Directed energy deposition of Al-Mg-Si alloys with fully-equiaxed microstructure and isotropic high strength/ductility

被引:1
|
作者
Li, Wenzhe [1 ,3 ]
Pan, Shiwei [1 ]
Zhu, Yichao [1 ]
Qian, Feng [1 ]
Liang, Yaojian [1 ]
Xu, Shun [1 ]
Cheng, Xingwang [1 ,2 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Natl Key Lab Sci & Technol Mat Shock & Impact, Beijing 100081, Peoples R China
[2] Beijing Inst Technol, Tangshan Res Inst, Tangshan 063000, Peoples R China
[3] Hong Kong Polytech Univ, Dept Mech Engn, Hong Kong 999077, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing (AM); Aluminum alloys; Nucleant; Equiaxed microstructure; Anisotropy; ALUMINUM-ALLOYS; MECHANICAL-PROPERTIES; ALSI10MG ALLOY; LASER; ANISOTROPY; STRENGTH; CRACK; PARTICLES; SCANDIUM; BEHAVIOR;
D O I
10.1016/j.addma.2024.104020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-Mg-Si alloys fabricated by additive manufacturing (AM) are known to suffer from the coarse columnar microstructure, which usually causes severe hot cracking and anisotropy in mechanical properties. Introducing potent nucleants to promote columnar to equiaxed transition (CET) is an efficient method to solve this problem. However, nanoscale nucleant particles are prone to agglomerate and form clusters during high-temperature AM, which are detrimental to the ductility. In this work, in the AA6061 fabricated by directed energy deposition (DED), we designed a novel approach to alleviate the agglomeration of TiB2 particles by adopting interlayer pause (IP) strategy on the basis of TiB2 nucleant addition. Resultantly, due to the discontinuous heat input interrupted by IP and thus a reduced heat accumulation, dispersed fine TiB2 particles can be achieved, which reduce the stress concentration and allow for a good metallurgical binding. Moreover, these dispersed fine TiB2 particles, (a) effectively promote the CET by providing numerous heterogeneous nucleation sites, resulting in an ultra-fine fully-equiaxed grain microstructure (similar to 21 mu m) with a reduced texture; (b) significantly inhibit the formation of pores, reducing both their density and size. Consequently, crack-free high-performance DEDed AA6061 without anisotropy in mechanical properties are successfully fabricated, achieving high strength and high ductility at T6-treated state along both the vertical direction (YS: 266 +/- 2 MPa, EL: 8 +/- 1%) and the horizontal direction (YS: 262 +/- 2 MPa, EL: 7 +/- 1%), simultaneously. This combination of nucleant addition and deliberately-controlled IP strategy is expected to be applicable to a wide range of wrought aluminum alloys (e.g. 2xxx and 7xxx) fabricated by AM.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Microstructure evolution and aging kinetics of Al-Mg-Si and Al-Mg-Si-Sc alloys processed by ECAP
    Angella, G
    Bassani, P
    Tuissi, A
    Ripamonti, D
    Vedani, M
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION, 2006, 503-504 : 493 - 498
  • [32] Effect of iron on the microstructure and mechanical property of Al-Mg-Si-Mn and Al-Mg-Si diecast alloys
    Ji, Shouxun
    Yang, Wenchao
    Gao, Feng
    Watson, Douglas
    Fan, Zhongyun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 564 : 130 - 139
  • [33] Strength and Electrical Conductivity Relationships in Al-Mg-Si and Al-Sc Alloys
    Rometsch, Paul A.
    Xu, Zhou
    Zhong, Hao
    Yang, Huai
    Ju, Lin
    Wu, Xinhua
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 827 - +
  • [34] Influence of microstructure on deformation behavior and fracture mode of Al-Mg-Si alloys
    Jiang, D
    Wang, C
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 352 (1-2): : 29 - 33
  • [35] Influence of cooling rate on distortion and microstructure in extrusion of Al-Mg-Si alloys
    Andreas Jäger
    Markus Heilmann
    Wojciech Z. Misiolek
    Marco Schikorra
    A. Erman Tekkaya
    International Journal of Material Forming, 2009, 2
  • [36] INFLUENCE OF COOLING RATE ON DISTORTION AND MICROSTRUCTURE IN EXTRUSION OF Al-Mg-Si ALLOYS
    Jaeger, Andreas
    Heilmann, Markus
    Misiolek, Wojciech Z.
    Schikorra, Marco
    Tekkaya, A. Erman
    INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2009, 2 : 81 - 84
  • [37] Microstructural Effects of Al-Mg-Si Alloys on Sustained Load Cracking and Strength
    Kim, Dae-Kyeom
    Nam, Sun-Woo
    Kim, Seong Chul
    Cho, Sung-Min
    Kim, Taek-Soo
    SCIENCE OF ADVANCED MATERIALS, 2017, 9 (12) : 2121 - 2125
  • [38] Simultaneously Enhanced Strength and Ductility of Al-Mg-Si Alloys during Aging Process Induced by Electro-Pulsing Treatment
    Wang, Yitong
    Zhao, Yuguang
    Xu, Xiaofeng
    Pan, Dong
    Jiang, Wenqiang
    Chong, Xueying
    MATERIALS, 2019, 12 (09)
  • [39] Microstructure characterization of as-cast Al-Mg-Si alloys with high content Li element addition
    Yang, Xiaokun
    Xiong, Baiqing
    Li, Xiwu
    Yan, Lizhen
    Li, Zhihui
    Zhang, YongAn
    Liu, Hongwei
    Yan, Hongwei
    Wen, Kai
    MATERIALS RESEARCH EXPRESS, 2019, 6 (11):
  • [40] Effect of the Addition of High Li Concentration on the Microstructure and Mechanical Properties of Al-Mg-Si Alloys with Different Mg Contents
    Xiao-Kun Yang
    Bai-Qing Xiong
    Xi-Wu Li
    Li-Zhen Yan
    Zhi-Hui Li
    Yong-An Zhang
    Ya-Nan Li
    Kai Wen
    ActaMetallurgicaSinica(EnglishLetters), 2021, 34 (12) : 1721 - 1733