Hot Ductility of Severe Plastic Deformed AA6061 Aluminum Alloy

被引:0
|
作者
Ali Akbar Khamei [1 ]
Kamran Dehghani [1 ]
机构
[1] Mining and Metallurgical Engineering Department,Amirkabir University of Technology
关键词
Al-Mg-Si alloy; Deformation behavior; Equal channel angular pressing(ECAP); Rolling; Hot tensile deformation;
D O I
暂无
中图分类号
TG146.21 [];
学科分类号
080502 ;
摘要
The hot ductility of 6061 aluminum alloy,which was subjected to two different severe plastic deformations(SPD),was studied at different temperatures and strain rates.The tensile tests were carried out at the temperature range of 300-500 ℃ and at the strain rates of 0.0005-0.01 s.The microstructure evolution was characterized using optical microscopy,transmission electron microscopy and X-ray diffraction technique.The influences of the microstructure after SPD,thermomechanical parameters(temperature and strain rate) and specimen size on the hot formability of this alloy were then analyzed.The results show that a decrease in grains/subgrains exhibited significant effect on the hot ductility of SPDed samples.The constitutive equations were then developed to model the hot formability of the studied alloy.The developed model can be represented by Zener-Hollomon parameter in a hyperbolic sinusoidal equation form.Both the changes of elongation to failure and Zener-Hollomon parameter indicate that the hot ductility of the alloy is more sensitive to the temperature rather than to the strain rate.The uniform elongation is independent of the specimen size,but the postnecking elongation increases dramatically as the ratio of l/Adecreases.
引用
收藏
页码:322 / 330
页数:9
相关论文
共 50 条
  • [31] Microstructure and Mechanical Properties of Cold Roll-Bonded Layered AA6061/AA5052/AA6061/AA5052 Aluminum Alloy Sheet
    Jo, Sang-Hyeon
    Park, Bo-Bae
    Lee, Seong-Hee
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2022, 32 (03): : 161 - 167
  • [32] Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy
    Zaid, B.
    Saidi, D.
    Benzaid, A.
    Hadji, S.
    CORROSION SCIENCE, 2008, 50 (07) : 1841 - 1847
  • [33] MICROSTRUCTURE AND HARDNESS OF EXTRUSION WELDING ON HOLLOW PANEL AA6061 ALUMINUM ALLOY
    Sutowijoyo, A. B. P.
    Putri, E. D. W. S.
    Muhayat, N.
    Prabowo, A. R.
    Depari, Y. P. D. S.
    Triyono
    METALURGIJA, 2025, 64 (1-2): : 17 - 19
  • [34] FATIGUE BEHAVIOR OF A SAFFIL-REINFORCED ALUMINUM-ALLOY (AA6061)
    LEVIN, M
    KARLSSON, B
    COMPOSITES, 1993, 24 (03): : 288 - 295
  • [35] HOT FORMABILITY OF AA 6061 PM ALUMINUM-ALLOY
    EVANGELISTA, E
    FORCELLESE, A
    GABRIELLI, F
    MENGUCCI, P
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1990, 24 : 323 - 332
  • [36] Solid state recycling of aluminium AA6061 alloy chips by hot extrusion
    Abd El Aal, Mohamed Ibrahim
    Taha, Mohamed Adel
    Selmy, A., I
    El-Gohry, A. M.
    Kim, H. S.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (03):
  • [37] Local Deformation and Texture of Cold-Rolled AA6061 Aluminum Alloy
    Zhou, Diaoyu
    Du, Wenwen
    Wen, Xiyu
    Qiao, Junwei
    Liang, Wei
    Yang, Fuqian
    MATERIALS, 2018, 11 (10)
  • [38] Effect of surface morphology on the adhesion of silicone elastomers on AA6061 aluminum alloy
    Grard, A.
    Belec, L.
    Perrin, F. X.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2020, 102
  • [39] Properties of AA6061 aluminum alloy reinforced with different intermetallics and ceramics particles
    da Costa, Cesar Edil
    de Aguiar, Luana
    Borras, Vicente Amigo
    ADVANCED POWDER TECHNOLOGY V, 2006, 530-531 : 255 - +