
    A. Mukherjee
    U. Jain
    G. K. Dey
    Journal of Thermal Analysis and Calorimetry, 2017, 128 : 819 - 824
  • [38] Deuterium and Tritium Permeation in the Reduced Activation Ferritic/Martensitic Steel
    Fan Dongjun
    Lu Guangda
    Zhang Guikai
    Bao Jinchun
    Yang Feilong
    Xiang Xin
    Chen Chang'an
    ACTA METALLURGICA SINICA, 2018, 54 (04) : 519 - 526
  • [39] Oxidation studies of Indian reduced activation ferritic martensitic steel
    Mukherjee, A.
    Jain, U.
    Dey, G. K.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2017, 128 (02) : 819 - 824
  • [40] Recent results of the reduced activation ferritic/martensitic steel development
    Jitsukawa, S
    Kimura, A
    Kohyama, A
    Klueh, RL
    Tavassoli, AA
    van der Schaaf, B
    Odette, GR
    Rensman, JW
    Victoria, M
    Petersen, C
    JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 39 - 46