Experimental and FEM investigation of adhesion strength of dental ceramic to milled and SLM fabricated Ti6Al4V alloy

被引:7
|
作者
Dikova, Tsanka [1 ]
Maximov, Jordan [2 ]
Gagov, Yavor [1 ]
机构
[1] MU Prof Dr Paraskev Stoyanov Varna, Fac Dent Med, 84 Tsar Osvoboditel Blvd, Varna 9000, Bulgaria
[2] Tech Univ Gabrovo, Fac Mech Engn, 4 Hadji Dimitar Str, Gabrovo 5300, Bulgaria
关键词
Dental ceramic; Titanium alloy; CAD/CAM milling; SLM; Adhesion strength; FEM and test; BOND STRENGTH; PORCELAIN; TITANIUM; COATINGS;
D O I
10.1016/j.engfracmech.2023.109528
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
The aim of the present paper is to investigate the adhesion strength of dental ceramic to milled and selective laser melted (SLM) Ti6Al4V alloy by experiment and finite element method (FEM). The experimental study was done by three-point bending test. Before applying the porcelain, the metal surface was treated by sandblasting, application of bonding agent and a combination of sandblasting and bonding layer. The novelty is that FEM simulations of individual samples from each group were conducted using the experimental load-strain graphs. The normal, tangential and equivalent von Mises stresses at endpoint of the edge of porcelain coating and bonding agent sublayer were determined. It was found that the distribution of the equivalent stresses along the porcelain edge on the porcelain/metal interface is uneven: low stresses at both ends and maximum value in the central part. The Y-axis normal stresses, acting perpendicular to the porcelain/metal, bond/metal, or porcelain/bond interface, have greatest values which is primary reason the coating to be adhesively delaminated by peeling the porcelain off the metal or bonding agent. For the milled specimens, the stress trend follows the adhesion strength trend. In the combined treatment, the highest equivalent and normal stresses are generated in the bond sub-layer. If they are higher than the cohesive strength of the ceramic, the porcelain coating is destroyed cohesively by cracking. For the SLM fabricated specimens, the bond treatment increased the stresses at the bond/metal interface, and the stresses at the bond/porcelain interface were commensurate with the experimental adhesion strength. This causes the destruction of the coating to occur by peeling the porcelain off the bonding agent.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Microstructure and properties of metal/ceramic and ceramic/ceramic multilayer coatings on titanium alloy Ti6Al4V
    Wiecinski, P.
    Smolik, J.
    Garbacz, H.
    Bonarski, J.
    Mazurkiewicz, A.
    Kurzydlowski, K. J.
    SURFACE & COATINGS TECHNOLOGY, 2017, 309 : 709 - 718
  • [42] Thermal cycling In (α+β) Ti6Al4V alloy
    M. N. Mungole
    Rahul Kanojiya
    Rakesh Sharma
    Bijayani Panda
    Transactions of the Indian Institute of Metals, 2008, 61 : 93 - 97
  • [43] Thermal Cycling In (α+β) Ti6Al4V Alloy
    Mungole, M. N.
    Kanojiya, Rahul
    Sharma, Rakesh
    Panda, Bijayani
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2008, 61 (2-3) : 93 - 97
  • [44] Hydrogenation Behavior of Ti6Al4V Alloy
    Yuan Baoguo
    Wang Yujie
    Zheng Yubin
    Gong Longqing
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (06) : 1486 - 1490
  • [45] Multiaxial fatigue behavior of SLM Ti6Al4V alloy under different loading conditions
    Renzo, Danilo A.
    Sgambitterra, Emanuele
    Maletta, Carmine
    Furgiuele, Franco
    Biffi, Carlo A.
    Fiocchi, Jacopo
    Tuissi, Ausonio
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2021, 44 (10) : 2625 - 2642
  • [46] Cryogenic turning of Ti6Al4V alloy
    Sola, R.
    Veronesi, P.
    METALLURGIA ITALIANA, 2020, 112 (7-8): : 28 - 36
  • [47] Pack Siliconizing of Ti6Al4V Alloy
    Efe, G. Celebi
    Ipek, M.
    Bindal, C.
    Zeytin, S.
    ACTA PHYSICA POLONICA A, 2017, 132 (03) : 760 - 762
  • [48] Ultrasonic fatigue testing in as-built and polished Ti6Al4V alloy manufactured by SLM
    da Costa, Pedro R.
    Sardinha, Manuel
    Reis, Luis
    Freitas, Manuel
    Fonte, Manuel
    FORCES IN MECHANICS, 2021, 4
  • [49] Relevant Aspects of Piranha Passivation in Ti6Al4V Alloy Dental Meshes
    Cruz, Nuno
    Gil, Javier
    Punset, Miquel
    Manero, Jose Maria
    Tondela, Joao Paulo
    Verdeguer, Pablo
    Aparicio, Conrado
    Ruperez, Elisa
    COATINGS, 2022, 12 (02)
  • [50] Barbed Dental Ti6Al4V Alloy Screw: Design and Bench Testing
    Lovera-Prado, Keila
    Vanaclocha, Vicente
    Atienza, Carlos M.
    Vanaclocha, Amparo
    Jorda-Gomez, Pablo
    Saiz-Sapena, Nieves
    Vanaclocha, Leyre
    MATERIALS, 2023, 16 (06)