Predicting degradation of composite-titanium adhesively bonded joints exposed to seawater environment

被引:4
|
作者
Wang, Jian [1 ,2 ]
Gao, Jiaxin [3 ]
Jiang, Junxia [1 ,2 ]
Bi, Yunbo [1 ,2 ]
机构
[1] Zhejiang Univ, Sch Mech Engn, State Key Lab Fluid Power & Mechatron Syst, Hangzhou 310027, Peoples R China
[2] Zhejiang Univ, Sch Mech Engn, Key Lab Adv Mfg Technol Zhejiang Prov, Hangzhou 310027, Peoples R China
[3] Zhejiang Univ, Ocean Coll, Hangzhou 310027, Peoples R China
基金
中国国家自然科学基金;
关键词
Prediction method; Composite-titanium adhesively bonded; structures; Degradation; Spatial variation; DURABILITY PREDICTION; MOISTURE ABSORPTION; FRP/STEEL JOINTS; CSM-LAMINATE; TEMPERATURE; MODEL;
D O I
10.1016/j.engstruct.2023.116993
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this paper, focusing on the composite-titanium adhesively bonded structures aging in seawater environment, a prediction method coupling the experiments, theoretical model and numerical simulation for degradation of the tensile behavior of adhesively bonded joint was proposed. Bulk adhesive and fracture specimens were aged in 45 celcius artificial seawater to characterize the adhesive moisture absorption behavior and degraded fracture properties, respectively. Based on the discrete experimental degraded fracture properties, a theoretical continuous water coupled fracture model for the prediction of degraded fracture properties was developed. The theoretical model can predict the degraded fracture toughness based on the moisture. Prediction of the degraded tensile properties of single-lap adhesively bonded joint was conducted. The predicted tensile strength of the aging specimen agreed well with the experimental results, with less than 5 % error. Moreover, spatial variations of the damage and stress of the aging adhesive layer can be predicted by the prediction method coupling the moisture absorption. The predicted results indicated that the damage value and area of the width edge of the adhesive layer were both greater than central region, and the predicted peak stress in the central region was nearly 33.2 MPa while that of the edge decreased to 12.5 MPa.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Ultrasonic characterization of accelerated environmental degradation of adhesively bonded joints
    Rokhlin, SI
    Baltazar, A
    Xie, B
    Chen, J
    ADHESIVE JOINTS: FORMATION, CHARACTERISTICS AND TESTING, VOL 2, 2002, : 337 - 360
  • [32] A NUMERICAL STUDY OF ADHESIVELY BONDED COMPOSITE PANEL FLANGE JOINTS
    TONG, LY
    SHEPPARD, A
    KELLY, D
    COMPOSITE STRUCTURES, 1994, 28 (04) : 449 - 458
  • [33] Experimental Research on Shearing Strength of Adhesively Bonded Composite Joints
    Shi, Xin-Hong
    Wang, Kang-Kang
    International Conference on Mechanics, Building Material and Civil Engineering (MBMCE 2015), 2015, : 247 - 251
  • [34] Fracture Behaviour of Adhesively Bonded Joints in Sandwich Composite Beams
    Shahin, Khaled
    Taheri, Farid
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2009, 23 (10-11) : 1531 - 1546
  • [35] Experimental determination of fracture toughness for adhesively bonded composite joints
    Senthil, K.
    Arockiarajan, A.
    Palaninathan, R.
    ENGINEERING FRACTURE MECHANICS, 2016, 154 : 24 - 42
  • [36] Tensile failure of adhesively bonded CFRP composite scarf joints
    Kumar, S. B.
    Sridhar, I.
    Sivashanker, S.
    Osiyemi, S. O.
    Bag, A.
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2006, 132 (1-2): : 113 - 120
  • [37] An analytical solution for the analysis of symmetric composite adhesively bonded joints
    Zou, GP
    Shahin, K
    Taheri, F
    COMPOSITE STRUCTURES, 2004, 65 (3-4) : 499 - 510
  • [38] Damage tolerance of adhesively bonded composite single lap joints
    Tong, L
    Zhu, XC
    Steven, GP
    FRACTURE AND STRENGTH OF SOLIDS, PTS 1 AND 2: PT 1: FRACTURE MECHANICS OF MATERIALS; PT 2: BEHAVIOR OF MATERIALS AND STRUCTURE, 1998, 145-9 : 537 - 542
  • [39] Crack stopping in composite adhesively bonded joints through corrugation
    Tserpes, K. I.
    Peikert, G.
    Floros, I. S.
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2016, 83 : 152 - 157
  • [40] Environmentally assisted crack growth in adhesively bonded composite joints
    Tracy, Jared
    Yin, Yikai
    Yang, Jeffrey
    Osborne, John C.
    Blohowiak, Kay Y.
    Dauskardt, Reinhold
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2017, 102 : 368 - 377