Extending interfacial toughness and thermal cycling lifetime of thermal barrier coatings via interfacial 3D pattern

被引:0
|
作者
Luo, Lirong [1 ]
Wang, Weize [2 ]
Zhang, Xiancheng [2 ]
Lu, Jie [1 ]
Guo, Fangwei [1 ]
Zhao, Xiaofeng [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai Key Lab Adv High Temp Mat & Precis Formin, Shanghai 200240, Peoples R China
[2] East China Univ Sci & Technol, Minist Educ, Sch Mech & Power Engn, Key Lab Pressure Syst & Safety, Shanghai, Peoples R China
基金
中国国家自然科学基金;
关键词
interface structure; interfacial toughness; laser deposition; thermal barrier coating; thermal cycling lifetime; CRACK DEFLECTION; STRESS; PROPAGATION; BONDCOAT;
D O I
10.1111/jace.20254
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Weak interface bonding is a critical factor that compromises the long-term durability of the thermal barrier coatings. To mitigate this, we introduce an innovative interface-strengthening approach by integrating four types of 3D patterns at the top coat/bond coat interface using the laser cladding technique. Tensile tests demonstrate a significant enhancement in interfacial bonding strength, increasing by over 139.2% from 21.6 +/- 1.7 MPa for conventional thermal barrier coatings without patterns to 51.67 MPa for the patterned coatings. Moreover, the thermal cycling lifetime has been extended by 41%, from 1026 +/- 25 cycles for the conventional coating to 1936 +/- 164 cycles for the patterned coating. This enhancement in interfacial toughness and thermal cycling lifetime is primarily because of the blocking and deflection effects of 3D patterns on interfacial crack propagation. Besides, the geometric parameters of the patterns play a crucial role in determining the failure behavior of the thermal barrier coatings. This strategy presents a practical solution for the development of durable thermal barrier coatings and provides the valuable insights for the optimization of other heterogeneous interfaces.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Evaluation of interfacial fracture toughness of thermal barrier coating under heat cycles
    Gao, L
    Nakasa, K
    Kato, M
    Nishida, H
    PROGRESS IN EXPERIMENTAL AND COMPUTATIONAL MECHANICS IN ENGINEERING, 2003, 243-2 : 267 - 272
  • [42] Effect of preexisting surface cracks on the interfacial thermal fracture of thermal barrier coatings: an experimental study
    Zhou, B
    Kokini, K
    SURFACE & COATINGS TECHNOLOGY, 2004, 187 (01): : 17 - 25
  • [43] Development of bending tests for near shear mode interfacial toughness measurement of EB-PVD thermal barrier coatings
    Vaunois, Jean-Roch
    Poulain, Martine
    Kanoute, Pascale
    Chaboche, Jean-Louis
    ENGINEERING FRACTURE MECHANICS, 2017, 171 : 110 - 134
  • [44] Effects of surface modification on thermal cycling lifetime of thermal barrier coatings with HVOF NiCrAlY bond coat
    Ni, Liyong
    Zhou, Chungen
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2012, 22 (03) : 237 - 243
  • [46] EFFECT OF BOND COAT AND SUBSTRATE CHEMISTRY ON THE INTERFACIAL DEGRADATION OF THERMAL BARRIER COATINGS
    Wu, L. T.
    Wu, R. T.
    Osada, T.
    Lee, K., I
    Bai, M.
    Xiao, P.
    PROCEEDINGS OF THE 13TH INTENATIONAL SYMPOSIUM OF SUPERALLOYS (SUPERALLOYS 2016), 2016, : 167 - 176
  • [47] Quantitative Characterization of Interfacial Defects in Thermal Barrier Coatings by Long Pulse Thermography
    Wei, Jinfeng
    Xu, Guangnan
    Liu, Guolin
    Guo, Jinwei
    Zhu, Wang
    Ma, Zengsheng
    COATINGS, 2022, 12 (12)
  • [48] Evolution of interfacial toughness of a thermal barrier system with a Pt-diffused γ/γ′ bond coat
    Zhao, X.
    Liu, J.
    Rickerby, D. S.
    Jones, R. J.
    Xiao, P.
    ACTA MATERIALIA, 2011, 59 (16) : 6401 - 6411
  • [49] Role of impact on determination of interfacial toughness measurement by indentation for thermal barrier coating systems
    Ekici, B
    SURFACE ENGINEERING, 2005, 21 (5-6) : 456 - 462
  • [50] Influence of isothermal and cyclic oxidation on the apparent interfacial toughness in thermal barrier coating systems
    Liu, Y.
    Vidal, V.
    Le Roux, S.
    Blas, F.
    Ansart, F.
    Lours, P.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2015, 35 (15) : 4269 - 4275