Observation of the Hydrogen-Dislocation Interactions in a High-Manganese Steel after Hydrogen Adsorption and Desorption

被引:5
|
作者
An, Dayong [1 ]
Zhou, Yuhao [2 ]
Xiao, Yao [2 ]
Liu, Xinxi [1 ]
Li, Xifeng [1 ]
Chen, Jun [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Dept Plast Technol, Shanghai 200030, Peoples R China
[2] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Hydrogen embrittlement; Stacking fault; Dislocation movement; High-manganese steel; Electron channeling contrast imaging (ECCI); EMBRITTLEMENT; BEHAVIOR; PLASTICITY; PATTERNS; FE;
D O I
10.1007/s40195-022-01426-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Hydrogen embrittlement (HE) poses a significant challenge for the development of high-strength metallic materials. However, explanations for the observed HE phenomena are still under debate. To shed light on this issue, here we investigated the hydrogen-defect interaction by comparing the dislocation structure evolution after hydrogen adsorption and desorption in a Fe-28Mn-0.3C (wt%) twinning-induced plasticity steel with an austenitic structure using in situ electron channeling contrast imaging. The results indicate that hydrogen can strongly affect dislocation activities. In detail, hydrogen can promote the formation of stacking faults with a long dissociation distance. Besides, dislocation movements are frequently observed during hydrogen desorption. The required resolved shear stress is considered to be the residual stresses rendered by hydrogen segregation. Furthermore, the microstructural heterogeneity could lead to the discrepancy of dislocation activities even within the same materials.
引用
收藏
页码:1105 / 1112
页数:8
相关论文
共 50 条
  • [31] Performance analysis of hydrogen blowing in high manganese stainless steel smelting
    Xu, Hao
    Liu, Jianhua
    He, Yang
    Liu, Hongbo
    CLEAN TECHNOLOGIES AND ENVIRONMENTAL POLICY, 2023, 25 (07) : 2377 - 2391
  • [32] Development of an austenitic chromium-manganese steel with high hydrogen resistance
    V. I. Tkachov
    L. M. Ivas’kevych
    V. I. Vytvyts’kyi
    Materials Science, 2005, 41 : 673 - 679
  • [33] Development of an austenitic chromium-manganese steel with high hydrogen resistance
    Tkachov, VI
    Ivas'kevych, LM
    Vytvyts'kyi, VI
    MATERIALS SCIENCE, 2005, 41 (05) : 673 - 679
  • [34] Hydrogen desorption change after deformation of a bainitic steel with unstable retained austenite
    Pu, S. D.
    Turk, A.
    Lenka, S.
    Ooi, S. W.
    SCRIPTA MATERIALIA, 2019, 170 : 38 - 42
  • [35] The regulation of dislocation and precipitated phase improving hydrogen embrittlement resistance of pipeline steel in high pressure hydrogen environment
    Zhou, Chengshuang
    Jiang, Changcheng
    Jin, Yan
    Zhou, Hongbin
    Qiu, Qingxiong
    Hu, Yuqing
    Xie, Yuchen
    Zhang, Lin
    Zheng, Jinyang
    INTERNATIONAL JOURNAL OF FATIGUE, 2025, 190
  • [36] Study of the hydrogen traps in a high strength TRIP steel by Thermal Desorption Spectroscopy
    Escobar, D. Perez
    Duprez, L.
    Verbeken, K.
    Verhaege, M.
    THERMEC 2011, PTS 1-4, 2012, 706-709 : 2253 - 2258
  • [37] Adsorption/Desorption of mono- and diblock copolymers on surfaces using specific hydrogen bonding interactions
    Sanyal, A
    Norsten, TB
    Uzun, O
    Rotello, VM
    LANGMUIR, 2004, 20 (14) : 5958 - 5964
  • [38] Influence of Hydrogen on Delayed Fracture in High-Manganese Twinning-Induced Plasticity Steels and Advanced High-Strength Steels
    Rajput, Ajeet Singh
    JOM, 2025,
  • [39] Microstructural Effect on Hydrogen Embrittlement of High Nitrogen Chromium-Manganese Steel
    Panchenko, M. Yu
    Nifontov, A. S.
    Astafurova, E. G.
    PHYSICAL MESOMECHANICS, 2022, 25 (05) : 453 - 465
  • [40] Enhancing hydrogen embrittlement resistance of high manganese steel by warm rolling process
    Li, Yifeng
    Cheng, Zhaoyi
    Xia, Yuanguang
    Xu, Juping
    Liu, Shulin
    Chen, Huaican
    Yin, Wen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 925