Hot-Cracking Mechanism of Laser Welding of Aluminum Alloy 6061 in Lap Joint Configuration

被引:5
|
作者
Rakhi, Km [1 ]
Kang, Seunggu [1 ]
Shin, Joonghan [1 ,2 ,3 ]
机构
[1] Kongju Natl Univ, Dept Future Convergence Engn, 1223-24 Cheonandaero, Cheonan 31080, South Korea
[2] Kongju Natl Univ, Dept Mech & Automot Engn, 1223-24 Cheonandaero, Cheonan 31080, South Korea
[3] Kongju Natl Univ, Global Inst Mfg Technol GITECH, 1223-24 Cheonandaero, Cheonan 31080, South Korea
基金
新加坡国家研究基金会;
关键词
laser welding; aluminum alloy 6061 (AA6061); lap joint; cracking susceptibility; hot-cracking mechanism; ND-YAG LASER; SOLIDIFICATION CRACKING; MICROSTRUCTURE;
D O I
10.3390/ma16196426
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Laser welding, known for its distinctive advantages, has become significantly valuable in the automotive industry. However, in this context, the frequent occurrence of hot cracking necessitates further investigation into this phenomenon. This research aims to understand the hot-cracking mechanism in aluminum alloy (AA) 6061, welded using a laser beam in a lap joint setup. We used an array of material characterization methods to study the effects of processing parameters on the cracking susceptibility and to elucidate the hot-cracking mechanism. A laser power of 2000 W generated large hot cracks crossing the whole weld zone for all welding speed conditions. Our findings suggest that using a heat input of 30 J/mm significantly mitigates the likelihood of hot cracking. Furthermore, we observed that the concentrations of the alloying elements in the cracked region markedly surpassed the tolerable limits of some elements (silicon: 2.3 times, chromium: 8.1 times, and iron: 2.7 times, on average) in AA6061. The hot-cracking mechanism shows that the crack initiates from the weld root at the interface between the two welded plates and then extends along the columnar dendrite growth direction. Once the crack reaches the central region of the fusion zone, it veers upward, following the cooling direction in this area. Our comprehensive investigation indicates that the onset and propagation of hot cracks are influenced by a combination of factors, such as stress, strain, and the concentration of alloying elements within the intergranular region.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Underwater friction welding of 6061 aluminum alloy
    Sakurada, Daisuke
    Katoh, Kazuyoshi
    Tokisue, Hiroshi
    Keikinzoku/Journal of Japan Institute of Light Metals, 2002, 52 (01): : 2 - 6
  • [42] Effect of laser cleaning on mechanical properties of laser lap welded joint of SUS310S stainless steel and 6061 aluminum alloy
    Wei, Pengyu
    Chen, Zihang
    Wang, Dan
    Zhang, Ruonan
    Li, Xinyan
    Zhang, Feng
    Sun, Kailin
    Lei, Yucheng
    MATERIALS LETTERS, 2021, 291
  • [43] Microstructure and Mechanical Properties of 6061 Aluminum Alloy by Laser Welding with Filling Wire
    Xu Fei
    Guo Yafei
    Gong Shuili
    Chen Li
    Guo Luyun
    MACHINERY, MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, 2012, 510 : 585 - +
  • [44] An investigation on hot-cracking mechanism of Sr addition into Mg-6Al-0.5Mn alloy
    Li, Shuang-Shou
    Tang, Bin
    Jin, Xin-Yan
    Zeng, Da-Ben
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (04) : 2000 - 2004
  • [45] Formation Mechanism of 6009 Aluminum Alloy Joint by Laser-MIG Arc Hybrid Welding
    Zhang, Defen
    Han, Jinli
    Chen, Xiaowen
    Yang, Yang
    Tang, Yu
    ADVANCES IN ENERGY AND ENVIRONMENTAL MATERIALS, 2018, : 329 - 340
  • [46] Direct Analysis of Solidification-Mode During Welding for the Assessment of Hot-Cracking
    Terasaki, Hidenori
    Komizo, Yu-ichi
    IN-SITU STUDIES WITH PHOTONS, NEUTRONS AND ELECTRONS SCATTERING, 2010, : 77 - 83
  • [47] Lap Joint of 6061 Aluminum Alloy Sheet and DP590 Steel Sheet by Magnetic Pulse Welding and Characterization of Its Interfacial Microstructure
    Itoi, Takaomi
    Inoue, Shoichi
    Nakamura, Kouki
    Kitta, Syunichi
    Okagawa, Keigo
    MATERIALS TRANSACTIONS, 2019, 60 (01) : 121 - 129
  • [48] RETRACTED: Microstructure and Fatigue Properties of 6061 Aluminum Alloy Laser-MIG Hybrid Welding Joint (Retracted Article)
    Fan, Cong
    Yang, Shanglei
    Zhu, Minqi
    Bai, Yishan
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2021, 2021
  • [49] Comparative investigation on single laser beam and dual laser beam for lap welding of aluminum alloy
    Chen, Lin
    Mi, Gaoyang
    Zhang, Xiong
    Wang, Chunming
    JOURNAL OF LASER APPLICATIONS, 2020, 32 (04)
  • [50] Cracking susceptibility and joint property study of the 6061 aluminum
    Xue, Xiaohuai
    Du, Hua
    Yu, Hailiang
    Yang, Shufang
    Deng, Zhengcai
    Lou, Songnian
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 911 - +