Thermal Fatigue Resistance Studies of Multilayer CrN and AlTiN Coatings Deposited on Plasma Nitrided H-13 Hot Work Steel

被引:2
|
作者
Gurada, Chetan [1 ]
Mundotia, Rajesh [2 ]
Mhatre, Umesh [2 ]
Kale, Ashwin [2 ]
Kothari, Dushyant [1 ]
机构
[1] Univ Mumbai, Dept Phys, Mumbai 400098, Maharashtra, India
[2] Surface Modificat Technol Pvt Ltd, Sativali Rd, Palghat 401208, Maharashtra, India
关键词
duplex-treatment; corrosion; die-casting; hot work steel; plasma nitriding; PVD coatings; thermal fatigue; wear rate; hardness; CATHODIC ARC TECHNIQUE; MECHANICAL-PROPERTIES; OXIDATION RESISTANCE; ELASTIC-MODULUS; WEAR BEHAVIOR; CUTTING TOOLS; DUPLEX; PVD; H13; ALUMINUM;
D O I
10.3390/lubricants11010019
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
H-13 steel surface was duplex-treated using Plasma Nitriding (PN) and PVD coatings to solve the thermal fatigue problem faced in die-casting applications. Chromium-based multilayer CrN/Cr (m-CrN) coatings and multi-component aluminium-titanium-based AlTiN (m-AlTiN) coatings were deposited using a cathodic arc deposition technique after plasma nitriding the H-13 steel surface with different case-depths of 50 mu m and 200 mu m. The structural, tribological, corrosion, and mechanical properties of the duplex-treated samples were studied. The thermal fatigue (TF) test was conducted by heating the sample to 600 degrees C and rapidly cooling it to room temperature, simulating the die-casting process conditions. After multiple cycles, it was observed that the oxide layer thickness formed was lower on duplex-treated samples compared to that on the uncoated plasma nitride sample. In addition, the mechanical properties were improved with the increase in PN diffusion depth. The duplex-treated samples showed better mechanical and thermal fatigue properties compared to untreated and only coated samples. The sample with m-AlTiN deposited on plasma nitrided H-13 with 200 mu m case depth displays better thermal fatigue properties compared to the other samples.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Fatigue resistance of CrN thin films deposited by arc evaporation process on H11 tool steel and 2205 duplex stainless steel
    Baragetti, S
    Gelfi, M
    La Vecchia, GM
    Lecis, N
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2005, 28 (07) : 615 - 621
  • [32] The composite of nitrided steel of H13 and TiN coatings by plasma duplex treatment and the effect of pre-nitriding
    Ma, SL
    Li, YH
    Xu, KW
    SURFACE & COATINGS TECHNOLOGY, 2001, 137 (2-3): : 116 - 121
  • [33] EFFECT OF PLASMA NITRIDING ON THE PROPERTIES OF (TI, AL)N COATINGS DEPOSITED ONTO HOT WORK STEEL SUBSTRATES
    GREDIC, T
    ZLATANOVIC, M
    POPOVIC, N
    BOGDANOV, Z
    THIN SOLID FILMS, 1993, 228 (1-2) : 261 - 266
  • [34] Micro-abrasion wear testing of PVD TiN coatings on untreated and plasma nitrided AISI H 13 steel
    Batista, JCA
    Joseph, MC
    Godoy, C
    Matthews, A
    WEAR, 2001, 249 (10-11) : 971 - 979
  • [35] Thermal Fatigue Behavior of Nitrocarburized and Low Pressure Nitrided Modified JIS SKD61 Hot Work Mold Steel
    Yeh, Shu-Hung
    Chiu, Liu-Ho
    Lo, Wan-Chung
    Huang, Chien-Lung
    MATERIALS TRANSACTIONS, 2013, 54 (07) : 1187 - 1194
  • [36] Temperature dependent erosion and Raman analyses of arc-deposited H free thick DLC coating on Cr/CrN coated plasma nitrided steel
    Bonu, Venkataramana
    Srinivas, G.
    Kumar, V. Praveen
    Joseph, Anjana
    Narayana, Chandrabhas
    Barshilia, Harish C.
    SURFACE & COATINGS TECHNOLOGY, 2022, 436
  • [37] Thermal stability and wear resistance of hard TiN/TiCN coatings on plasma nitrided PH15-5 steel
    Zukerman, I.
    Raveh, A.
    Kalman, H.
    Klemberg-Sapieha, J. E.
    Martinu, L.
    WEAR, 2007, 263 (1249-1252) : 1249 - 1252
  • [38] Effects of deep cryogenic treatment on the microstructure evolution, mechanical and thermal fatigue properties of H13 hot work die steel
    Li, Jun
    Zhang, Xu
    Bu, Hengyong
    Qi, Huarong
    Zuo, Pengpeng
    Li, Shaohong
    Li, Mengnie
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 8100 - 8118
  • [39] Effect of strain amplitude on the isothermal fatigue behavior of H13 hot work die steel
    Zhu Z.-Q.
    Ning H.
    Zuo P.-P.
    Wu X.-C.
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2021, 43 (05): : 656 - 662
  • [40] Influence of plasma peening on oxidation of H13 hot work steel in water vapor
    Min, YA
    Xu, X
    Wu, XC
    Li, L
    Xu, LP