Effects of pre-stretching on mechanical properties and corrosion behavior of superplastic formed 2A97 Al-Li alloy

被引:0
|
作者
Xu, Yaqi [1 ]
Zou, Guotong [1 ]
Li, Jun [1 ]
Chen, Shijie [1 ]
Ye, Lingying [1 ,2 ,3 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Key Lab Nonferrous Met Mat Sci & Engn, Minist Educ, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, Nonferrous Met Oriented Adv Struct Mat & Mfg Coope, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Superplastic forming; Pre-stretching; Mechanical property; Corrosion behavior; LOCALIZED CORROSION; INTERGRANULAR CORROSION; T-1; PHASE; MG ALLOY; ALUMINUM; MICROSTRUCTURE; STRENGTH; QUANTIFICATION; DEFORMATION; PROPAGATION;
D O I
10.1016/j.matchar.2025.114801
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Effects of pre-stretching on mechanical properties and corrosion behavior of superplastic formed 2A97 Al-Li alloy were investigated by using tensile test, intergranular corrosion test, electrochemical analysis, electron backscattering diffraction analysis and transmission electron microscopy. The results show that compared with T6 heat treatment, the T8 heat treatment effectively improves the strength by introducing more finer and more homogeneous T1 precipitations. And the pre-stretching strain has significant influence on the microstructure and properties of superplastic formed alloy. When the pre-stretching strain reaches 4 %, the cavities formed during superplastic forming are obviously elongated along the pre-stretching direction. During 4 %-8 % pre-stretching strain, the increment of strength gradually decreases, but the elongation drops sharply. When the pre-stretching strain reaches 8 %, the elongated cavities and cracked coarse second phases result in a slight decrease in strength. The corrosion behavior of samples after heat treatment with different pre-stretching strain are obviously different. The corrosion microscopy of T6 and T82 sample is pitting with intergranular corrosion (IGC) by the grain boundary precipitation free zones (PFZ) dissolving preferentially. After 4 %-8 % pre-stretching treatments, the corrosion microscopy is only pitting by the dissolution of the matrix around T1 precipitations. What's more, strength and corrosion resistance are both at a high level by 4 % pre-stretching treatment.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Effects of Pre-Stretching on Creep Behavior, Mechanical Property and Microstructure in Creep Aging of Al-Cu-Li Alloy
    Zhang, Jin
    Jiang, Zhen
    Xu, Fushun
    Chen, Mingan
    MATERIALS, 2019, 12 (03)
  • [22] Corrosion Behavior of Friction Stir Welded 2A97 Al-Cu-Li alloy
    Zhang, Xinxin
    Liu, Bing
    Zhou, Xiaorong
    Wang, Junjie
    Luo, Chen
    Sun, Zhihua
    Tang, Zhihui
    Lu, Feng
    CORROSION, 2017, 73 (08) : 988 - 997
  • [23] Micro-Structure and Mechanical Properties of 2A97 Al-Li Alloy Cast by Low-Frequency Electromagnetic Casting
    Wang, Fuyue
    Wang, Xiangjie
    Cui, Jianzhong
    METALS, 2019, 9 (08)
  • [24] Micro-textures of high strength 2A97 Al-Li alloy plates
    State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an, China
    Cailiao Rechuli Xuebao, 6 (53-57):
  • [25] Effect of Li Content on Properties and Microstructure Evolution of Near-Rapid Solidified 2A97 Al-Li Alloy
    Tang Yingchun
    Luo Lei
    Luo Liangshun
    Liu Yulin
    Xu Yanjin
    Su Yanqing
    Guo Jingjie
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (09) : 2737 - 2744
  • [26] Effect of Li Content on Properties and Microstructure Evolution of Near-Rapid Solidified 2A97 Al-Li Alloy
    Tang, Yingchun
    Luo, Lei
    Luo, Liangshun
    Liu, Yulin
    Xu, Yanjin
    Su, Yanqing
    Guo, Jingjie
    Fu, Hengzhi
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (09): : 2737 - 2744
  • [27] An Experimental Study on Tensile Properties of Al-Li Alloy 2198-T3 by Pre-stretching and Artificial Aging
    Choi, Dongkuk
    Lee, Gyeonghan
    Lee, Sooyong
    Lee, Junseong
    INTERNATIONAL JOURNAL OF AERONAUTICAL AND SPACE SCIENCES, 2024, 25 (01) : 92 - 101
  • [28] Comparative Study on Electrochemical Behavior of Al-Li Alloy 2A97 Machined Surfaces in Sodium Chloride Solution
    Niu, Jintao
    Liu, Zhanqiang
    Wang, Guijie
    IEEE ACCESS, 2019, 7 : 134198 - 134205
  • [29] Effects of heat treatment and pre-stretching on the mechanical properties and microstructure evolution of extruded 2050 Al-Cu-Li alloy
    Xu, Xuanxi
    Wu, Guohua
    Zhang, Liang
    Tong, Xin
    Zhang, Xiaolong
    Sun, Jiangwei
    Li, Liangbin
    Xiong, Xunman
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 845
  • [30] Effects of pre-stretching and aging process on tensile properties of 2195 Al-Cu-Li alloy
    Li, ZX
    Mirshams, R
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 1233 - 1238