Study of hybrid isocyanate and high-mono-hydroxymethyl urea content urea-formaldehyde resins

被引:0
|
作者
Han, Chenyu [1 ]
Luo, Zhengmei [1 ]
Su, Xinlong [1 ]
Chen, Yanhua [1 ]
Yang, Zhaojin [2 ]
Mao, An [3 ]
Lei, Hong [1 ]
Zhou, Xiaojian [1 ]
Wan, Hui [1 ]
Du, Guanben [1 ]
机构
[1] Southwest Forestry Univ, Yunnan Prov Key Lab Wood Adhes & Glued Prod, Kunming, Yunnan, Peoples R China
[2] Kunming Feilin Panel Board Co Ltd, Qual Control Dept, Kunming, Yunnan, Peoples R China
[3] Shandong Agr Univ, Coll Forestry, Tai An, Shandong, Peoples R China
基金
中国国家自然科学基金;
关键词
bonding strength; hot pressing process; isocyanate; mono-hydroxymethylurea; reaction rate; urea-formaldehyde resin; CURING BEHAVIOR; ADHESIVE;
D O I
10.1002/app.53378
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Based on the difference in the reaction rate of different groups of urea-formaldehyde resins and isocyanate resins, this study designed two different urea-formaldehyde resins: a normal urea-formaldehyde resin (UF) and one with high mono-hydroxymethylurea content (UF*) to react with polymeric methylene diphenyl diisocyanate (pMDI) resin. The difference in mono- and di-hydroxymethyl urea content between UF and UF* resins was analyzed by nuclear magnetic resonance (NMR) spectroscopy, and results showed that the mono-hydroxymethyl urea content of the UF* resin was much higher than that of the conventional UF resin. The fourier transform infrared spectrometer (FTIR) analysis of differences between UF* and UF resin showed that the UF* process did not change the main structure of the conventional urea formaldehyde resin. Differential scanning calorimeter (DSC) analysis showed that the curing temperature of the hybrid UF*-pMDI resin was reduced 27.3 degrees C compared to that of the UF-pMDI resin. When these hybrid resins were used to bond plywood respectively, test results showed that the UF*-pMDI resin improved the dry and wet bonding strength by 2.6% and 3.9%, respectively, compared with the UF-pMDI resin under the condition of hot pressing time (3 min) and temperature (140 degrees C), meeting the requirement of Chinese standard of GB/T 9846-2015 for Class III board. This study provides a new path for further improving the performance and design of hybrid resins based on isocyanate and urea-formaldehyde resin.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Pyrolysis of melamine-formaldehyde and urea-formaldehyde resins
    Hirata, Toshimi
    Kawamoto, Sumire
    Okuro, Akio
    Journal of Applied Polymer Science, 1991, 42 (12): : 3147 - 3163
  • [32] FORMALDEHYDE LIBERATION AND CURE BEHAVIOR OF UREA-FORMALDEHYDE RESINS
    MYERS, GE
    KOUTSKY, JA
    HOLZFORSCHUNG, 1990, 44 (02) : 117 - 126
  • [33] Urea-formaldehyde (UF) adhesive resins for wood
    Dunky, M
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1998, 18 (02) : 95 - 107
  • [34] Curing of urea-formaldehyde resins on a wood substrate
    Siimer, K
    Kaljuvee, T
    Christjanson, P
    Lasn, I
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2006, 84 (01) : 71 - 77
  • [35] MODERN ANALYTIC METHODS FOR UREA-FORMALDEHYDE RESINS
    DANKELMAN, W
    WIT, JD
    HOLZ ALS ROH-UND WERKSTOFF, 1976, 34 (04) : 131 - 134
  • [36] Rheological behavior of urea-formaldehyde adhesive resins
    Christjanson, O
    Suurpere, A
    Siimer, K
    MATERIALS RESEARCH INNOVATIONS, 2005, 9 (01) : 7 - 8
  • [37] PHOTOMETRIC-DETERMINATION OF UREA-FORMALDEHYDE RESINS
    GNEEVA, VI
    BASOV, VN
    INDUSTRIAL LABORATORY, 1988, 54 (10): : 1123 - 1124
  • [38] Rheological behaviour of urea-formaldehyde adhesive resins
    Christjanson, P
    Suurpere, A
    Siimer, K
    E-POLYMERS, 2004,
  • [39] HYDROLYTIC STABILITY OF CURED UREA-FORMALDEHYDE RESINS
    MYERS, GE
    WOOD SCIENCE, 1982, 15 (02): : 127 - 138
  • [40] A Comparison of Adhesion Behavior of Urea-Formaldehyde Resins with Melamine-Urea-Formaldehyde Resins in Bonding Wood
    Park, Seongsu
    Jeong, Bora
    Park, Byung-Dae
    FORESTS, 2021, 12 (08):