Microstructure, corrosion and mechanical properties of as-cast Mg-Zn-Y with different Zn-to-Y ratios

被引:5
|
作者
Li, Pengyu [1 ]
Sun, Yufeng [1 ]
Zhu, Shijie [1 ]
Wang, Liguo [1 ]
Guan, Shaokang [1 ]
Wang, Jianfeng [1 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Zhengzhou 450001, Peoples R China
来源
关键词
Magnesium alloy; Second phase; Corrosion resistance; Mechanical properties; QUASI-CRYSTALLINE PHASE; GRAIN-REFINEMENT; W-PHASE; ALLOY; STRENGTH; EVOLUTION; TEXTURE; LPSO;
D O I
10.1016/j.mtcomm.2023.107562
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
As-cast Mg-8Zn-xY (x = 1.4, 3.4, and 6.7; wt%) alloys containing I-phase, mixed I- and W-phases, W-phase were prepared, respectively. With the decrease of Zn/Y ratio, the second phase gradually changes from discontinuous network structure to continuous network structure. The effect of second phase on the corrosion resistance of MgZn-Y alloy was studied in detail by testing the hydrogen evolution, polarization curve, corrosion morphology and Volta potential. The results show that Mg-8Zn-3.4Y alloy containing mixed W- and I-phases has the best corrosion resistance. The good corrosion resistance can be attributed to the network structure of mixed W- and I-phases which can prevent the extension of corrosion. In addition, Mg-8Zn-3.4Y alloy exhibits the yielding strength of 123 MPa, ultimate strength of 219 MPa, and elongation to fracture of 14 %. The good combination of corrosion and mechanical properties for the current alloy is helpful for the further application.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] Microstructure and mechanical properties of a Mg-Zn-Y alloy produced by a powder metallurgy route
    Asgharzadeh, H.
    Yoon, E. Y.
    Chae, H. J.
    Kim, T. S.
    Lee, J. W.
    Kim, H. S.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 586 : S95 - S100
  • [42] Microstructure and mechanical properties of Mg-Zn-Y alloy under a steady magnetic field
    Zhang, L.
    Jin, F.
    Zhan, W.
    Hu, P. H.
    Zhou, Q.
    MATERIALS SCIENCE AND TECHNOLOGY, 2017, 33 (18) : 2197 - 2202
  • [43] Influence of the Heat Treatment on Mechanical Properties and Microstructure in LPSO Mg-Zn-Y Alloys
    Noda, Masafumi
    Mayama, Tsuyoshi
    Kawamura, Yoshihito
    MAGNESIUM TECHNOLOGY 2010, 2010, : 501 - +
  • [44] Effect of Artificial Cooling Extrusion on Microstructure and Mechanical Properties of Mg-Zn-Y Alloys
    Liao, Qi-Yu
    Zhao, Da-Zhi
    Le, Qi-Chi
    Hu, Wen-Xin
    Jiang, Yan-Chao
    Zhou, Wei-Yang
    Ren, Liang
    Li, Dan-Dan
    Yin, Zhao-Yang
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2024, 37 (07) : 1115 - 1127
  • [45] Microstructures and mechanical properties of consolidated Mg-Zn-Y alloy
    Lee, J. K.
    Kim, T. S.
    Jeong, H. G.
    Bae, J. C.
    PROGRESS IN POWDER METALLURGY, PTS 1 AND 2, 2007, 534-536 : 833 - +
  • [46] Effect of multimodal microstructure evolution on mechanical properties of Mg-Zn-Y extruded alloy
    Yamasaki, Michiaki
    Hashimoto, Kenji
    Hagihara, Koji
    Kawamura, Yoshihito
    ACTA MATERIALIA, 2011, 59 (09) : 3646 - 3658
  • [47] Comparative Study on Corrosion Behavior and Mechanism of As-Cast Mg–Zn–Y and Mg–Zn–Gd Alloys
    Guoqiang Xi
    Xuhan Zhao
    Yanlong Ma
    Yu Mou
    Ju Xiong
    Kai Ma
    Jingfeng Wang
    Acta Metallurgica Sinica (English Letters), 2023, 36 : 310 - 322
  • [48] Effects of Cooling Rate and Component on the Microstructure and Mechanical Properties of Mg-Zn-Y Alloys
    Shao, Shuang
    Liu, Yong
    Xu, Chun-Shui
    Xu, Ying-Xuan
    Wu, Bin
    Zeng, Xiao-Shu
    Lu, Xian-Feng
    Yang, Xiang-Jie
    Acta Metallurgica Sinica-English Letters, 2015, 28 (01) : 7 - 14
  • [49] Microstructure and Properties of As-Cast Mg-2.0Sn-1.0Zn-1.0Y-0.3Zr Alloys at Different Extrusion Ratios
    Gong, Yuan
    He, Junguang
    Wen, Jiuba
    Feng, Wuyun
    Zheng, Xiangyang
    Li, Huan
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (12)
  • [50] Microstructure and phase compositions of as-cast Mg–3.9Zn–0.6RE (Gd, Y) alloy with different Gd/Y ratios
    Yang Yang
    Kui Zhang
    Ming-Long Ma
    Jia-Wei Yuan
    Rare Metals, 2015, 34 : 160 - 163