Life and failure of oriented carbon nanotubes composite electrode for resistance spot welding

被引:0
|
作者
Zheng, Zhong [1 ]
Tao, Jiafeng [1 ]
Fang, Xing [1 ]
Xue, Huan [1 ]
机构
[1] Hubei Univ Technol, Dept Mech Engn, Wuhan 430068, Hubei, Peoples R China
来源
MATERIA-RIO DE JANEIRO | 2023年 / 28卷 / 01期
基金
中国国家自然科学基金;
关键词
Carbon Nanotube; Orientation Arrangement; Resistance Spot-Weld; Electrode; Failure; MECHANICAL-PROPERTIES; DEGRADATION; CONDUCTIVITY; TEMPERATURE; ALLOYS; METAL;
D O I
10.1590/1517-7076-RMAT-2023-0005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In view of the poor weldability of electrodes in resistance spot welding (RSW) of galvanized steel sheets, the life of oriented multi-walled carbon nanotubes reinforced Cu matrix composites (Cu@MWCNTs/Cu) electrodes was studied, in which Cu coated multi-walled carbon nanotubes (MWCNTs) are arranged along the flow direction of working electric/force. By analyzing the macro/microscopic morphology, microstructure, hardness, texture and composition of the failed composite electrodes and the commercially CuCrZr electrode, the mechanism of the weldability enhancement and failure of electrodes was discussed. The results show that the life of Cu@ MWCNTs/Cu electrodes (2150 welds) is 3 times longer than that of CuCrZr electrode (600 welds), and the degradation rate is much slower. The hardness of Cu@MWCNTs/Cu electrodes is 30-40Hv higher. The content of recrystallized and recovery grains of Cu@MWCNTs/Cu electrodes is less. This is due to the pinning effect of MWCNTs, and straight and long MWCNTs are arranged along the electrical/force direction. These improve the hardness, mechanical properties, conductivity, and resistance to thermal deformation, cracking, and pitting of Cu@MWCNTs/Cu electrodes, which effectively slows down the failure rate and makes the spot welding life of Cu@MWCNTs/Cu electrodes longer. This work provides a new idea for the application of CNTs/Cu composites.
引用
收藏
页数:17
相关论文
共 50 条
  • [21] Mathematical Modeling of Electrode Cooling in Resistance Spot Welding
    Rao, Z. H.
    Liao, S. M.
    Tsai, H. L.
    Wang, P. C.
    Stevenson, R.
    WELDING JOURNAL, 2009, 88 (05) : 111S - 119S
  • [22] Characteristics of Electrode Displacement and Force in Resistance Spot Welding
    Ji, Chuntao
    Deng, Lipeng
    MATERIALS PROCESSING TECHNOLOGY, 2011, 337 : 379 - 382
  • [23] Effect of resistance spot welding parameters on electrode deformation
    Aravinthan, A
    Sivayoganathan, K
    Balendran, V
    Al-Dabass, D
    ADVANCES IN MANUFACTURING TECHNOLOGY - XIV, 2000, : 285 - 289
  • [24] Electrode Degradation in Resistance Spot Welding of Magnesium Alloy
    Lang, B.
    Sun, D. Q.
    Li, G. Z.
    Zhu, B. Q.
    ISIJ INTERNATIONAL, 2009, 49 (11) : 1744 - 1748
  • [25] 12-ELECTRODE EQUIPMENT FOR RESISTANCE SPOT WELDING
    IMOGILEVSKII, EI
    WELDING PRODUCTION, 1976, 23 (08): : 51 - 51
  • [26] Extending resistance welding electrode life
    Irving, B
    WELDING JOURNAL, 2001, 80 (11) : 58 - 61
  • [27] Extending resistance welding electrode life
    Irving, Bob
    Welding Journal (Miami, Fla), 2001, 80 (11): : 58 - 61
  • [28] Influence of the coating type in the electrode life in spot welding
    da Silva, Ramses Ferreira
    Vieira, Sergio Luiz
    SOLDAGEM & INSPECAO, 2008, 13 (02): : 105 - 110
  • [29] Influence of the coating type in the electrode life in spot welding
    Da Silva, Ramsés Ferreira
    Vieira, Sérgio Luiz
    Soldagem e Inspecao, 2008, 13 (02): : 105 - 110
  • [30] Cu/oriented-carbon nanotubes composite with ultralow thermal contact resistance
    Yu, Zunyue
    Huang, Jianguo
    Xiao, Chenglong
    Zhao, Wenru
    Zhang, Beibei
    Ren, Shubin
    Qu, Xuanhui
    MATERIALS TODAY COMMUNICATIONS, 2023, 35