Elimination of surface spottiness defects and characterisation of the nitrocarburised surface for 40Cr steel

被引:0
|
作者
Fan, Dong Xu [1 ]
Liu, Cong [1 ]
Xu, Jing Sheng [1 ]
Wang, Man Fu [1 ]
机构
[1] Dalian Polytech Univ, Sch Mech Engn & Automat, Dalian 116034, Peoples R China
基金
中国国家自然科学基金;
关键词
nitrocarburising; spottiness defects; microhardness; element distribution; phase identification; STAINLESS-STEEL; CARBON-STEELS; BEHAVIOR; TEMPERATURE;
D O I
10.1177/02670844241263603
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nitrocarburising was an effective technique to enhance the surface strength of iron-based alloys and has been widely used in engineering. However, an unfavourable issue was the potential development of spottiness defects on specimen surfaces due to nitrocarburising treatment. This paper focused on the nitrocarburised 40Cr steel shafts with surface spottiness defects in production conditions. Optimisation of the production process was conducted by pre-cleaning the furnace with organic solvents before nitrocarburising treatment to address spottiness defects on the workpiece surfaces. The microhardness values of the specimens were measured, and surface characteristics were analysed using scanning electron microscope, energy-dispersive spectroscopy, and X-ray diffractometer. The surface microhardness results indicated that the specimens with spottiness defects displayed lower levels, which implied that spottiness defects were detrimental to surface microhardness. The main elements distributed on the surface of the specimens were iron, oxygen, nitrogen, and carbon. The phase identification results proved that the nitrocarburised surface layers were mainly composed of Fe3O4, Fe3C, and Fe4N. The spottiness defects were most likely caused by the accumulation of iron oxides, which hindered the diffusion of nitrogen and carbon atoms in the nitrocarburising process. As a result, the Fe3O4 levels on the surface of the optimised-treated specimens decreased, while the Fe3C and Fe4N content increased. This research served as valuable insights for enhancing the visual appearance and properties of alloy steels post nitrocarburising treatment.
引用
收藏
页码:1022 / 1028
页数:7
相关论文
共 50 条
  • [41] Tribological Behavior of Coating Cr Layer on 40Cr after Surface Electron Beam Pretreatment
    Hu, J. J.
    Wang, J.
    Jiang, P.
    Xu, H. B.
    Li, H.
    Hou, T. F.
    1ST INTERNATIONAL WORKSHOP ON MATERIALS SCIENCE AND MECHANICAL ENGINEERING, 2017, 281
  • [42] Analysis and modeling of flow stress of 40Cr steel
    Li, Xiong
    Zhang, Hong-Bing
    Ruan, Xue-Yu
    Luo, Zhong-Hua
    Zhang, Yan
    Cailiao Gongcheng/Journal of Materials Engineering, 2004, (11): : 41 - 44
  • [43] Failure analysis on 40Cr steel of dacromet bolt
    Wang, H.-Q. (wanghuiqiang666@eyou.com), 1600, Northeastern University (33):
  • [44] Fracture Analysis of 40Cr Steel Pin Roll
    Li, Yong
    Jia, Youlu
    Xie, Xianjiao
    2017 3RD INTERNATIONAL CONFERENCE ON ENVIRONMENTAL SCIENCE AND MATERIAL APPLICATION (ESMA2017), VOLS 1-4, 2018, 108
  • [45] Investigation of Prestress Hard Turning of 40Cr Steel
    Qin, Meng-Yang
    Ye, Bang-Yan
    Liu, Lei-Feng
    He, Ai-Dong
    MATERIALS AND MANUFACTURING PROCESSES, 2012, 27 (10) : 1118 - 1122
  • [46] Study on the Joint of Isothermal Superplastic Solid State Welding between Cr12MoV Steel and 40Cr Steel after Laser Surface Quenching
    Shi, Hongxin
    Wu, Zhiwei
    Sun, Jing
    Yu, Hua
    Qiu, Ranfeng
    Zhang, Keke
    MATERIALS PROCESSING TECHNOLOGIES, PTS 1 AND 2, 2011, 154-155 : 817 - 821
  • [47] A study on the impact wear behaviors of 40Cr steel
    Wang, Jing
    Lu, Leilei
    Ji, Zhikuan
    Tribology Online, 2015, 10 (04) : 273 - 281
  • [48] Optimization of Laser Shock Process Parameters for 40Cr Steel
    Chen, Xiuyu
    Sun, Jie
    Xu, Zhilong
    Chen, Junying
    Jiang, Qingshan
    Li, Yi
    Li, Jiayuan
    Cheng, Jun
    COATINGS, 2022, 12 (12)
  • [49] Galvanic corrosion between depleted uranium and 40Cr Steel
    Pu Zhen
    Wang Qing-fu
    Shuai Mao-bin
    Lang Ding-mu
    MATERIALS SCIENCE AND NANOTECHNOLOGY I, 2013, 531-532 : 220 - +
  • [50] Residual stress distribution at grind-hardening layer surface of the 40Cr workpiece
    Zou, J. F.
    Pei, H. J.
    Hua, C. L.
    Jiao, B.
    Wang, G. C.
    MATERIALS RESEARCH INNOVATIONS, 2015, 19 : 580 - 584