Damage modes and mechanisms for fine woven pierce SiO2f/SiO2 composite under quasi-static compression

被引:0
|
作者
Zhang, Yawei [1 ,2 ]
Sun, Tao [1 ]
Zeng, Zhaoyong [3 ]
Peng, Siping [3 ]
Zhou, Shanyi [1 ]
机构
[1] Donghua Univ, Coll Mech Engn, Shanghai, Peoples R China
[2] Donghua Univ, State Key Lab Modificat Chem Fibers & Polymer Mat, Shanghai, Peoples R China
[3] Shanghai Radio Equipment Res Inst, Shanghai, Peoples R China
关键词
damage modes and mechanisms; FEA; fine woven pierce SiO2f/SiO2 ceramic matrix composites; interface damage; quasi-static compression; FAILURE CRITERIA; BEHAVIOR; TENSILE;
D O I
10.1111/ijac.14989
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Finite element analysis (FEA) for fine woven pierce SiO2f/SiO2 composites quasi-static compression is conducted in weft and Z yarn directions, strain-stress curves with experiments and FEA are compared, and finite element model proves to be valid. During quasi-static compression, the strain difference between matrix and fiber rise. As for compression in the weft direction, matrix micro-cracks increased into large cracks and mainly distribute around warp fibers. The interfacial stress increases and results in interface damage around the warp fiber. The stress fields are superimposed and rise in warp and weft yarns overlapping regions, in which damage modes include matrix cracks, fiber debonding, and breakage. Obvious V-shaped shear bands are formed on YZ surface. As for compression in the Z-direction, interfacial stresses around the warp and weft fibers are superposited and strengthened, fibers debonding occurs continuously with increasing interfacial stress; stress field inside composites in the Z yarn gets great, SiO2f/SiO2 composites have greater compression strength in the Z-yarn direction than that in the weft direction.
引用
收藏
页数:19
相关论文
共 50 条
  • [41] On the tensile behaviors of 2D twill woven SiO2f/SiO2 composites at ambient and elevated temperatures: Mesoscale analysis and in situ experimental investigation
    Shi, Duoqi
    Liu, Changqi
    Cheng, Zhen
    Li, Zhenlei
    Yang, Xiaoguang
    Chen, Haofeng
    CERAMICS INTERNATIONAL, 2021, 47 (09) : 12680 - 12694
  • [42] Effect of boron doping on waterproof and dielectric properties of polyborosiloxane coating on SiO2f/SiO2 composites
    Xia, Long
    Lu, Siru
    Zhong, Bo
    Huang, Longnan
    Yang, Hua
    Zhang, Tao
    Han, Haibo
    Wang, Pan
    Xiong, Li
    Wen, Guangwu
    CHINESE JOURNAL OF AERONAUTICS, 2019, 32 (08) : 2017 - 2027
  • [43] Microstructure evolution and mechanical properties of SiO2f/SiO2 composites joints brazed by bismuth glass
    Wang, Haohan
    Wang, Pengcheng
    Zhong, Zhengxiang
    Cao, Jian
    Qi, Junlei
    CERAMICS INTERNATIONAL, 2022, 48 (04) : 5840 - 5844
  • [44] Interfacial microstructure and improved wetting mechanism of SiO2f/SiO2 brazed with Nb by plasma treatment
    Lin, Jinghuang
    Ba, Jin
    Liu, Yulin
    Wang, Yiheng
    Guo, Jiale
    Luo, Dalin
    Cai, Yifei
    Mao, Deshun
    Qi, Junlei
    Feng, Jicai
    VACUUM, 2017, 143 : 320 - 328
  • [45] Effects of high-temperature annealing on microstructure and mechanical property of SiO2f/SiO2 composites
    Xiang Yang
    Cao Feng
    Cao Jie
    Chen Xiao-na
    Xiong Qiang
    VACUUM, 2017, 144 : 1 - 7
  • [46] Machining quality improvement through ice densification pretreatment during rotary ultrasonic face grinding SiO2f/SiO2 composite
    Yao, Longxu
    Liu, Zhanqiang
    Song, Qinghua
    Wang, Bing
    Cai, Yukui
    Luan, Qiang
    Wang, Hongxin
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2025, 193
  • [47] SiO2f/SiO2织物复合材料变形及弹性常数研究
    刘晓宇
    李哲
    翟奋楼
    航空制造技术, 2018, 61 (09) : 92 - 95
  • [48] Effect of boron doping on waterproof and dielectric properties of polyborosiloxane coating on SiO2f/SiO2 composites
    Long XIA
    Siru LU
    Bo ZHONG
    Longnan HUANG
    Hua YANG
    Tao ZHANG
    Haibo HAN
    Pan WANG
    Li XIONG
    Guangwu WEN
    Chinese Journal of Aeronautics, 2019, 32 (08) : 2017 - 2027
  • [49] Damage evolution and failure mechanism of 2.5D woven composite tubes under quasi-static lateral compression
    Wang, Yajuan
    Wang, Zunqing
    Wang, Xiaoxu
    Zhang, Diantang
    COMPOSITE STRUCTURES, 2025, 351
  • [50] Brazing of SiO2f/SiO2 composite to Invar using a graphene-modified Cu-23Ti braze filler
    Sun, Z.
    Zhang, L. X.
    Hao, T. D.
    Feng, J. C.
    CERAMICS INTERNATIONAL, 2018, 44 (13) : 15809 - 15816