Fatigue and Fracture Evaluations in Ti-10V-2Fe-3Al (Ti 10-2-3)

被引:3
|
作者
Bache, Martin [1 ]
机构
[1] Swansea Univ, Inst Struct Mat, Fac Sci & Engn, Swansea SA1 8EN, Wales
关键词
Ti; 10-2-3; low cycle fatigue; crack growth; salt fog environment; notches; TITANIUM-ALLOY;
D O I
10.3390/met13121986
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A mechanical assessment was conducted to characterise the near beta titanium alloy Ti-10V-2Fe-3Al (Ti 10-2-3), which was heat-treated to provide two strength variants. Low cycle fatigue and crack propagation tests were performed under standard laboratory air plus a salt fog environment. The differences in static strength were also demonstrated under fatigue conditions utilising plain specimens. However, the alloy was essentially insensitive to the test environment when comparing LCF performance in air and salt fog. Salt fog also provided no effect on crack growth behaviour. A double edge notch specimen geometry was employed to measure free initiation and the growth of cracks from a stress-raising feature. The current data now supplement previous studies aimed at expanding the mechanical database for Ti 10-2-3 component design and in-service life predictions.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] The Ageing Behavior of Titanium Alloy Ti-10V-2Fe-3Al
    Al-Salihi, Huda
    Bettles, Colleen
    Muddle, Barry
    PRICM 7, PTS 1-3, 2010, 654-656 : 843 - 846
  • [22] LASER SURFACE MELTING OF TI-10V-2FE-3AL ALLOY
    ABBOUD, JH
    WEST, DRF
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1992, 11 (19) : 1322 - 1326
  • [23] PROPERTY OPTIMIZATION OF TI-10V-2FE-3AL BY MICROSTRUCTURE MODIFICATION
    MARTORELL, IA
    MAHAJAN, YR
    EYLON, D
    FROES, FH
    JOURNAL OF METALS, 1985, 37 (08): : A75 - A75
  • [24] Cyclic softening of the Ti-10V-2Fe-3Al titanium alloy
    Luquiau, D
    Feaugas, X
    Clavel, M
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 224 (1-2): : 146 - 156
  • [25] The powder sintering and isothermal forging of Ti-10V-2Fe-3Al
    Guo, Hongzhen
    Zhao, Zhanglong
    Duan, Chunyan
    Yao, Zekun
    JOM, 2008, 60 (11) : 47 - 49
  • [26] Ti-10V-2Fe-3Al合金的再结晶
    胡大为
    潘雅琴
    吴云书
    金属学报 , 1987, (03) : 240 - 242
  • [27] PROCESSING PROPERTIES RELATIONSHIPS OF TI-10V-2FE-3AL FORGINGS
    BOYER, RR
    KUHLMAN, GW
    JOURNAL OF METALS, 1985, 37 (08): : A75 - A75
  • [28] HIGH-TEMPERATURE DEFORMATION OF TI-10V-2FE-3AL
    OGAWA, A
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 (05): : S757 - S757
  • [29] The powder sintering and isothermal forging of Ti-10V-2Fe-3Al
    Hongzhen Guo
    Zhanglong Zhao
    Chunyan Duan
    Zekun Yao
    JOM, 2008, 60 : 47 - 49
  • [30] COMPACTION AND MECHANICAL PROPERTY EVALUATION OF GAS ATOMIZED TI-10V-2FE-3AL AND TI-10V-2FE-3AL+(ER2O3)
    SMITH, PR
    WEISS, I
    YOLTON, CF
    FROES, FH
    JOURNAL OF METALS, 1987, 39 (10): : A11 - A11