Chloride permeability and chloride-induced corrosion of concrete containing lithium slag as a supplementary cementitious material

被引:0
|
作者
Amin, Md Tanvir Ehsan [1 ]
Sarker, Prabir Kumar [1 ]
Shaikh, Faiz Uddin Ahmed [1 ]
Hosan, Anwar [1 ]
机构
[1] Curtin Univ, Sch Civil & Mech Engn, Perth, Australia
基金
澳大利亚研究理事会;
关键词
Lithium slag; Supplementary cementitious material; Rapid chloride permeability test; Accelerated corrosion test; Chloride diffusion co-efficient; HIGH-PERFORMANCE CONCRETE; FLY-ASH; REINFORCEMENT CORROSION; EXPOSED CONCRETE; SERVICE LIFE; SILICA FUME; RESISTANCE; DURABILITY; STRENGTH; PENETRATION;
D O I
10.1016/j.conbuildmat.2025.140629
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The durability of concrete structures in marine environments is often compromised by chloride penetration which accelerates the corrosion of reinforcing steel. As supplementary cementitious materials (SCMs) are widely used to reduce chloride penetration in concrete, this study introduces lithium slag (LS) as an emerging SCM at 20-60 % replacement of cement. To assess its impact on chloride penetration and corrosion resistance, RCPT, chloride diffusion test and accelerated corrosion tests were conducted. The results showed that LS significantly reduced chloride penetration even at higher cement replacement levels (40-60 %) and the chloride ion penetration decreased by 76-78 % compared to that of the control mix. Among the mixes, 40 % cement replacement by LS showed the best performance with reduced rebar corrosion rates, higher electrical resistance, and lower chloride penetration over time due to its compact structure and reduced porosity. In addition, the 40LS mix also reduced the mass loss of steel bar by 25 % and crack width by 48 % in the accelerated corrosion test. Finally, the chloride diffusion coefficient was found 30 %, 49 %, and 14 % lower for the 20LS, 40LS, and 60LS samples, respectively, compared to that of the control sample. The findings demonstrate that LS is an effective SCM for enhancing chloride resistance and mitigating reinforcement corrosion in concrete.
引用
收藏
页数:14
相关论文
共 50 条
  • [41] Risk of chloride-induced corrosion of steel in SF concrete exposed to a chloride-bearing environment
    Jung, Min Sun
    Kim, Ki Beom
    Lee, Sang Ah
    Ann, Ki Yong
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 166 : 413 - 422
  • [42] Effects of AC-interference on chloride-induced corrosion of reinforced concrete
    Brenna, Andrea
    Beretta, Silvia
    Bolzoni, Fabio
    Pedeferri, MariaPia
    Ormellese, Marco
    CONSTRUCTION AND BUILDING MATERIALS, 2017, 137 : 76 - 84
  • [43] Initiation of chloride-induced reinforcement corrosion in concrete structural members - Discussion
    Mohammed, TU
    Hamada, H
    ACI STRUCTURAL JOURNAL, 2003, 100 (01) : 126 - 126
  • [44] Initiation of chloride-induced reinforcement corrosion in concrete structural members - Prediction
    Li, CQ
    ACI STRUCTURAL JOURNAL, 2002, 99 (02) : 133 - 141
  • [45] Initiation of chloride-induced reinforcement corrosion in concrete structural members - Experimentation
    Li, Chun Qing
    2001, American Concrete Institute (98)
  • [46] Potential of ladle furnace slag as supplementary cementitious material in concrete
    Sultana, Iffat
    Islam, G. M. Sadiqul
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 18
  • [47] Numerical analysis of concrete degradation due to chloride-induced steel corrosion
    Ayinde, Olawale O.
    Zuo, Xiao-Bao
    Yin, Guang-Ji
    ADVANCES IN CONCRETE CONSTRUCTION, 2019, 7 (04) : 203 - 210
  • [48] INHIBITION OF CHLORIDE-INDUCED CORROSION IN REINFORCED CONCRETE BY CALCIUM NITRITE.
    Gaidis, James M.
    Rosenberg, Arnold M.
    Cement, Concrete and Aggregates, 1987, 9 (01): : 30 - 33
  • [49] Performance of organic and inorganic substances as inhibitors for chloride-induced corrosion in concrete
    Aydin, Ozlem
    Cizmeciglu, Zeki
    MATERIALS TESTING, 2015, 57 (01) : 85 - 90
  • [50] Initiation of chloride-induced corrosion of steel in concrete: role of the interfacial zone
    Page, C. L.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2009, 60 (08): : 586 - 592