Weld Strength and Microstructure Analysis on Resistance Spot Welding of Austenitic AISI 347 Stainless Steel and Duplex AISI 2205 Stainless Steel

被引:4
|
作者
Prabhakaran, M. [1 ,2 ]
Duraisamy, Jeyasimman [1 ]
Shanmugam, N. Siva [3 ]
Kannan, A. Rajesh [3 ]
Varatharajalu, M. [4 ]
机构
[1] Periyar Maniammai Inst Sci & Technol, Dept Mech Engn, Vallam 613403, Thanjavur, India
[2] Agnel Inst Technol & Design, Dept Mech Engn, Bardez 403507, Goa, India
[3] Natl Inst Technol, Dept Mech Engn, Trichy 620015, India
[4] Sri Krishna Coll Technol, Dept Mech Engn, Kovaipudur 641042, Tamil Nadu, India
关键词
Resistance spot weld; AISI; 347; 2205; Duplex stainless steel; Tensile shear strength; Failure mode; EDS; Fractography; PROCESS PARAMETERS; FAILURE BEHAVIOR; METALLURGY; ALUMINUM; SHEETS; MODE;
D O I
10.1007/s12666-022-02789-x
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this research, the effect of welding current and heating cycle is studied against the weld strength. The AISI 347 and AISI 2205 of 2 mm thickness are taken for conducting the experiment. The squeezing time cycle, holding time cycle and electrode tip diameter are kept constant. The welded specimens are fractured using a tensile shear load testing facility and a macrograph examination is carried out. The specimen welded with the highest welding current of 8.5 kA and 14 heating cycles obtained the largest weld nugget and absorbed a maximum tensile shear load of 18.5 kN. All the samples except one failed under interfacial mode and sample 9 failed under pull-out failure mode. The scanning electron microscope (SEM) image of the failed nuggets shows a smooth transition from the austenitic to a mixture of austenitic-ferritic phase structures. The SEM-energy-dispersive spectroscopy analysis was carried out on the selected samples for their weld composition. The elemental spectrum shows a Cr-eq/Ni-eq ratio of 2.52 which confirms a ferritic phase formation upon solidification. The fractography results show the formation of dimples and torn bands on the lower and upper surfaces of the fractured nugget revealing the ductile failure of the weld. Maximizing the welding current and heating cycle maximizes the weld nugget area. The specimens which did not attain the minimum weld nugget size failed in the interfacial mode.
引用
收藏
页码:925 / 936
页数:12
相关论文
共 50 条
  • [41] Transition behavior of welding HAZ microstructure of 2205 duplex Stainless Steel
    Xiong, Qingren
    Huo, Chunyong
    Li, Weiwei
    Zhang, Jianxun
    Hanjie Xuebao/Transactions of the China Welding Institution, 2007, 28 (11): : 53 - 57
  • [42] Characterization of the hot deformation microstructure of AISI 321 austenitic stainless steel
    Ghazani, M. Shaban
    Eghbali, B.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 730 : 380 - 390
  • [43] Effect of aging at 700°C on precipitation and toughness of AISI 321 and AISI 347 austenitic stainless steel welds
    Guan, KS
    Xu, XD
    Xu, H
    Wang, ZW
    NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (23) : 2485 - 2494
  • [44] Formability evaluation of tailor weld blanks of austenitic stainless steel (AISI 304)
    Krishnamraju, M.
    Reddy, P. Venkateshwar
    Mahajan, Peeyush
    Mishra, Sushil Kumar
    Narasimhan, K.
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2024, 10 (03) : 2008 - 2020
  • [45] Use of EPR test to study the degree of sensitization in resistance spot welding joints of AISI 304 austenitic stainless steel
    de Tiedra, Pilar
    Martin, Oscar
    Lopez, Manuel
    San-Juan, Manuel
    CORROSION SCIENCE, 2011, 53 (04) : 1563 - 1570
  • [46] Characterization of AISI 316L Stainless Steel/Low Alloy Steel Resistance Spot Dissimilar Weld
    Alali, Muhaed
    Alnaffakh, Maysaa G.
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2023, 12 (04) : 622 - 633
  • [47] Artificial neural networks for pitting potential prediction of resistance spot welding joints of AISI 304 austenitic stainless steel
    Martin, Oscar
    De Tiedra, Pilar
    Lopez, Manuel
    CORROSION SCIENCE, 2010, 52 (07) : 2397 - 2402
  • [48] Characterization of AISI 316L Stainless Steel/Low Alloy Steel Resistance Spot Dissimilar Weld
    Muhaed Alali
    Maysaa G. Alnaffakh
    Metallography, Microstructure, and Analysis, 2023, 12 : 622 - 633
  • [49] Creep ruptures of AISI 347 austenitic stainless steel foils at elevated temperature of 750?
    Osman, H.
    Nor, F. M.
    Hamdan, Y. M.
    Tamin, M. N.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2017, 231 (06) : 516 - 522
  • [50] Sensitization evaluation of the AISI 2205 duplex stainless steel by the IQ value in EBSD technique
    Lv Jinlong
    Wang Zhuqing
    ENGINEERING FAILURE ANALYSIS, 2019, 105 : 65 - 69