Study of hybrid isocyanate and high-mono-hydroxymethyl urea content urea-formaldehyde resins

被引:0
|
作者
Han, Chenyu [1 ]
Luo, Zhengmei [1 ]
Su, Xinlong [1 ]
Chen, Yanhua [1 ]
Yang, Zhaojin [2 ]
Mao, An [3 ]
Lei, Hong [1 ]
Zhou, Xiaojian [1 ]
Wan, Hui [1 ]
Du, Guanben [1 ]
机构
[1] Southwest Forestry Univ, Yunnan Prov Key Lab Wood Adhes & Glued Prod, Kunming, Yunnan, Peoples R China
[2] Kunming Feilin Panel Board Co Ltd, Qual Control Dept, Kunming, Yunnan, Peoples R China
[3] Shandong Agr Univ, Coll Forestry, Tai An, Shandong, Peoples R China
基金
中国国家自然科学基金;
关键词
bonding strength; hot pressing process; isocyanate; mono-hydroxymethylurea; reaction rate; urea-formaldehyde resin; CURING BEHAVIOR; ADHESIVE;
D O I
10.1002/app.53378
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Based on the difference in the reaction rate of different groups of urea-formaldehyde resins and isocyanate resins, this study designed two different urea-formaldehyde resins: a normal urea-formaldehyde resin (UF) and one with high mono-hydroxymethylurea content (UF*) to react with polymeric methylene diphenyl diisocyanate (pMDI) resin. The difference in mono- and di-hydroxymethyl urea content between UF and UF* resins was analyzed by nuclear magnetic resonance (NMR) spectroscopy, and results showed that the mono-hydroxymethyl urea content of the UF* resin was much higher than that of the conventional UF resin. The fourier transform infrared spectrometer (FTIR) analysis of differences between UF* and UF resin showed that the UF* process did not change the main structure of the conventional urea formaldehyde resin. Differential scanning calorimeter (DSC) analysis showed that the curing temperature of the hybrid UF*-pMDI resin was reduced 27.3 degrees C compared to that of the UF-pMDI resin. When these hybrid resins were used to bond plywood respectively, test results showed that the UF*-pMDI resin improved the dry and wet bonding strength by 2.6% and 3.9%, respectively, compared with the UF-pMDI resin under the condition of hot pressing time (3 min) and temperature (140 degrees C), meeting the requirement of Chinese standard of GB/T 9846-2015 for Class III board. This study provides a new path for further improving the performance and design of hybrid resins based on isocyanate and urea-formaldehyde resin.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Urea-formaldehyde resins and free formaldehyde content
    Vargha, V
    ACTA BIOLOGICA HUNGARICA, 1998, 49 (2-4): : 463 - 477
  • [2] Urea-Formaldehyde Resins and Free Formaldehyde Content
    Viktória Vargha
    Acta Biologica Hungarica, 1998, 49 : 463 - 477
  • [3] Microencapsulation of polymeric isocyanate for the modification of urea-formaldehyde resins
    Lubis, Muhammad Adly Rahandi
    Park, Byung-Dae
    Lee, Sang-Min
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2020, 100
  • [4] UREA-FORMALDEHYDE RESINS
    EISELE, W
    WITTMANN, O
    KUNSTSTOFFE-GERMAN PLASTICS, 1980, 70 (10): : 687 - 689
  • [5] UREA-FORMALDEHYDE RESINS
    JOHNS, WE
    DUNKER, AK
    ACS SYMPOSIUM SERIES, 1986, 316 : 76 - 86
  • [6] Decreasing the Content of Free Formaldehyde in Urea-Formaldehyde Resins
    V. Z. Maslosh
    V. V. Kotova
    O. V. Maslosh
    Russian Journal of Applied Chemistry, 2005, 78 : 685 - 687
  • [7] Decreasing the content of free formaldehyde in urea-formaldehyde resins
    Maslosh, VZ
    Kotova, VV
    Maslosh, OV
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2005, 78 (04) : 685 - 687
  • [8] DISTRIBUTION OF PRODUCTS OF UREA-FORMALDEHYDE CONDENSATION AND OF AGING OF UREA-FORMALDEHYDE RESINS
    BRAUN, D
    BAYERSDORF, F
    ANGEWANDTE MAKROMOLEKULARE CHEMIE, 1980, 89 (AUG): : 183 - 200
  • [9] THE STRUCTURE OF UREA-FORMALDEHYDE RESINS
    JADA, SS
    JOURNAL OF APPLIED POLYMER SCIENCE, 1988, 35 (06) : 1573 - 1592
  • [10] STRUCTURE OF UREA-FORMALDEHYDE RESINS
    SLONIM, IY
    ALEKSEEVA, SG
    URMAN, YG
    ARSHAVA, BM
    AKSELROD, BY
    GURMAN, IM
    SMIRNOVA, LN
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA B, 1977, 19 (03): : 163 - 163