Effect of cryogenic treatment on wear behavior of Sleipner cold work tool steel

被引:42
|
作者
Kara, Fuat [1 ]
Kucuk, Yilmaz [2 ]
Ozbek, Onur [3 ]
Ozbek, Nursel Altan [4 ]
Gok, Mustafa Sabri [2 ]
Altas, Emre [2 ]
Uygur, Ilyas [1 ]
机构
[1] Duzce Univ, Dept Mech Engn, TR-81620 Duzce, Turkiye
[2] Bartin Univ, Dept Mech Engn, TR-74100 Bartin, Turkiye
[3] Duzce Univ, Gumusova Vocat Sch Higher Educ, TR-81850 Duzce, Turkiye
[4] Duzce Univ, Dr Engin PAK Cumayeri Vocat Sch Higher Educ, TR-81700 Duzce, Turkiye
关键词
Sleipner steel; Cryogenic treatment; Wear rate; Tribology; CARBIDE PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURE;
D O I
10.1016/j.triboint.2023.108301
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Cryogenic treatment, also known as subzero heat treatment, is a cooling process that complements conventional heat treatment to improve the properties of metals. Unlike coatings, it is a one-time, inexpensive, permanent operation that affects the entire part. This method is mainly applied to tool steels used in mold making. In this study, the changes caused by the effects of shallow and deep cryogenic treatment on Sleipner cold work tool steel were investigated in terms of microhardness, microstructure, coefficient of friction (COF), and wear rate (WR). For this purpose, the test specimens were subjected to the cryogenic treatments performed at two different temperatures (80 degrees C for the shallow cryogenic treatment (SCT) and 180 degrees C for the deep cryogenic treatment (DCT)) and various retention times (12 h, 24 h for SCT and 12 h, 24 h, 36 h for DCT). Dry sliding wear tests were carried out under different loads (10 N and 20 N) and varying test durations (60, 120, and 240 min) at a constant sliding speed of 0.075 m/s. According to the microhardness results, it was determined that the cryogenic treatment increased the hardness by 6.53 %. According to the microstructure investigations, a more homogeneous structure was observed with the cryogenic treatment, and secondary carbide precipitations were detected. It was observed that the conventional heat-treated (CHT) sample gave the highest COF value with an average coefficient of friction of 0.63. The lowest COF value of 0.58 was observed in the DCT-12 sample. After the wear tests, the lowest wear rate value for both load values was obtained from the DCT-36 specimen.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Investigation of the effect of cutting parameters on cutting force, surface roughness and chip shape in turning of Sleipner cold work tool steel
    Ozlu, Baris
    JOURNAL OF THE FACULTY OF ENGINEERING AND ARCHITECTURE OF GAZI UNIVERSITY, 2021, 36 (03): : 1242 - 1251
  • [22] Effect of deep cryogenic treatment on the formation of nano-sized carbides and the wear behavior of D2 tool steel
    Amini, Kamran
    Akhbarizadeh, Amin
    Javadpour, Sirus
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2012, 19 (09) : 795 - 799
  • [23] Effect of deep cryogenic treatment on the formation of nano-sized carbides and the wear behavior of D2 tool steel
    Kamran Amini
    Amin Akhbarizadeh
    Sirus Javadpour
    International Journal of Minerals, Metallurgy, and Materials, 2012, 19 : 795 - 799
  • [24] Investigating the effect of the quench environment on the final microstructure and wear behavior of 1.2080 tool steel after deep cryogenic heat treatment
    Amini, Kamran
    Akhbarizadeh, Amin
    Javadpour, Sirus
    MATERIALS & DESIGN, 2013, 45 : 316 - 322
  • [25] Effect of deep cryogenic treatment on the formation of nano-sized carbides and the wear behavior of D2 tool steel
    Kamran Amini
    Amin Akhbarizadeh
    Sirus Javadpour
    International Journal of Minerals Metallurgy and Materials, 2012, 19 (09) : 795 - 799
  • [26] Cryogenic Treatment and Peening of Hot-work Tool Steel
    Nakonieczny, A.
    Ciski, A.
    Babul, T.
    BHM Berg- und Huttenmannische Monatshefte, 2010, 155 (03): : 105 - 109
  • [27] Investigating the effect of the deep cryogenic heat treatment on the corrosion behavior of the 1.2080 tool steel
    Amini, K.
    Akhbarizadeh, A.
    Javadpour, S.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2016, 54 (05): : 331 - 338
  • [28] Effect of Cryogenic Treatment on Properties of Cr8-Type Cold Work Die Steel
    Hong-xiao Chi
    Dang-shen Ma
    Qi-long Yong
    Li-zhi Wu
    Zhan-pu Zhang
    Yong-wei Wang
    Journal of Iron and Steel Research International, 2010, 17 : 43 - 46
  • [29] Effect of Cryogenic Treatment on Properties of Cr8-Type Cold Work Die Steel
    CHI Hong-xiao1
    2. Institute for Structural Materials
    3. Heye Special Steel Co Ltd
    JournalofIronandSteelResearch(International), 2010, 17 (06) : 43 - 46
  • [30] Effect of Cryogenic Treatment on Properties of Cr8-Type Cold Work Die Steel
    Chi Hong-xiao
    Ma Dang-shen
    Yong Qi-long
    Wu Li-zhi
    Zhang Zhan-pu
    Wang Yong-wei
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2010, 17 (06) : 43 - +