Effect of post-weld heat treatments on the microstructure and mechanical properties of underwater friction stir welded joints of 7003-T4/6060-T4 aluminium alloys

被引:19
|
作者
Dong, Jialiang [1 ]
Zhang, Datong [2 ]
Zhang, Weiwen [2 ]
Cao, Genghua [3 ]
Qiu, Cheng [2 ]
机构
[1] Guizhou Minzu Univ, Sch Mat Sci & Engn, Guiyang 550025, Peoples R China
[2] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Met Mat, Guangdong Key Lab Proc & Forming Adv Met Mat, Guangzhou 510640, Guangdong, Peoples R China
[3] Guangdong Haomei New Mat Co Ltd, Guangzhou 510640, Qingyuan, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2023年 / 862卷
关键词
Post-weld heat treatment; Underwater friction stir weld; Microstructure; Mechanical properties; GRAIN-GROWTH; CELLULAR MICROSTRUCTURES; TENSILE PROPERTIES; UNIFIED THEORY; STABILITY; BEHAVIOR; RECRYSTALLIZATION; RECOVERY; 2024-T4;
D O I
10.1016/j.msea.2022.144423
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To further improve the mechanical properties of underwater friction stir welded joints of 7003/6060 aluminium alloys, post-weld heat treatment (PWHT) was carried out. The results show that the combination of water-cooling and PWHT is an efficient method to greatly improve the strength of the dissimilar joints. Through solution heat treatment followed by artificial aging (STA), the largest ultimate tensile strength (UTS) of the dissimilar joint can reach 254.0 MPa, which is equal to the UTS of 6060-T6, and the elongation of the joint is 12.7%. The improvement in strength is attributed to reprecipitation of the high density of the beta" phase. For direct artificial aging (AA) after welding, the largest UTS (218.9 MPa) is obtained when aged at 175 degrees C for 8 h. Although the pre-existing beta ' phase grows coarse to some extent, GP zones and the beta" phase are reprecipitated during AA, which leads to a great increase in joint strength compared with the as-welded samples. However, the elongation severely deteriorates to 4.4% due to strain localization caused by the decreasing width of the soft region. Abnormal grain growth (AGG) takes place in the stir zone (SZ) of all joints subjected to STA, while equiaxed grains with limited growth are retained in joints subjected to AA. Compared with the distribution of precipitation phases, the grain size plays a minor role in the mechanical properties of the dissimilar joints.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Effects of different post-weld heat treatment conditions on mechanical properties and microstructure of welded joints
    Qi, Kai
    Chen, Jingyuan
    Liu, Bin
    Wang, Fengjiang
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2022, 36 (12N13):
  • [42] Effect of post weld heat treatments on microstructure and mechanical properties of friction stir welded joints of Al-Zn-Mg alloy AA7039
    Sharma, Chaitanya
    Dwivedi, Dheerendra Kumar
    Kumar, Pradeep
    MATERIALS & DESIGN, 2013, 43 : 134 - 143
  • [43] Influence of Post-Weld Heat Treatments on Microstructure and Mechanical Properties of Laser Beam Welded 2060-T3/2099-T3Al-Li T-Joints
    Zhang, Yunlong
    Chen, Yanbin
    Tao, Wang
    Lei, Zhenglong
    Yang, Zhaohui
    Nan, Tiantian
    METALS, 2019, 9 (12)
  • [44] Effect of post-weld heat treatment on mechanical properties and microstructure in electric arc welded mild steel joints
    Aninda, Rayan Karim
    Karobi, Shazrina Mariam
    Shariar, Redwan
    Rahman, Md. Musfiqur
    Rabby, Md Insiat Islam
    JOURNAL OF ENGINEERING RESEARCH, 2024, 12 (02): : 210 - 215
  • [45] Effects of a Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of a Friction-Stir-Welded Beryllium-Copper Alloy
    Lim, Yeongseok
    Lee, Kwangjin
    Moon, Sangdon
    METALS, 2019, 9 (04):
  • [46] EFFECT OF TOOL GEOMETRY AND WELDING SPEED ON MECHANICAL PROPERTIES AND MICROSTRUCTURE OF FRICTION STIR WELDED JOINTS OF ALUMINIUM ALLOYS AA6082-T-6
    Patil, Hiralal Subhash
    Soman, Sanjay N.
    ARCHIVE OF MECHANICAL ENGINEERING, 2014, 61 (03) : 455 - 468
  • [47] Impact of post weld heat treatment on mechanical and microstructural properties of underwater friction stir spot welded 6061 aluminium alloy
    Shekhawat, Ravindra S.
    Nadakuduru, Vijay N.
    MATERIALS TODAY-PROCEEDINGS, 2022, 56 : 2647 - 2652
  • [48] Effect of post-weld heat treatment on mechanical properties and fatigue crack growth behaviour of friction stir welded 7075-T651 Al alloy
    Joshi A.
    Gope A.
    Chandra Gope P.
    Theoretical and Applied Fracture Mechanics, 2023, 123
  • [49] Influences of Post-weld Heat Treatments on Friction Stir-welded AZ31B Magnesium Alloy Joints
    Guo Wei
    Wang Kuaishe
    Wang Wen
    Wang Feng
    Wang Wenli
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (06) : 1075 - 1078
  • [50] Microstructure and mechanical properties of friction stir welded 6082 AA in as welded and post weld heat treated conditions
    El-Danaf, Ehab A.
    El-Rayes, Magdy M.
    MATERIALS & DESIGN, 2013, 46 : 561 - 572